    Residual stress characterization of single and triple-pass autogenously welded stainless steel pipes

    Get PDF
    Using neutron diffraction the components of the residual stress field have been determined in the region near a mid-length groove in two identical austenitic stainless pipes in which weld beads had been laid down. One pipe sample had a single pass, and the second a triple pass, autogenous weld deposited around the groove circumference. The results show the effect on the stress field of the additional weld deposited and are compared to the results of Finite Element Modelling. The hoop stress component is found to be generally tensile, and greater in the triple pass weldment than in the single pass weldment. The hoop stresses reach peak values of around 400 MPa in tension. X-ray measurements of the residual stress components on the near inner surface of the pipe weldments are also presented, and show tensile stresses in both pipes, with a higher magnitude in the three-pass weldment

    Residual stress measurement round robin on an electron beam welded joint between austenitic stainless steel 316L(N) and ferritic steel P91

    Get PDF
    This paper is a research output of DMW-Creep project which is part of a national UK programme through the RCUK Energy programme and India's Department of Atomic Energy. The research is focussed on understanding the characteristics of welded joints between austenitic stainless steel and ferritic steel that are widely used in many nuclear power generating plants and petrochemical industries as well as conventional coal and gas-fired power systems. The members of the DMW-Creep project have under- taken parallel round robin activities measuring the residual stresses generated by a dissimilar metal weld (DMW) between AISI 316L(N) austenitic stainless steel and P91 ferritic-martensitic steel. Electron beam (EB) welding was employed to produce a single bead weld on a plate specimen and an additional smoothing pass (known cosmetic pass) was then introduced using a defocused beam. The welding re- sidual stresses have been measured by five experimental methods including (I) neutron diffraction (ND), (II) X-Ray diffraction (XRD), (III) contour method (CM), (IV) incremental deep hole drilling (iDHD) and (V) incremental centre hole drilling (iCHD). The round robin measurements of weld residual stresses are compared in order to characterise surface and sub-surface residual stresses comprehensively

    Perspectives on Interstellar Dust Inside and Outside of the Heliosphere

    Full text link
    Measurements by dust detectors on interplanetary spacecraft appear to indicate a substantial flux of interstellar particles with masses exceeding 10^{-12}gram. The reported abundance of these massive grains cannot be typical of interstellar gas: it is incompatible with both interstellar elemental abundances and the observed extinction properties of the interstellar dust population. We discuss the likelihood that the Solar System is by chance located near an unusual concentration of massive grains and conclude that this is unlikely, unless dynamical processes in the ISM are responsible for such concentrations. Radiation pressure might conceivably drive large grains into "magnetic valleys". If the influx direction of interstellar gas and dust is varying on a ~10 yr timescale, as suggested by some observations, this would have dramatic implications for the small-scale structure of the interstellar medium.Comment: 13 pages. To appear in Space Science Review

    Bumpy black holes from spontaneous Lorentz violation

    Full text link
    We consider black holes in Lorentz violating theories of massive gravity. We argue that in these theories black hole solutions are no longer universal and exhibit a large number of hairs. If they exist, these hairs probe the singularity inside the black hole providing a window into quantum gravity. The existence of these hairs can be tested by future gravitational wave observatories. We generically expect that the effects we discuss will be larger for the more massive black holes. In the simplest models the strength of the hairs is controlled by the same parameter that sets the mass of the graviton (tensor modes). Then the upper limit on this mass coming from the inferred gravitational radiation emitted by binary pulsars implies that hairs are likely to be suppressed for almost the entire mass range of the super-massive black holes in the centers of galaxies.Comment: 40 pages, 4 figure

    Reddening law and interstellar dust properties along Magellanic sight-lines

    Full text link
    This study establishes that SMC, LMC and Milky Way extinction curves obey the same extinction law which depends on the 2200A bump size and one parameter, and generalizes the Cardelli, Clayton and Mathis (1989) relationship. This suggests that extinction in all three galaxies is of the same nature. The role of linear reddening laws over all the visible/UV wavelength range, particularly important in the SMC but also present in the LMC and in the Milky Way, is also highlighted and discussed.Comment: accepted for publication in Astrophysics and Space Science. 16 pages, 12 figures. Some figures are colour plot

