67,366 research outputs found

    Aspects of SU(3) baryon extrapolation

    Full text link
    We report on a recent chiral extrapolation, based on an SU(3) framework, of octet baryon masses calculated in 2+1-flavour lattice QCD. Here we further clarify the form of the extrapolation, the estimation of the infinite-volume limit, the extracted low-energy constants and the corrections in the strange-quark mass.Comment: 4 pages, 3 figures, pdftex, prepared for the proceedings of CIPANP 09, San Diego, USA, March 26-31, 200

    Silicon-slurry/aluminide coating

    Get PDF
    A low cost coating protects metallic base system substrates from high temperatures, high gas velocity ovidation, thermal fatigue and hot corrosion and is particularly useful fo protecting vanes and blades in aircraft and land based gas turbine engines. A lacquer slurry comprising cellulose nitrate containing high purity silicon powder is sprayed onto the superalloy substrates. The silicon layer is then aluminized to complete the coating. The Si-Al coating is less costly to produce than advanced aluminides and protects the substrates from oxidation and thermal fatigue for a much longer period of time than the conventional aluminide coatings. While more expensive Pt-Al coatings and physical vapor deposited MCrAlY coatings may last longer or provide equal protection on certain substrates, the Si-Al coating exceeded the performance of both types of coatings on certain superalloys in high gas velocity oxidation and thermal fatigue and increased the resistance of certain superalloys to hot corrosion

    Method of protecting a surface with a silicon-slurry/aluminide coating

    Get PDF
    A low cost coating for protecting metallic base system substrates from high temperatures, high gas velocity oxidation, thermal fatigue and hot corrosion is described. The coating is particularly useful for protecting vanes and blades in aircraft and land based gas turbine engines. A lacquer slurry comprising cellulose nitrate containing high purity silicon powder is sprayed onto the superalloy substrates. The silicon layer is then aluminized to complete the coating. The Si-Al coating is less costly to produce than advanced aluminides and protects the substrate from oxidation and thermal fatigue for a much longer period of time than the conventional aluminide coatings. While more expensive Pt-Al coatings and physical vapor deposited MCrAlY coatings may last longer or provide equal protection on certain substrates, the Si-Al coating exceeded the performance of both types of coatings on certain superalloys in high gas velocity oxidation and thermal fatigue. Also, the Si-Al coating increased the resistance of certain superalloys to hot corrosion

    High dispersion observations of Venus during 1972. The CO2 band at 7820 angstrom

    Get PDF
    Photographic plates of Venus which show the spectrum of the carbon dioxide band at 7820A were obtained at Table Mountain Observatory in September-October 1972. These spectra showed a semi-regular 4-day variation in the CO2 abundance over the disk of the planet. Evidence for temporal variations in the rotational temperature of this band and temperature variations over the disk was found. The two quantities, CO2 abundance and temperature, do not show any obvious relationship; however, an increase in the temperature usually is accompanied by a decrease in the abundance of CO2. The average temperature, found from a curve of growth analysis assuming a constant CO2 line of width, is 249 plus or minus 1.4 K (one standard deviation)

    Evaluation of dry lubricants and bearings for spacecraft applications

    Get PDF
    Performance of dry film lubricated ball bearings in high vacuum environmen

    An experimental, low-cost, silicon slurry/aluminide high-temperature coating for superalloys

    Get PDF
    A duplex silicon-slurry/aluminide coating has been developed and cyclically tested in Mach 1 combustion gases for oxidation and thermal fatigue resistance at 1093 C and in Mach 0.3 gases for hot-corrosion resistance at 900 C. The base-metal superalloys were VIA and B-1900. The coated B-1900 specimens performed much better in oxidation than similar specimens coated with aluminides and almost as well as the more-expensive Pt-Al and MCrAlY (where M is Ni and/or Co) coatings deposited by the physical vapor deposition process. The coating also provided good hot-corrosion protection. Metallographic, X-ray, and electron microprobe studies were made to characterize the coating, determine failure mechanisms, and study some of the changes due to exposure

    Experimental study of an independently deflected wingtip mounted on a semispan wing

    Get PDF
    The results of a subsonic wind tunnel test of a semispan wing with an independently deflected tip surface are presented and analyzed. The tip surface was deflected about the quarter chord of the rectangular wing and accounted for 17 percent of the wing semispan. The test was conducted to measure the loads on the tip surface and to investigate the nature of aerodynamic interference effects between the wing and the deflected tip. Results are presented for two swept tip surfaces of similar planform but different airfoil distributions. The report contains plots of tip lift, drag, and pitching moment for various Reynolds numbers and tip deflection angles with respect to the inboard wing. Oil flow visualization photographs for a typical Reynolds number are also included. Important aerodynamic parameters such as lift and pitching moment slopes and tip aerodynamic center location are tabulated. A discussion is presented on the relationship between tip experimental data acquired in a steady flow and the prediction of unsteady tip motion at fixed wing angles of attack

    An experimental, low-cost, silicon-aluminide high-temperature coating for superalloys

    Get PDF
    An evaluation of a duplex silicon-slurry/aluminide coating is presented. The coating is cyclically tested in Mach 1 combustion gases for oxidation and thermal fatigue resistance at 1093 C and in Mach 0.3 gases for hot-corrosion resistance at 900 C. The base metal superalloys are ViA and B-1900. The coated B-1900 specimens performed much better in oxidation than similar specimens coated with aluminides and almost as well as the more expensive Pt-Al and MCrAlY (where M is Ni and/or Co) coatings deposited by the physical vapor deposition process. The coating also provided good hot corrosion protection. Metallographic, X-ray, and electron microprobe studies are used to characterize the coating, determine failure mechanisms, and study some of the changes due to exposure

    Experience with fluorine and its safe use as a propellant

    Get PDF
    The industrial and the propulsion experience with fluorine and its derivatives is surveyed. The hazardous qualities of fluorine and safe handling procedures for the substance are emphasized. Procedures which fulfill the safety requirements during ground operations for handling fluorinated propulsion systems are discussed. Procedures to be implemented for use onboard the Space Transportation System are included

    Neonatal weight loss in breast and formula-fed infants

    Get PDF
    We have observed an increase in the number of breast fed babies presenting with dehydration and/or failure to thrive because of lactation failure and non-recognition of feeding problems. Recent reports1,2 support this experience and recommend monitoring of the weight of infants through the neonatal period. However, these reports acknowledge uncertainty as to what actually constitutes normal neonatal weight loss. Maisels and colleagues published two studies which have been quoted as giving guidance on normal loss. Both studies were designed primarily to study factors that influence breast milk jaundice. The first3 reported a mean weight loss of about 6% in 100 unselected well babies during the first 3 days. The subsequent study4 reported a mean weight loss of 6.86% in 186 infants. The timescale over which babies were weighed was not clearly indicated, although it may have only been 2-3 days. The sample was neither population based nor randomly selected, being largely preselected because of the presence of more pronounced jaundice. The distribution of data points for early neonatal weight loss are likely to be skewed, yet both studies reported the results as mean (SD). Owing to the design and method of data presentation, these studies cannot reliably inform the debate as to what constitutes the norm. Marchini and colleagues published reports also designed primarily to study other issues. One5 indicated a mean early weight loss of 5.7%. Measurements were recorded over a three day period, and no indication is given of the skewness of the data. Another study6 reported a median weight loss of about 6% recorded over a four day period. At least one baby lost > 15% of his/her birth weight during this time, but there is no clear information as to the frequency with which more extreme degrees of weight loss are observed
    • …
    corecore