195 research outputs found

    Management of chest keloids

    Get PDF
    Keloid formation is one of the most challenging clinical problems in wound healing. With increasing frequency of open heart surgery, chest keloid formations are not infrequent in the clinical practice. The numerous treatment methods including surgical excision, intralesional steroid injection, radiation therapy, laser therapy, silicone gel sheeting, and pressure therapy underscore how little is understood about keloids. Keloids have a tendency to recur after surgical excision as a single treatment. Stretching tension is clearly associated with keloid generation, as keloids tend to occur on high tension sites such as chest region. The authors treated 58 chest keloid patients with surgical excision followed by intraoperative and postoperative intralesional steroid injection. Even with minor complications and recurrences, our protocol results in excellent outcomes in cases of chest keloids

    IceCube - the next generation neutrino telescope at the South Pole

    Get PDF
    IceCube is a large neutrino telescope of the next generation to be constructed in the Antarctic Ice Sheet near the South Pole. We present the conceptual design and the sensitivity of the IceCube detector to predicted fluxes of neutrinos, both atmospheric and extra-terrestrial. A complete simulation of the detector design has been used to study the detector's capability to search for neutrinos from sources such as active galaxies, and gamma-ray bursts.Comment: 8 pages, to be published with the proceedings of the XXth International Conference on Neutrino Physics and Astrophysics, Munich 200

    Search for Charged Higgs Bosons in e+e- Collisions at \sqrt{s} = 189 GeV

    Full text link
    A search for pair-produced charged Higgs bosons is performed with the L3 detector at LEP using data collected at a centre-of-mass energy of 188.6 GeV, corresponding to an integrated luminosity of 176.4 pb^-1. Higgs decays into a charm and a strange quark or into a tau lepton and its associated neutrino are considered. The observed events are consistent with the expectations from Standard Model background processes. A lower limit of 65.5 GeV on the charged Higgs mass is derived at 95 % confidence level, independent of the decay branching ratio Br(H^{+/-} -> tau nu)

    Search for the standard model Higgs boson at LEP

    Get PDF

    Modification and re-validation of the ethyl acetate-based multi-residue method for pesticides in produce

    Get PDF
    The ethyl acetate-based multi-residue method for determination of pesticide residues in produce has been modified for gas chromatographic (GC) analysis by implementation of dispersive solid-phase extraction (using primary–secondary amine and graphitized carbon black) and large-volume (20 ΌL) injection. The same extract, before clean-up and after a change of solvent, was also analyzed by liquid chromatography with tandem mass spectrometry (LC–MS–MS). All aspects related to sample preparation were re-assessed with regard to ease and speed of the analysis. The principle of the extraction procedure (solvent, salt) was not changed, to avoid the possibility invalidating data acquired over past decades. The modifications were made with techniques currently commonly applied in routine laboratories, GC–MS and LC–MS–MS, in mind. The modified method enables processing (from homogenization until final extracts for both GC and LC) of 30 samples per eight hours per person. Limits of quantification (LOQs) of 0.01 mg kg−1 were achieved with both GC–MS (full-scan acquisition, 10 mg matrix equivalent injected) and LC–MS–MS (2 mg injected) for most of the pesticides. Validation data for 341 pesticides and degradation products are presented. A compilation of analytical quality-control data for pesticides routinely analyzed by GC–MS (135 compounds) and LC–MS–MS (136 compounds) in over 100 different matrices, obtained over a period of 15 months, are also presented and discussed. At the 0.05 mg kg−1 level acceptable recoveries were obtained for 93% (GC–MS) and 92% (LC–MS–MS) of pesticide–matrix combinations

    Effect of ageing on the microstructural evolution in a new design of maraging steels with carbon

    Get PDF
    A new maraging steel, based on carbide precipitation, is described. Two alloys were designed namely Fe-10Mn-0.25C-2Cr-1Mo wt% (2CrMo) and Fe-10Mn-0.25C-1Cr-2Mo wt% (Cr2Mo). These compositions were chosen to achieve ultra-high strength and high tensile elongation; the former and latter are promoted through the simulatenous precipitation of Cr- and Mo-rich carbides and Mn-rich reverted austenite. The alloys were manufactured through the standard melting, casting and hot working route. Following a solution treatment at 870 °C and quench, which gave a fully martensitic structure, the alloys were aged for various times at 510 °C. The microstructure and tensile properties were investigated in detail as a function of ageing time. The microstructure observed was dominated by micron scale and nanometre scale Mn segregation which determined the local Ac3 temperature. Austenite reversion occurred in both alloys, peaking at 16 h in both cases. In the 2CrMo alloy, the reverted austenite was mainly globular in morphology due the Ac3 temperature being lower than the ageing temperature, but was acicular in the Cr2Mo with Ac3 similar to the ageing temperature of 510 °C. Moreover, acicular austenite was promoted by Mn segregation at martensite lath boundaries in Cr2Mo. In the 2CrMo steel, carbide precipitation (M3C and M7C3) occurred during heating to the ageing temperature, but the carbides gradually dissolved with further ageing. In contrast, in the Cr2Mo alloy, precipitation of carbides (M7C3 and M2C) occurred during ageing, the volume fraction of which increased with ageing time. In both alloys a TRIP effect was observed, but the extent of this was greater for the Cr2Mo alloy. The complex microstructure obtained after 16 h led to an excellent combination of strength of 1.3 GPa and elongation of 18%. Physics-based models for the microstructure in martensite, precipitation kinetics, as well as for TRIP in austenite were employed to explain and predict the individual strengthtening contributions of the microstructure to the total strength, confirming that the maximum strength-elongation relationship found after 16 h is due to an optimal combination of a slightly overaged - but still strong- martensite and 30% of reverted austenite, for increased work hardening and ductility
    • 