7 research outputs found

    Durabilité d’un ciment composé à base de mâchefer de Tefereyre (Niger): absorption capillaire, porosité accessible à l’eau et attaque acide

    Get PDF
    In this study, we evaluate the durability characteristics of composite cement with coal bottom ash produced by SONICHAR (Société Nigérienne de Charbon). The study firstly consists in the determination of the pozzolanic activity index of the coal bottom ash and the optimum rate to use in the composite cement. Thereafter an evaluation of capillary absorption, porosity accessible to water and resistance to sulfuric and nitric acid attack of mortar prepared made with the composite cement is performed. The results showed that the coal bottom ash powder obtained by grinding can partially substitute Portland cement at a rate of 15% enable to develop a CEM II A composite cement according to EN 197-1 Standard.Dans la présente étude, nous évaluons les caractéristiques vis-à-vis de la durabilité d’un ciment composé à base de mâchefer de charbon produit par la SONICHAR (Société Nigérienne de production d’énergie à base de  charbon minéral). L’étude consiste d’abord en la détermination de l’indice d’activité pouzzolanique du mâchefer et du taux optimal à utiliser pour mettre en place un ciment composé. Par la suite une évaluation du taux d’absorption capillaire, de la porosité accessible à l’eau et à la résistance à l’attaque acide sulfurique et nitrique de mortier confectionné à base du ciment composé élaboré est effectuée. Les résultats montrent que la poudre de ce mâchefer obtenu par broyage peut substituer partiellement le ciment Portland à un taux de 15% permettant d’élaborer un ciment composé de type CEM II A selon la norme EN 197-1

    Élaboration et caractérisation d’un écociment à base de poudre de mâchefer de charbon

    No full text
    This research is part of a process of valorization of local industrial by-products in the cement industry. lt focuses on the possibility f using coal bottom ash powder produced by SONICHAR in Niger as cement partial addition. After a physicochemical and environmental characterization of the coal bottom ash powder, we determined its pozzolanic reactivity and it mechanical activity index. The results show that the coal bottom ash powder presents a pozzolanicity whose relatively slow kinetics do ne start before 14 days. On the other hand, this coal bottom ash can be considered as a mineral addition of type 11 according to the standard EN 206-1 with an activity index of 0.76. This is why we used it to develop three CEM 11/A composite cements with a strength class of 42.5 when the substitution rate is 10% and a strength class of 32.5 when the rate of substitution is 15% and 20%. Normal mortars have been formulated with these cements and are characterized physically and mechanically. The durability of the mortars has also been studied, in particular from the point of view of the kinetics of carbonation and leaching in the presence of ammonium nitrate. Finally, it appears that the coal bottom ash powder may indeed be incorporated as an addition in the preparation of composite cements. The long-term mechanical characteristics (90 days) and the durability of the mortars made from these cements are preserved when the substitution rate does not exceed 10%.Ce travail de recherche s'inscrit dans une dynamique de valorisation des sous-produits industriels locaux dans l'industrie cimentière. Il porte essentiellement sur la possibilité d'utiliser la poudre de mâchefer de charbon produit par la SONICHAR au Niger pour élaborer des ciments composés. Après une caractérisation physico-chimique et environnementale de la poudre de mâchefer, nous avons déterminé sa réactivité pouzzolanique et son indice d'activité mécanique. Les résultats montrent que la poudre de mâchefer présente une pouzzolanicité dont la cinétique relativement lente ne démarre pas avant 14 jours. D'autre part, ce mâchefer peut être considéré comme une addition minérale du type Il selon la norme EN 206-1 avec un indice d'activité de 0,76. C'est pourquoi nous l'avons utilisé pour élaborer trois ciments composés de type CEM 11/A avec une classe de résistance de 42,5 lorsque le taux de substitution est de 10% et une classe de résistance de 32,5 lorsque Je taux de substitution est de 15% et 20%. Des mortiers normaux ont été élaborés à partir de ces ciments et caractérisés sur les plans physiques et mécaniques. La durabilité des mortiers a également été étudiée notamment du point de vue de la cinétique de carbonatation et de lixiviation en présence de nitrate d'ammonium. Il ressort en définitive que la poudre de mâchefer peut bien être incorporée comme addition dans l’élaboration de ciments composés. Les caractéristiques mécaniques à long terme (90 jours) et la durabilité des mortiers confectionnés à partir de ces ciments sont conservées lorsque le taux de substitution n'excède pas 10%

