30 research outputs found

    РОСТ ЗЕРНОГРАНИЧНОЙ ПРОСЛОЙКИ (αTi) В СПЛАВАХ Ti–Co

    Get PDF
    The paper studies the effect of temperature on the formation of (αTi) grain boundary layer in Ti–2wt.%Co and Ti–4wt.%Co alloys in the (αTi) + (βTi) two-phase region of the Ti–Co phase diagram within the temperature range of 690–810 °C. The paper studies kinetics of thickness growth (∆) of the (αTi) phase grain boundary layer in Ti–2wt.%Co alloy at a temperature of 750 °C. It demonstrates dependence of the thickness of grain boundary layer on the annealing time as ∆ ~ t 1/3. Analysis of experimental results suggests that increase in ∆ is a manifestation of the (αTi) coalescence process controlled by volume diffusion.Исследовалось влияние температуры на образование зернограничной прослойки (αTi) в сплавах Ti–2мас.%Co и Ti–4мас.%Co в двухфазной области (αTi) + (βTi) фазовой диаграммы Ti–Co в интервале температур 690–810 °С. Изучена кинетика роста толщины (∆) зернограничной прослойки фазы (αTi) в сплаве Ti–2мас.%Co при температуре 750 °С.Показана ее зависимость от времени отжига как ∆ ~ t 1/3. Анализ результатов экспериментальных наблюдений позволяет предположить, что увеличение ∆ является проявлением процесса коалесценции (αTi), который контролируется объемной диффузией
    corecore