    Heat treatment of tunisian soft wood species: Effect on the durability, chemical modifications and mechanical properties

    Get PDF
    Last decades, wood was promoted as building material. Wood heat treatment by mild pyrolysis has been reported to improve biological durability and dimensional stability of the material and constitutesan attractive « non biocidal » alternative to classical preservation treatments. Previous studies have shown that conferred properties strongly depend on the heat treatment intensity. A quality control markerbased on mass loss has been developed. For several years, the increased development of Tunisian wood industry provides a significant capacity of wood production and transformation. Forests in Tunisia consistessentially of coniferous species [Aleppo pine (Pinus halepensis), Radiata pine (Pinus radiata), Maritime pine (Pinus pinaster), Stone pine (Pinus pinea)], characterised by a weak natural durability. Improveddurability and fungal resistance should allow the use of Tunisian species in the wood industry. Import limitation of European species and the use of local species allow the conservation of economic valueadded in the country and improve the economic balance. For this reason, several Tunisian softwood species (Aleppo pine, Radiata pine and Maritime pine) have been heat-treated under vacuum atmosphere at230°C to obtain a thermal degradation with mass losses of approximately 8, 10 and 12%. The oven device allows recording the dynamic Mass Loss (ML) during the treatment and following the thermodegradationkinetic. The chemical composition of the studied wood samples was determined before and after heat treatment. For each wood species and treatment intensity, wood chemical and mechanical analyses wereperformed by measuring O/C ratio, bending and hardness tests. Afterward, tests of decay resistance were performed according to the EN 113 Standard, with different fungal attacks (Poria Placenta, CoriolusVersicolor) at 22°C and 70% of humidity for 16 weeks. Results were related to the mass loss. Furthermore, intensity of thermal degradation was evaluated by TD-GC-MS. Treated and untreated wood sampleswere maintained during 15 minutes at 230 °C under nitrogen in the thermodesorption tube in order to analyse and compare resulting from the wood thermodegradation volatile compounds

    Utilization of temperature kinetics as a method to predict treatment intensity and corresponding treated wood quality: Durability and mechanical properties of thermally modified wood

    Get PDF
    Wood heat treatment is an attractive alternative to improve decay resistance of wood species with low natural durability. However, this improvement of durability is realized at the expense of the mechanical resistance. Decay resistance and mechanical properties are strongly correlated to thermal degradation of wood cells wall components. Mass loss resulting from this degradation is a good indicator of treatment intensity and final treated wood properties. However, the introduction of a fast and accurate system for measuring this mass loss on an industrial scale is very difficult. Nowadays, many studies are conducted on the determination of control parameters which could be correlated with the treatment conditions and final heat treated wood quality such as decay resistance. The aim of this study is to investigate the relations between kinetics of temperature used during thermal treatment process representing heat treatment intensity, mass losses due to thermal degradation and conferred properties to heat treated wood. It might appear that relative area of treatment temperature curves is a good indicator of treatment intensity. Heat treatment with different treatment conditions (temperature-time) have been performed under vacuum, on four wood species (one hardwood and three softwoods) in order to obtain thermal degradation mass loses of 8, 10 and 12%. For each experiment, relative areas corresponding to temperature kinetics, mass loss, decay resistance and mechanical properties have been determined. Results highlight the statement that the temperature curves’ area constitutes a good indicator in the prediction of needed treatment intensity, to obtain required wood durability and mechanical properties such as bending resistance and Brinell hardness

    Utilization of temperature kinetics as a method to predict treatment intensity and corresponding treated wood quality: Durability and mechanical properties of thermally modified wood

    No full text
    Wood heat treatment is an attractive alternative to improve decay resistance of wood species with low natural durability. However, this improvement of durability is realized at the expense of the mechanical resistance. Decay resistance and mechanical properties are strongly correlated to thermal degradation of wood cells wall components. Mass loss resulting from this degradation is a good indicator of treatment intensity and final treated wood properties. However, the introduction of a fast and accurate system for measuring this mass loss on an industrial scale is very difficult. Nowadays, many studies are conducted on the determination of control parameters which could be correlated with the treatment conditions and final heat treated wood quality such as decay resistance. The aim of this study is to investigate the relations between kinetics of temperature used during thermal treatment process representing heat treatment intensity, mass losses due to thermal degradation and conferred properties to heat treated wood. It might appear that relative area of treatment temperature curves is a good indicator of treatment intensity. Heat treatment with different treatment conditions (temperature-time) have been performed under vacuum, on four wood species (one hardwood and three softwoods) in order to obtain thermal degradation mass loses of 8, 10 and 12%. For each experiment, relative areas corresponding to temperature kinetics, mass loss, decay resistance and mechanical properties have been determined. Results highlight the statement that the temperature curves’ area constitutes a good indicator in the prediction of needed treatment intensity, to obtain required wood durability and mechanical properties such as bending resistance and Brinell hardnes