    Elaboration and characterization of mineral coal bottom ash powder eco-cement

    No full text
    Ce travail de recherche s'inscrit dans une dynamique de valorisation des sous-produits industriels locaux dans l'industrie cimentière. Il porte essentiellement sur la possibilité d'utiliser la poudre de mâchefer de charbon produit par la SONICHAR au Niger pour élaborer des ciments composés. Après une caractérisation physico-chimique et environnementale de la poudre de mâchefer, nous avons déterminé sa réactivité pouzzolanique et son indice d'activité mécanique. Les résultats montrent que la poudre de mâchefer présente une pouzzolanicité dont la cinétique relativement lente ne démarre pas avant 14 jours. D'autre part, ce mâchefer peut être considéré comme une addition minérale du type Il selon la norme EN 206-1 avec un indice d'activité de 0,76. C'est pourquoi nous l'avons utilisé pour élaborer trois ciments composés de type CEM 11/A avec une classe de résistance de 42,5 lorsque le taux de substitution est de 10% et une classe de résistance de 32,5 lorsque Je taux de substitution est de 15% et 20%. Des mortiers normaux ont été élaborés à partir de ces ciments et caractérisés sur les plans physiques et mécaniques. La durabilité des mortiers a également été étudiée notamment du point de vue de la cinétique de carbonatation et de lixiviation en présence de nitrate d'ammonium. Il ressort en définitive que la poudre de mâchefer peut bien être incorporée comme addition dans l’élaboration de ciments composés. Les caractéristiques mécaniques à long terme (90 jours) et la durabilité des mortiers confectionnés à partir de ces ciments sont conservées lorsque le taux de substitution n'excède pas 10%.This research is part of a process of valorization of local industrial by-products in the cement industry. lt focuses on the possibility f using coal bottom ash powder produced by SONICHAR in Niger as cement partial addition. After a physicochemical and environmental characterization of the coal bottom ash powder, we determined its pozzolanic reactivity and it mechanical activity index. The results show that the coal bottom ash powder presents a pozzolanicity whose relatively slow kinetics do ne start before 14 days. On the other hand, this coal bottom ash can be considered as a mineral addition of type 11 according to the standard EN 206-1 with an activity index of 0.76. This is why we used it to develop three CEM 11/A composite cements with a strength class of 42.5 when the substitution rate is 10% and a strength class of 32.5 when the rate of substitution is 15% and 20%. Normal mortars have been formulated with these cements and are characterized physically and mechanically. The durability of the mortars has also been studied, in particular from the point of view of the kinetics of carbonation and leaching in the presence of ammonium nitrate. Finally, it appears that the coal bottom ash powder may indeed be incorporated as an addition in the preparation of composite cements. The long-term mechanical characteristics (90 days) and the durability of the mortars made from these cements are preserved when the substitution rate does not exceed 10%

    Élaboration et caractérisation d’un écociment à base de poudre de mâchefer de charbon minéral

