    Environmental Aging of Scotch-Weld(TradeMark) AF-555M Structural Adhesive in Composite to Composite Bonds

    Get PDF
    Fiber reinforced resin matrix composites have found increased usage in recent years. Due to the lack of service history of these relatively new material systems, their long-term aging performance is not well established. In this study, adhesive bonds were prepared by the secondary bonding of Scotch-Weld(TradeMark) AF-555M between pre-cured adherends comprised of T800H/3900-2 uni-directional laminate. The adherends were co-cured with wet peel-ply for surface preparation. Each bond-line of single-lap-shear (SLS) specimen was measured to determine thickness and inspected visually for voids. A three-year environmental aging plan for the SLS specimens at 82 C and 85% relative humidity was initiated. SLS strengths were measured for both controls and aged specimens at room temperature and 82 C. The aging results of strength retention and failure modes to date are reported

    The Effects of Temperature, Humidity and Aircraft Fluid Exposure on T800H/3900-2 Composites Bonded with AF-555M Adhesive

    Get PDF
    Fiber reinforced resin matrix composites and structural adhesives have found increased usage on commercial and military aircraft in recent years. Due to the lack of service history of these relatively new material systems, their long-term aging performance has not been well established. In this study, single lap shear specimens (SLS) were fabricated by secondary bonding of Scotch-Weld(TradeMark) AF-555M between pre-cured adherends comprised of T800H/3900-2 uni-directional laminates. The adherends were co-cured with wet peel-ply for surface preparation. Each bond-line of the SLS specimen was measured to determine thickness and inspected visually using an optical microscope for voids. A three-year environmental aging plan for the SLS specimens at 82 C (180 F) and 85% relative humidity was initiated. SLS strengths were measured for both controls and aged specimens at room temperature and 82 C. The effect of this exposure on lap shear strength and failure modes to date is reported. In addition, the effects of water, saline water, deicing fluid, JP-5 jet fuel and hydraulic fluid on both the composite material and the adhesive bonds were investigated. The up to date results on the effects of these exposures will be discussed

    Laser-Induced Fabrication of Metallic Interlayers and Patterns in Polyimide Films

    Get PDF
    Self-metallizing polyimide films are created by doping polyamic acid solutions with metallic ions and solubilizing agents. Upon creating a film, the film is exposed to coherent light for a specific time and then cured. The resulting film has been found to have a metallic surface layer and a metallic subsurface layer (interlayer). The layer separating the metallic layer has a uniform dispersion of small metal particulates within the polymer. The layer below the interlayer has larger metal particulates uniformly distributed within the polymer. By varying the intensity or time of exposure to the coherent light, three-dimensional control of metal formation within the film is provided

    Reduced dimer production in solar-simulator-pumped continuous wave iodine lasers based on model simulations and scaling and pumping studies

    Get PDF
    A numerical rate equation model for a continuous wave iodine laser with longitudinally flowing gaseous lasant is validated by approximating two experiments that compare the perfluoroalkyl iodine lasants n-C3F7I and t-C4F9I. The salient feature of the simulations is that the production rate of the dimer (C4F9)2 is reduced by one order of magnitude relative to the dimer (C3F7)2. The model is then used to investigate the kinetic effects of this reduced dimer production, especially how it improves output power. Related parametric and scaling studies are also presented. When dimer production is reduced, more monomer radicals (t-C4F9) are available to combine with iodine ions, thus enhancing depletion of the laser lower level and reducing buildup of the principal quencher, molecular iodine. Fewer iodine molecules result in fewer downward transitions from quenching and more transitions from stimulated emission of lasing photons. Enhanced depletion of the lower level reduces the absorption of lasing photons. The combined result is more lasing photons and proportionally increased output power

    Hazard Calculations of Diffuse Reflected Laser Radiation for the SELENE Program

    No full text
    The hazards from diffuse laser light reflections off water clouds, ice clouds, and fog and from possible specular reflections off ice clouds were assessed with the American National Standards (ANSI Z136.1--1986) for the free-electron-laser parameters under consideration for the Segmented Efficient Laser Emission for NonNuclear Electricity (SELENE) Program. Diffuse laser reflection hazards exist for water cloud surfaces less than 722 m in altitude and ice cloud surfaces less than 850 m in altitude. Specular reflections from ice crystals in cirrus clouds are not probable; however, any specular reflection is a hazard to ground observers. The hazard to the laser operators and any ground observers during heavy fog conditions is of such significant magnitude that the laser should not be operated in fog. Introduction Outdoor laser systems require two additional safety concerns not associated with indoor laser systems: (1) atmospheric scattering and (2) safeviewing distances for specular and ..

    Effects of H2O Vapor on Vibrational Relaxation in Expanding and Contracting Flows

    No full text
    As opposed to previous explanations based on the effects of anharmonicity of simple diatomic molecules, traces of water vapor are suggested to be the most likely cause of the anomalously fast vibrational relaxation of such gases observed in supersonic and hypersonic nozzles. The mechanism is the strong V-VR coupling with H2O molecules that dramatically facilitates the collisional transfer of vibrational energy. Slight moisture content is thus a real world aspect of gas dynamics that must be considered in characterizations of shock tubes, reflected shock tunnels, and expansion tubes

    The Wettability of LaRC Colorless Polyimide Resins on Casting Surfaces

    No full text
    INTRODUCTION Two colorless polyimides developed at NASA Langley Research Center, LaRC^TM-CP1 and LaRC^TM-CP2, are noted for being optically transparent, resistant to radiation, and soluble in the imide form. 1-3 These materials may be used to make transparent, thin polymer films for building large space reflector/collector inflatable antennas, solar arrays, radiometers, etc. Structures such as these require large area, seamless films produced via spin casting or spray coating the soluble imide on a variety of substrates. The ability of the soluble imide to wet and spread over the mandrel or casting substrate is needed information for processing these structures with minimum waste and reprocessing, thereby, reducing the production costs. 4 The wettability of a liquid is reported as the contact angle of the solid/liquid system. 5,6 This fairly simple measurement is complicated by the porosity and the amount of contamination of the