    Chemical Composition and Cytotoxic Activity of Eucalyptus torquata Luehm. and Eucalyptus salmonophloia F. Muell. Trunk Bark Essential Oils against Human SW620 and MDA-MB-231 Cancer Cell Lines

    No full text
    In recent years, there has been a growing interest in the screening of natural active ingredients from Eucalyptus essential oils because of their evident importance in practical utility and their undeniable therapeutic properties. Based on this, the aim of the present study was to investigate the chemical profile of the essential oils of the trunk bark of Eucalyptus torquata Luehm. (ETEO), and E. salmonophloia F. Muell. (ESEO), growing in Tunisia. The in vitro cytotoxic properties of the extracted EOs were also evaluated against two human cancer cell lines: breast carcinoma cell lines MDA-MB-231 and colorectal cancer cell lines SW620. The analysis by gas chromatography coupled with mass spectrometry (GC/MS) led to the identification of 32 compounds from the ETEO, with the dominant constituents being the monoterpenes trans-myrtanol (73.4 %) and myrtenol (4.7 %), and the apocarotene (E)-ÎČ-ionone (3.9 %). In the case of ESEO, 29 compounds were identified with trans-myrtanol (25.0 %), decanoic acid (22.1 %), nonanoic acid (9.8 %), Îł-elemene (6.5 %), Îł-maaliene (5.5 %), and α-terpineol (5.3 %) as the main components. The cytotoxicity of EOs against the two chosen cell lines was tested using Crystal Violet Staining (CVS) assay and 5-fluorouracil as a reference drug. The two EOs exhibited a significant dose-dependent inhibition against the viability of the used cell lines. Their inhibitory effects were particularly observed towards SW620 colon carcinoma cells with IC50 values of 26.71±1.22 and 22.21±0.85 ÎŒg/mL, respectively, indicating that both oils were more cytotoxic for SW620 cells compared to MDA-MB-231 one

    Climate change‐induced ecosystem disturbance: a review on sclerophyllous and semi‐deciduous forests in Tunisia

    No full text
    International audienceAccording to the sixth assessment report of the Intergovernmental Panel on Climate Change (IPCC), global climate change is now unequivocal. Tunisia, like many other countries, has been affected by climate changes, including rising temperatures, intense heatwaves, and altered precipitation regimes. Tunisia's mean annual temperatures has risen about +1.4 °C in the twentieth century, with the most rapid warming taking place since the 1970s. Drought represents a primary contributing factor to tree decline and dieback. Long‐term drought can result in reduced growth and health of trees, thereby increasing their susceptibility to insect pests and pathogens. Reported increases in tree mortality point toward accelerating global forest vulnerability under hotter temperatures and longer, more intense droughts. In order to assess the effect of these climate changes on the current state of forest ecosystems in Tunisia and their evolution, an investigative study was required. Here, we review the current state of knowledge on the effects of climate change on sclerophyllous and semi‐deciduous forest ecosystems in Tunisia. Natural disturbance during recent years, as well as the adaptability and resilience of some forest species to climate change, were surveyed. The Standardized Precipitation Evapotranspiration Index (SPEI) is a multi‐scalar drought index based on climate data that has been used to analyse drought variability. The SPEI time scale analysis showed a negative trend over the 1955–2021 period in Tunisian forest regions. In 2021, Tunisia lost 280 km 2 of tree cover to fires, which is equivalent to 26% of the total lost area between 2008 and 2021. Changing climate conditions have also affected phenological parameters, with an advance in the start of the green season (SOS) of 9.4 days, a delay at the end of the green season (EOS) of 5 days, with a consequent extended duration of the green season (LOS) by an average of 14.2 days. All of these alarming findings invite us to seek adaptation strategies for forest ecosystems. Adapting forests to climate change is therefore a challenge for scientists as well as policymakers and managers
    corecore