    No full text
    This research is part of a process of valorization of local industrial by-products in the cement industry. lt focuses on the possibility f using coal bottom ash powder produced by SONICHAR in Niger as cement partial addition. After a physicochemical and environmental characterization of the coal bottom ash powder, we determined its pozzolanic reactivity and it mechanical activity index. The results show that the coal bottom ash powder presents a pozzolanicity whose relatively slow kinetics do ne start before 14 days. On the other hand, this coal bottom ash can be considered as a mineral addition of type 11 according to the standard EN 206-1 with an activity index of 0.76. This is why we used it to develop three CEM 11/A composite cements with a strength class of 42.5 when the substitution rate is 10% and a strength class of 32.5 when the rate of substitution is 15% and 20%. Normal mortars have been formulated with these cements and are characterized physically and mechanically. The durability of the mortars has also been studied, in particular from the point of view of the kinetics of carbonation and leaching in the presence of ammonium nitrate. Finally, it appears that the coal bottom ash powder may indeed be incorporated as an addition in the preparation of composite cements. The long-term mechanical characteristics (90 days) and the durability of the mortars made from these cements are preserved when the substitution rate does not exceed 10%.Ce travail de recherche s'inscrit dans une dynamique de valorisation des sous-produits industriels locaux dans l'industrie cimentière. Il porte essentiellement sur la possibilité d'utiliser la poudre de mâchefer de charbon produit par la SONICHAR au Niger pour élaborer des ciments composés. Après une caractérisation physico-chimique et environnementale de la poudre de mâchefer, nous avons déterminé sa réactivité pouzzolanique et son indice d'activité mécanique. Les résultats montrent que la poudre de mâchefer présente une pouzzolanicité dont la cinétique relativement lente ne démarre pas avant 14 jours. D'autre part, ce mâchefer peut être considéré comme une addition minérale du type Il selon la norme EN 206-1 avec un indice d'activité de 0,76. C'est pourquoi nous l'avons utilisé pour élaborer trois ciments composés de type CEM 11/A avec une classe de résistance de 42,5 lorsque le taux de substitution est de 10% et une classe de résistance de 32,5 lorsque Je taux de substitution est de 15% et 20%. Des mortiers normaux ont été élaborés à partir de ces ciments et caractérisés sur les plans physiques et mécaniques. La durabilité des mortiers a également été étudiée notamment du point de vue de la cinétique de carbonatation et de lixiviation en présence de nitrate d'ammonium. Il ressort en définitive que la poudre de mâchefer peut bien être incorporée comme addition dans l’élaboration de ciments composés. Les caractéristiques mécaniques à long terme (90 jours) et la durabilité des mortiers confectionnés à partir de ces ciments sont conservées lorsque le taux de substitution n'excède pas 10%

    Physico-mechanical and durability characterization of earthen plaster stabilized with fermented rice husk for coating adobe walls

    No full text
    AbstractThe present study aims to study the effect of fermented rice husk (RH) on earth plaster for coating and improving the durability of adobe walls. The mixtures of clayey earthen materials and 0%, 33%, 50%, and 67% of fermented RH of the total volume of the mixture are studied to assess their physicomechanical and durability properties. The RH is previously fermented separately in water for the periods of 2, 3, and 3 weeks. The pastes obtained after mixing the clayey earth material and fermented RH were used to mold 4 × 4 × 16 cm3 test specimens. The specimens were dried under ambient laboratory conditions [Formula: see text] and 35[Formula: see text]HR) for 21 days before their characterization. The clay earthen material mainly contains silt (51%), clay (24%), sand (23%), and gravel (3%). It has a liquidity limit, plasticity index, and methylene blue value of 32%, 20%, and 2.66, respectively. The results show that apparent density, linear shrinkage, resistance to compression, and the thermal conductivity of the plaster specimens, respectively, decrease from 1.88 to 1.07 g/cm3, 4.52 to 0.83%, 3.88 to 0.82 MPa, and 0.87 to 0.05 W/m.K with increasing volumetric content of RH from 0% to 67%. Moreover, the resistance to abrasion increased. The resistance to capillary water absorption and water erosion was deficient for the content of RH above 50%. The mixture containing up to 33% of RH allows to improve engineering performances and reaches acceptable durability and would therefore be useful for coating adobe walls
    corecore