244 research outputs found

    Optimization, Surface Coating and Pilot Research of Li-rich Mn-based Cathode Material for Li-ion Batteries

    Get PDF
    由于层状富锂锰基正极材料xLi2MnO3•(1-x)LiMO2(M=Ni,Co,Mn等)的实际放电比容量高达250mAh/g,且同时具有热稳定性好、成本低以及对环境相对友好等优点,使得该材料成为高比能量锂离子电池正极材料研究的热点之一。然而,尽管富锂锰基材料的放电容量较高,由于其首次充电脱出的Li无法完全回嵌到材料晶格中,导致该材料首次不可逆容量损失较大。另外,富锂锰基材料由于充放电循环时材料结构的不可逆变化及电极/电解液界面膜改变等原因,材料容量和放电电压随循环进行衰退严重,这些问题都严重影响与制约了富锂锰基材料商品化的应用与发展。 本论文对组成为(1-x)LiNi0.4Co0...Due to specific capacity of layered Li-rich Mn-based cathodes xLi2MnO3•(1-x)LiMO2(M = Ni, Co, Mn, and so on)is higher than 250 mAh/g, besides their good thermal stability, low cost and being relative environment-friendly, this kind of cathodes gets many concerns as high specific energy cathodes of Li-ion batteries. Although Li-rich Mn-based cathodes have large discharge capacity, their first...学位:工程硕士院系专业:化学化工学院_工程硕士(化学工程)学号:X201019200

    当代朱熹陈淳研究的新突破——第三届海峡两岸朱熹陈淳学术研讨会综述

    Get PDF
    2016年6月24~25日,由漳州市人民政府、(中国)朱子学会、国际儒联、厦门大学国学院、山东大学儒家文明协同创新中心、山东大学儒学高等研究院、闽南师大闽南文化研究院联合主办的"第三届海峡两岸朱熹陈淳学术研讨会"于漳州召开。来自韩国成均馆大学、外国语大学,日本早稻田大学、埼玉大学,台湾大学、成功大学、辅仁大学、东海大学,北京大学、清华大学、中国人民大学、华东师范大学、中山大学、南开大学、厦门大学等著名高校的百余名专家学者参加会议,

    A new species of Encotyllabe from marine fishes in Minnan-Taiwan Bank,Fujian,China

    Get PDF
    报道了闽南-台湾浅滩野生鱼类真鲷(Pagrosomusmajor)鳃丝上寄生的分室科中柄虫属一新种——厦门中柄虫Encotyllabexiamenensissp.nov.,虫体在体型、体长宽比、大钩和小钩长度比值、小钩的形状、卵黄腺的分布以及卵巢的位置等特征与现有种类存在一定差异,且在卵巢左侧具有发达的肌肉束.A new species of Encotyllabe was reported. The type specimens are deposited in Parasitology Research Laboratory, Xiamen University. Encotyllabe xiamenensis sp. nov. (Plate I). Host: Pagrosomus major. Location: Gill. Locality: Minnan-Taiwan Bank, China. 23.5~24.3 °N, 117.5~118 °E.Body elongate 4.55~5.53 long including opisthaptor, 1.13~1.43 wide. Prohaptor in form of 2 large, frilled lobes, each bearing muscular sucker, 0.17~0.29 in diameter. Eye-spots, 2 pairs. Opisthaptor bell-shaped, aseptate, with plicated marginal membrane, armed with pair of large broad hamuli, pair of minute hamuli and 14 marginal hooklets. Opisthaptor 0.59~0.96 in diameter; large and small hamuli 350~410 μm and 27.5~35 μm long, respectively. Marginal hooklets 10~13.75 μm long. Testes 2, elongate-oval, 0.39~0.45×0.27~0.35. Vas deferens convoluted, winding anteriorly on the left side of body, dorsal to vitelline reservoir, entering base of penis bulb and enlarging inside to form internal seminal vesicle. Large prostatic reservoir outside penis; prostatic duct joins ejaculatory duct proximal to tip of penis bulb. One very stout band of muscle extend anteriorly on left side from level of ovary, joining to the base of penis bulb. Ovary pre-testicular 0.23~0.38 in diameter, with an intra-ovarian seminal vesicle. Uterus extends antero-laterally along dorso-lateral side of penis. Vaginal pore on ventral side at level of vitelline reservoir. Vitellarium extensive, in lateral and median fields, from level of pharynx to near base of peduncle. No eggs were observed.浙江大学医学院中青年科研启动基金

