    Avaliação da resistência ao cisalhamento da união entre duas ligas a base de CoCr e uma cerâmica

    Get PDF
    INTRODUCTION: Based on the importance of the integrity of the metal/ceramic interface, the purpose of this work was to evaluate the shear bond strength of the metal-ceramic union of two Co-Cr alloys (Wirobond C, Bego; Remanium 2000, Dentaurum) combined with Omega 900 ceramic (Vita Zahnfabrik). MATERIAL and METHOD: Eleven cylindrical matrixes were made for each alloy, and the metallic portion was obtained with the lost wax casting technique with standardized waxing of 4mm of height and of 4mm of diameter. The ceramic was applied according to the manufacturer’s recommendations with the aid of a teflon matrix that allowed its dimension to be standardized in the same size as the metallic portion. The specimens were submitted to the shear bond test in an universal testing machine (EMIC), with the aid of a device developed for such intention, and constant speed of 0.5mm/min. RESULTS and CONCLUSIONS: The mean resistance was 48.387MPa for Wirobond C alloy, with standard deviation of 17.718, and 55.956MPa for Remanium 2000, with standard deviation of 17.198. No statistically significant difference was observed between the shear strength of the two metal-ceramic alloys. ______________________________________________________________________________________________________________ RESUMOINTRODUÇÃO: Baseados na importância da integridade da interface metal-cerâmica, este trabalho tem como objetivo avaliar a resistência ao cisalhamento da união metal-cerâmica de duas ligas de Co-Cr (Wirobond C, Bego; Remanium 2000, Dentaurum) combinadas com a cerâmica Omega 900 (Vita Zahnfabrik). MATERIAIS E MÉTODOS: Foram confeccionados 11 corpos-de-prova cilíndricos para cada liga utilizada, sendo que a porção metálica foi obtida por fundição pela técnica da cera perdida, através de enceramentos padronizados com 4mm de altura por 4mm de diâmetro. A aplicação da cerâmica foi realizada segundo recomendações do fabricante, com auxílio de uma matriz de teflon que permitia sua padronização com as mesmas dimensões da porção metálica. Os corpos-de-prova foram submetidos ao ensaio de resistência ao cisalhamento em máquina de ensaios universal (EMIC), com auxílio de dispositivo desenvolvido para tal propósito, sob velocidade constante de 0,5mm/ min. RESULTADOS E CONCLUSÕES: As médias de resistência obtidas foram 48,387 MPa para a liga Wirobond C, com desvio padrão de 17,718, e 55,956 MPa para a Remanium 2000, com desvio padrão de 17,198. Após análise de variância foi possível observar que não há diferença estatisticamente significante entre os valores de resistência ao cisalhamento das duas ligas metalocerâmicas

    Cytotoxic Interactive Effects of Dentin Bonding Components on Mouse Fibroblasts

    Full text link
    Previous studies have shown a wide range of pulpal reactions to dentin bonding systems and a poor correlation between in vitro and in vivo toxicity of dentin bonding agents. Because dentin bonding agents are composed of multiple components which may diffuse through dentin, we hypothesized that these components may cause cytotoxicity through interactive (synergistic) effects. We investigated the cytotoxicities of four dentin bonding components-HEMA, Bis-GMA, TEGDMA, and UDMA-and interactive effects for three binary combinations of the dentin bonding components-HEMA and Bis-GMA, Bis-GMA and TEGDMA, and TEGDMA and UDMA. Cytotoxicities to Balb/c 3T3 mouse fibroblasts were measured by the MTT assay. Concentrations which caused 50% toxicity compared with controls (TC50 values) were compared, and the interactive effects were determined by evaluation of the differences between observed and expected MTT activities of the cells. The ranks of toxicity of the dentin bonding components in terms of TC50 values were as follows: Bis-GMA > UDMA > TEGDMA >>> HEMA (least toxic) after 24- and 72-hour exposures. As binary combinations, the three combinations of dentin bonding components interacted in three ways—synergism, additivism, and antagonism-which were influenced by the concentrations of both components. The longer period of exposure resulted in a significant increase in the cytotoxicity of the dentin bonding components and combinations. The findings indicate that both exposure time and the interactions between the dentin bonding components may be important parameters in determining the cytotoxicity of dentin bonding agents in vivo.Peer Reviewedhttp://deepblue.lib.umich.edu/bitstream/2027.42/66489/2/10.1177_00220345950740091601.pd

    E-Glass Fiber Reinforced Composites in Dental Applications

    Get PDF
    Fiber reinforced composites (FRCs) are more and more widely applied in dentistry to substitute for metallic restorations: periodontal splints, fixed partial dentures, endodontic posts, orthodontic appliances, and some other indirect restorations. In general in FRCs, the fiber reinforcement provides the composite structure with better biomechanical performance due to their superior properties in tension and flexure. Nowadays, the E-glass fiber is most frequently used because of its chemical resistance and relatively low cost. Growing interest is being paid to enhance its clinical performance. Moreover, various techniques are utilized to reinforce the adhesion between the fiber and the matrix. Oral conditions set special requirements and challenges for the clinical applications of FRCs. The biomechanical properties of dental materials are of high importance in dentistry, and given this, there is on-going scientific interest to develop E-glass fiber reinforced composite systems. FRCs are generally biocompatible and their toxicity is not a concern. © 2011 The Author(s).published_or_final_versionSpringer Open Choice, 21 Feb 201

    Retrieval analysis of different orthodontic brackets: the applicability of electron microprobe techniques for determining material heterogeneities and corrosive potential

    Get PDF
    OBJECTIVE: The objective of this study was to investigate the applicability of micro-analytical methods with high spatial resolution to the characterization of the composition and corrosion behavior of two bracket systems. MATERIAL AND METHODS: The surfaces of six nickel-free brackets and six nickel-containing brackets were examined for signs of corrosion and qualitative surface analysis using an electron probe microanalyzer (EPMA), prior to bonding to patient's tooth surfaces and four months after clinical use. The surfaces were characterized qualitatively by secondary electron (SE) images and back scattered electron (BSE) images in both compositional and topographical mode. Qualitative and quantitative wavelength-dispersive analyses were performed for different elements, and by utilizing qualitative analysis the relative concentration of selected elements was mapped two-dimensionally. The absolute concentration of the elements was determined in specially prepared brackets by quantitative analysis using pure element standards for calibration and calculating correction-factors (ZAF). RESULTS: Clear differences were observed between the different bracket types. The nickel-containing stainless steel brackets consist of two separate pieces joined by a brazing alloy. Compositional analysis revealed two different alloy compositions, and reaction zones on both sides of the brazing alloy. The nickel-free bracket was a single piece with only slight variation in element concentration, but had a significantly rougher surface. After clinical use, no corrosive phenomena were detectable with the methods applied. Traces of intraoral wear at the contact areas between the bracket slot and the arch wire were verified. CONCLUSION: Electron probe microanalysis is a valuable tool for the characterization of element distribution and quantitative analysis for corrosion studies