    Calculation of the stress-strain state of the deflector rollers

    Get PDF
    Numerous studies have established that the damage to the lower surface of hot-rolled strips is mainly due to their friction against rollers of mill rollers. In this case, the probability of scoring, scrapes and other mechanical damage increases otherwise severe wear on the surface of the rollers, improper installation and jamming. This also applies fully to the pulling and forming rollers of the coilers. On modern broadband mills the following measures are used to prevent damage to the surface of hot-rolled strips: reduce the distance between the axes of adjacent rollers; Increase the accuracy installation of rollers in the horizontal plane; apply the individual drive of each roller; provide a smooth increase in the speed rotation of the rollers along the length of the withdrawing roller table; increase the wear resistance of rollers. A prerequisite for preventing damage to the surface of hot-rolled strips is also the maintenance of a high level technical condition of the mill equipment, which includes inspections of wiring armature bars, roller conveyor rollers and other units for each transshipment, timely replacement and repair of individual parts and assemblies (primarily roller conveyors, interroller plates, etc.)

    Study on physical and chemical properties of steel 60С2ХА on a retractable roller conveyor

    Get PDF
    These days, ensuring the high quality of thin products (0,6 – 2,0 mm) is the most promising direction for the development of hot-rolled strip production. Hot-rolled strips can be used in place of a more expensive cold-rolled strip. The effect of cooling modes on quality of hot-rolled metal was observed heating at different temperature, the degree of deformation was observed after cooling by water-air mixture. It was observed that the micro hardness of the samples decreases and the amount of structurally free ferrite increases by decreasing the cooling time and increasing the temperature

    Development of hot rolling technology using the method of physical modeling

    Get PDF
    These days, ensuring the high quality of thin products (0,6 – 2,0 mm) is the most promising direction for the development of hot-rolled strip production. Hot-rolled strips can be used in place of a more expensive cold-rolled strip. The effect of cooling modes on quality of hot-rolled metal was observed heating at different temperature, the degree of deformation was observed after cooling by water-air mixture. It was observed that the micro hardness of the samples decreases and the amount of structurally free ferrite increases by decreasing the cooling time and increasing the temperature

    Development of hot rolling technology using the method of physical modeling

    Get PDF
    These days, ensuring the high quality of thin products (0,6 – 2,0 mm) is the most promising direction for the development of hot-rolled strip production. Hot-rolled strips can be used in place of a more expensive cold-rolled strip. The effect of cooling modes on quality of hot-rolled metal was observed heating at different temperature, the degree of deformation was observed after cooling by water-air mixture. It was observed that the micro hardness of the samples decreases and the amount of structurally free ferrite increases by decreasing the cooling time and increasing the temperature

    Study of stress-strain state of the roller conveyor

    Get PDF
    Numerous studies have established that the damage to the lower surface of hot-rolled strips is mainly due to their friction against rollers of mill rollers. In this case, the probability of scoring, scrapes and other mechanical damage increases otherwise severe wear on the surface of the rollers, improper installation and jamming. This also applies fully to the pulling and forming rollers of the coilers. A prerequisite for preventing damage to the surface of hotrolled strips is also the maintenance of a high level technical condition of the mill equipment, which includes inspections of wiring armature bars, roller conveyor rollers and other units for each transshipment, timely replacement and repair of individual parts and assemblies

    Softening behaviour at hot rolling of FeSi alloys with phase transformation

    Get PDF
    The microstructure of hot rolled strips affects to a large extent the resulting microstructure of the cold rolledand finally annealed FeSi based electrical steels. In this paper the hardening and softening behaviourof FeSi alloys with phase transformation at hot rolling will be regarded. It will be pointed out that the presentmodels describe the processes at hot rolling only in an incomplete way

    Investigation of the stress-strain state of the roller conveyor

    Get PDF
    Numerous studies have established that the damage to the lower surface of hot-rolled strips is mainly due to their friction against rollers of mill rollers. In this case, the probability of scoring, scrapes and other mechanical damage increases otherwise severe wear on the surface of the rollers, improper installation and jamming. This also applies fully to the pulling and forming rollers of the coilers. A prerequisite for preventing damage to the surface of hotrolled strips is also the maintenance of a high level technical condition of the mill equipment, which includes inspections of wiring armature bars, roller conveyor rollers and other units for each transshipment, timely replacement and repair of individual parts and assemblies

    Pickling Behaviour of 2205 Duplex Stainless Steel Hot-rolled Strips in Sulfuric Acid Electrolytes

    Full text link
    Pickling behaviour of the oxide layer on hot-rolled 2205 duplex stainless steel (DSS) was studied in H2SO4 solutions with electrolytic workstation.Comment: 12 pages, 14 figures,3 table