    Fast pyrolysis of halogenated plastics recovered from waste computers

    Get PDF
    The disposal of waste computers is an issue that is gaining increasing interest around the world. In this paper, results from the fast pyrolysis in a fluidized bed reactor of three different waste computer monitor casings composed of mainly acrylonitrile-butadiene-styrene (ABS) copolymer and two different waste computer body casings composed of mostly poly(vinyl chloride) (PVC) type polymers are presented. Preliminary characterization of the waste plastics was investigated using coupled thermogravimetric analysis-Fourier transform infrared spectrometry (TGA-FT-IR). The results showed that the plastics decomposed in two stages. For the ABS-containing monitor casings, aromatic and aliphatic material were released in the first and second stages. The PVC-containing computer body casing samples showed a first-stage evolution of HCl and a second stage evolution of aromatic and aliphatic material and further HCl. In addition, each of the five plastics was fast-pyrolyzed in a laboratory-scale fluidized bed reactor at 500 °C. The fluidized bed pyrolysis led to the conversion of most of the plastics to pyrolysis oil, although the two PVC computer body cases produced large quantities of HCl. The pyrolysis oils were characterized by GC-MS and it was found that they were chemically very heterogeneous and contained a wide range of aliphatic, aromatic, halogenated, oxygenated, and nitrogenated compounds

    Chitosan–Starch–Keratin composites: Improving thermo-mechanical and degradation properties through chemical modification

    Get PDF
    The lysozyme test shows an improved in the degradability rate, the weight loss of the films at 21 days is reduced from 73 % for chitosan-starch matrix up to 16 % for the composites with 5wt% of quill; but all films show a biodegradable character depending on keratin type and chemical modification. The outstanding properties related to the addition of treated keratin materials show that these natural composites are a remarkable alternative to potentiat-ing chitosan–starch films with sustainable featuresChitosan–starch polymers are reinforced with different keratin materials obtained from chicken feather. Keratin materials are treated with sodium hydroxide; the modified surfaces are rougher in comparison with untreated surfaces, observed by Scanning Electron Microscopy. The results obtained by Differential Scanning Calorimetry show an increase in the endothermic peak related to water evaporation of the films from 92 °C (matrix) up to 102–114 °C (reinforced composites). Glass transition temperature increases from 126 °C in the polymer matrix up to 170–200 °C for the composites. Additionally, the storage modulus in the composites is enhanced up to 1614 % for the composites with modified ground quill, 2522 % for composites with modified long fiber and 3206 % for the composites with modified short fiber. The lysozyme test shows an improved in the degradability rate, the weight loss of the films at 21 days is reduced from 73 % for chitosan-starch matrix up to 16 % for the composites with 5wt% of quill; but all films show a biodegradable character depending on keratin type and chemical modification. The outstanding properties related to the addition of treated keratin materials show that these natural composites are a remarkable alternative to potentiat-ing chitosan–starch films with sustainable featuresUniversidad Autónoma del Estado de México Tecnológico Nacional de México, Instituto Tecnológico de Querétaro Universidad Nacional Autónoma de México Tecnológico Nacional de México, Instituto Tecnológico de Celaya Universidad Autónoma de Cd. Juáre

    Assessing the survivability of biomarkers within terrestrial material impacting the lunar surface

    Get PDF
    The history of organic and biological markers (biomarkers) on the Earth is effectively non-existent in the geological record >3.8 Ga ago. Here, we investigate the potential for terrestrial material (i.e., terrestrial meteorites) to be transferred to the Moon by a large impact on Earth and subsequently survive impact with the lunar surface, using the iSALE shock physics code. Three-dimensional impact simulations show that a typical basin-forming impact on Earth can eject solid fragments equivalent to ~10–3 of an impactor mass at speeds sufficient to transfer from Earth to the Moon. Previous modelling of meteorite survivability has relied heavily upon the assumption that peak-shock pressures can be used as a proxy for gauging survival of projectiles and their possible biomarker constituents. Here, we show the importance of considering both pressure and temperature within the projectile, and the inclusion of both shock and shear heating, in assessing biomarker survival. Assuming that they survive launch from Earth, we show that some biomarker molecules within terrestrial meteorites are likely to survive impact with the Moon, especially at the lower end of the range of typical impact velocities for terrestrial meteorites (2.5 km s-1). The survival of larger biomarkers (e.g., microfossils) is also assessed, and we find limited, but significant, survival for low impact velocity and high target porosity scenarios. Thermal degradation of biomarkers shortly after impact depends heavily upon where the projectile material lands, whether it is buried or remains on the surface, and the related cooling timescales. Comparing sandstone and limestone projectiles shows similar temperature and pressure profiles for the same impact velocities, with limestone providing slightly more favourable conditions for biomarker survival

    Catalytic Hydrotreatment of Alcell Lignin Using Supported Ru, Pd, and Cu Catalysts

    No full text
    corecore