    The Effect of Abaloparatide-SC on Fracture Risk Is Independent of Baseline FRAX Fracture Probability: A Post Hoc Analysis of the ACTIVE Study

    Get PDF
    Daily subcutaneous (SC) injections of the investigational drug abaloparatide-SC (80 mcg) for 18 months significantly decrease the risk of vertebral and nonvertebral fracture compared with placebo in postmenopausal women. We examined the efficacy of abaloparatide-SC as a function of baseline fracture risk, assessed using the FRAX tool. Baseline clinical risk factors (age, body mass index [BMI], prior fracture, glucocorticoid use, rheumatoid arthritis, and smoking) were entered into country-specific FRAX models to calculate the 10-year probability of major osteoporotic fractures, with or without femoral neck bone mineral density (BMD). The interaction between probability of a major osteoporotic fracture and treatment efficacy was examined by a Poisson regression. A total of 821 women randomized to placebo and 824 women to abaloparatide-SC, mean age 69 years in both groups, were followed for up to 2 years. At baseline, the 10-year probability of major osteoporotic fractures (with BMD) ranged from 2.3% to 57.5% (mean 13.2%). Treatment with abaloparatide-SC was associated with a 69% (95% confidence interval [CI] 38–85%) decrease in major osteoporotic fracture (MOF) and a 43% (95% CI 9–64%) decrease in any clinical fracture compared with placebo. For all outcomes, hazard ratios tended to decrease (ie, greater efficacy) with increasing fracture probability. Whereas the interaction approached significance for the outcome of any fracture (p = 0.11), there was no statistically significant interaction for any of the fracture outcomes. Similar results were noted when FRAX probability was computed without BMD. Efficacy of abaloparatide-SC to decrease the risk of major osteoporotic fracture or any clinical fracture in postmenopausal women with low BMD and/or prior fracture appears independent of baseline fracture probability. © 2017 American Society for Bone and Mineral Research

    Analysis of Residual Stresses in Laser-Shock-Peened and Shot-Peened Marine Steel Welds

    Get PDF
    Laser peening is now the preferred method of surface treatment in many applications. The magnitude and depth of the compressive residual stress induced by laser peening can be influenced strongly by the number of peen layers (the number of laser hits at each point) and by processing conditions including the use of a protective ablative layer. In this study, residual stresses have been characterized in laser and shot-peened marine butt welds with a particular focus at the fatigue crack initiation location at the weld toe. X-ray diffraction, synchrotron X-ray diffraction, incremental center-hole drilling, and the contour method were used for determination of residual stress. Results showed that the use of ablative tape increased the surface compressive stress, and the depth of compressive stress increased with an increase in number of peening layers. A key result is that variation of residual stress profile across laser peen spots was seen, and the residual stress magnitude varies between the center and edges of the spots

    Neutron diffraction residual stress measurements on girth-welded 304 stainless steel pipes with weld metal deposited up to half and full pipe wall thickness

    Get PDF
    The residual stress distribution has been measured in two girth-welded austenitic stainless steel pipe weldments using time-of-flight neutron diffraction. One had weld filler metal deposited up to half the pipe wall thickness, and one had weld metal deposited up to full pipe wall thickness. The aim of the work is to evaluate the evolution in residual stress profile on filling the weld, on which there is little experimental data, and where the selection of the correct hardening model used in finite element modelling can benefit greatly from an understanding of the intermediate residual stresses partway through the welding operation. The measured residual stresses are compared with those calculated by finite element modelling and measured using X-ray diffraction. The results show a change in the measured hoop stress at the weld toe from tension to compression between the half-and fully-filled weld. The finite element results show an overprediction of the residual stress, which may be a consequence of the simple isotropic hardening model applied. The results have implications for the likely occurrence of stress corrosion cracking in this important type of pipe-to-pipe weldment
    • …