    锂离子电池高镍正极材料掺铝的作用及掺铝方法的研究

    Get PDF
    为了探究铝对高镍层状氧化物在结构、形貌及性能方面的影响,本文采用两种不同的方式掺铝以制备NCA正极材料(Li Ni0.8Co0.15Al0.05O2):一是固相法即将共沉淀合成的NC前驱体(Ni0.84Co0.16(OH)2)在混锂烧结过程混入铝源(纳米Al2O3或Al(NO3)3);二是共沉淀法即直接在合成前驱体过程中混入铝源(Al2(SO4)3或NaAlO2)即合成NCA前驱体(Ni0.8Co0.15Al0.05(OH)2.05)后再混锂烧结.结果表明,掺铝能够降低阳离子混排程度、维持层状结构的稳定性,改善材料在充放电循环过程的放电电压及中值电压大幅下降的情况,提高其循环性能.其中以NaAlO2为铝源合成NCA前驱体所制备的NCA材料性能最优:在3.0~4.3 V充放电区间,0.1C倍率下首圈放电比容量达198 m Ah·g-1,首次库仑效率可达94.6%,1C倍率下循环200圈后容量保持率达70%

    页岩气开发风险及风险治理——两次专题研讨会总结

    Get PDF
    美国页岩气革命使得美国实现了能源自给,带动了全球油气工业的发展,改变了世界能源供应格局。但随着美国页岩气的不断开发,各种风险也逐渐凸显,同时,在相关预算收紧的情况下,管理能力正在下降或变得不完整。在这种背景下,为全面认识与页岩气开发相关的风险及其管理中的一系列社会问题和决策问题,美国国家研究理事会(NRC)成立的指导委员会在2013年的5月和8月分别组织相关专家召开了研讨会,对页岩气开发面临的风险及风险治理问题进行了深入分析。 《页岩气开发风险及风险治理》一书是美国国家研究理事会项目主任保罗&middot;C&middot;斯特恩基于两次专题研讨会上的主题报告人和评论专家等的发言整理而成。该书分为&ldquo;非常规页岩气开发风险&rdquo;和&ldquo;页岩气开发风险治理&rdquo;两大部分、共20章,对页岩气开发风险的讨论主要从公众对页岩气开发风险的态度以及页岩气开发面临的运营风险、水资源风险、空气风险、生态风险、公共健康风险、对气候变化的影响、对开发区的影响、各种风险间相互作用等方面来展开,而对风险治理讨论则涉及管理内容、政府职责、政府能力、管理技术、设立试点区、公众和利益相关者参与、安全文化等方面。这些讨论与认识,对美国和其他页岩气开发国以及计划开发页岩气的国家认识页岩气开发的风险及对其实施有效管理将具有重要的参考意义。</p

    高首效富镍正极材料LiNi0.6Co0.2Mn0.2O2的合成及电化学性能研究

    Get PDF
    采用共沉淀—高温固相烧结的方法合成了富镍正极材料LiNi0.6Co0.2Mn0.2O2(简称NCM622),通过X射线粉末衍射(XRD)/Rietveld精修法、扫描电子显微镜(SEM)及电化学测试,对不同温度下合成材料的结构、形貌、电化学性能进行表征.结果表明,800℃下NCM622阳离子混排程度最低(1.97%),首周库仑效率高达92.2%,100周容量保持率为81.4%.国家自然科学基金项目(No.21233004,No.21428303)资