Rare-earth monosulfides as durable and efficient cold cathodes
In their rocksalt structure, rare-earth monosulfides offer a more stable
alternative to alkali metals to attain low or negative electron affinity when
deposited on various III-V and II-VI semiconductor surfaces. In this article,
we first describe the successful deposition of Lanthanum Monosulfide via pulsed
laser deposition on Si and MgO substrates and alumina templates. These thin
films have been characterized by X-ray diffraction, atomic force microscopy,
high resolution transmission electron microscopy, ellipsometry, Raman
spectroscopy, ultraviolet photoelectron spectroscopy and Kelvin probe
measurements. For both LaS/Si and LaS/MgO thin films, the effective work
function of the submicron thick thin films was determined to be about 1 eV from
field emission measurements using the Scanning Anode Field Emission Microscopy
technique. The physical reasons for these highly desirable low work function
properties were explained using a patchwork field emission model of the
emitting surface. In this model, nanocrystals of low work function materials
having a orientation perpendicular to the surface and outcropping it are
surrounded by a matrix of amorphous materials with higher work function. To
date, LaS thin films have been used successfully as cold cathode emitters with
measured emitted current densities as high as 50 A/cm2. Finally, we describe
the successful growth of LaS thin films on InP substrates and, more recently,
the production of LaS nanoballs and nanoclusters using Pulsed Laser Ablation.Comment: 61 pages, 24 figure
Mineralogical and geochemical analysis of Fe-phases in drill-cores from the Triassic Stuttgart Formation at Ketzin CO₂ storage site before CO₂ arrival
Reactive iron (Fe) oxides and sheet silicate-bound Fe in reservoir rocks may affect the subsurface storage of CO2 through several processes by changing the capacity to buffer the acidification by CO2 and the permeability of the reservoir rock: (1) the reduction of three-valent Fe in anoxic environments can lead to an increase in pH, (2) under sulphidic conditions, Fe may drive sulphur cycling and lead to the formation of pyrite, and (3) the leaching of Fe from sheet silicates may affect silicate diagenesis. In order to evaluate the importance of Fe-reduction on the CO2 reservoir, we analysed the Fe geochemistry in drill-cores from the Triassic Stuttgart Formation (Schilfsandstein) recovered from the monitoring well at the CO2 test injection site near Ketzin, Germany. The reservoir rock is a porous, poorly to moderately cohesive fluvial sandstone containing up to 2–4 wt% reactive Fe. Based on a sequential extraction, most Fe falls into the dithionite-extractable Fe-fraction and Fe bound to sheet silicates, whereby some Fe in the dithionite-extractable Fe-fraction may have been leached from illite and smectite. Illite and smectite were detected in core samples by X-ray diffraction and confirmed as the main Fe-containing mineral phases by X-ray absorption spectroscopy. Chlorite is also present, but likely does not contribute much to the high amount of Fe in the silicate-bound fraction. The organic carbon content of the reservoir rock is extremely low (<0.3 wt%), thus likely limiting microbial Fe-reduction or sulphate reduction despite relatively high concentrations of reactive Fe-mineral phases in the reservoir rock and sulphate in the reservoir fluid. Both processes could, however, be fuelled by organic matter that is mobilized by the flow of supercritical CO2 or introduced with the drilling fluid. Over long time periods, a potential way of liberating additional reactive Fe could occur through weathering of silicates due to acidification by CO2
The structure of SgrAI bound to DNA; recognition of an 8 base pair target
The three-dimensional X-ray crystal structure of the ‘rare cutting’ type II restriction endonuclease SgrAI bound to cognate DNA is presented. SgrAI forms a dimer bound to one duplex of DNA. Two Ca2+ bind in the enzyme active site, with one ion at the interface between the protein and DNA, and the second bound distal from the DNA. These sites are differentially occupied by Mn2+, with strong binding at the protein–DNA interface, but only partial occupancy of the distal site. The DNA remains uncleaved in the structures from crystals grown in the presence of either divalent cation. The structure of the dimer of SgrAI is similar to those of Cfr10I, Bse634I and NgoMIV, however no tetrameric structure of SgrAI is observed. DNA contacts to the central CCGG base pairs of the SgrAI canonical target sequence (CR|CCGGYG, | marks the site of cleavage) are found to be very similar to those in the NgoMIV/DNA structure (target sequence G|CCGGC). Specificity at the degenerate YR base pairs of the SgrAI sequence may occur via indirect readout using DNA distortion. Recognition of the outer GC base pairs occurs through a single contact to the G from an arginine side chain located in a region unique to SgrAI
Dynamics Of MoS<sub>2</sub> Photoablation
AbstractSpeed distributions were determined for the ions ejected from MoS2 by excimer laser ablation. It was found that the majority of ionic species were atomic and were ablated with speeds in excess of 6 km/s. The speed distributions were found to be non-Maxwellian and were best described by a supersonic expansion model. The differences in ArF and KrF excimer laser ablation are discussed.</jats:p
Grain size, texture, and crystallinity in lanthanum monosulfide thin films grown by pulsed laser deposition
We report a detailed investigation of the growth of lanthanum monosulfide (LaS) thin films by pulsed laser deposition on (001) magnesium oxide (MgO) substrates in a background of H2S for the purpose of optimizing their crystallinity, texture, and grain size. A variety of films were grown while varying the laser repetition rate, the temperature of the substrate, and the partial pressure of H2S. The thin films were characterized by X-ray diffraction (XRD), atomic force microscopy (AFM), Raman spectroscopy, and high resolution transmission electron microscopy. Films grown at 500 \ub0C with a H2S background pressure of 3.4
7 10 12 4 Pa and a laser repetition rate of 8 Hz produced the LaS film with the largest grains whose size averaged 293 nm. The XRD pattern of these films revealed that their orientation was predominantly (200). AFM images of the surface of these films showed large plate-like grains. This contrasts with the fine grain structure observed in LaS films grown at a lower substrate temperature and lower H2S pressure.Peer reviewed: YesNRC publication: Ye