    金属氧化物对油页岩热解产物收率及组成分布的影响

    No full text
    通过固定床反应器,对4种金属氧化物(Al_2O_3、MgO、CaO、Fe_2O_3)对油页岩热解所得油、气产率及成分的影响进行了研究。结果显示,碱性CaO对油、水、气、焦产率分布影响较为突出,可提高页岩油与半焦产率,并降低热解气产率;而酸性较强的Al_2O_3可同时提高页岩油、热解气和热解水的产率,有利于促进挥发分的析出;比较而言,MgO和Fe_2O_3的作用相对较弱。4种金属氧化物均可提高热解气中H_2、CH_4和C2的产率;CaO作用下CO_2含量降低,而其他金属氧化物对CO_2的产生有不同程度的促进作用;Fe_2O_3可促进H_2产生;Al_2O_3作用下CH_4含量有所增加。4种金属氧化物均可促进页岩油中芳香烃的产生,并且CaO和MgO两种碱土金属氧化物作用下,短链(C6~C12)烷烃和烯烃含量均增加,而掺混Al_2O_3时页岩油中仅短链(C6~C12)烷烃含量增加。对此机理进行推测认为,碱性CaO和MgO首先与以脂肪酸形式存在的有机质进行酸碱反应,得到脱羧活性更高的羧酸盐,后者脱羧所得中间产物具有生成烷烃或烯烃两条可能路径,同时得到碳酸盐;而在具有Lewis酸特征的Al_2O_3作用下,脱羧产物为CO_2,并同时得到饱和烃产物。</p

    金属氧化物对油页岩热解产物收率及组成分布的影响

    No full text
    通过固定床反应器,对4种金属氧化物(Al2O3、MgO、CaO、Fe2O3)对油页岩热解所得油、气产率及成分的影响进行了研究。结果显示,碱性CaO对油、水、气、焦产率分布影响较为突出,可提高页岩油与半焦产率,并降低热解气产率;而酸性较强的Al2O3可同时提高页岩油、热解气和热解水的产率,有利于促进挥发分的析出;比较而言,MgO和Fe2O3的作用相对较弱。4种金属氧化物均可提高热解气中H2、CH4和C2的产率;CaO作用下CO2含量降低,而其他金属氧化物对CO2的产生有不同程度的促进作用;Fe2O3可促进H2产生;Al2O3作用下CH4含量有所增加。4种金属氧化物均可促进页岩油中芳香烃的产生,并且CaO和MgO两种碱土金属氧化物作用下,短链(C6-C12)烷烃和烯烃含量均增加,而掺混Al2O3时页岩油中仅短链(C6-C12)烷烃含量增加。对此机理进行推测认为,碱性CaO和MgO首先与以脂肪酸形式存在的有机质进行酸碱反应,得到脱羧活性更高的羧酸盐,后者脱羧所得中间产物具有生成烷烃或烯烃两条可能路径,同时得到碳酸盐;而在具有Lewis酸特征的Al2O3作用下,脱羧产物为CO2,并同时得到饱和烃产物

    页岩灰对油页岩热解特性的影响

    No full text
    以吉林桦甸-公郎头四层油页岩为原料,以掺混SiO_2的油页岩为对比样品,利用热重-红外联用仪考察了页岩灰对油页岩热解特性的影响,通过分析热解固相产物组成变化对热解失重及产物析出规律进行了研究.结果表明,页岩灰对油页岩中的有机质和矿物质失重过程均有促进作用,当页岩灰或SiO_2含量为83%时,在300~600,600~750,750~900℃三个加热温度区间内,掺混页岩灰样品比掺混SiO_2样品的失重率分别提高1.92%, 3.39%和18.99%.低温段有机质热解过程中CO_2先于脂肪烃热解析出,且750℃后CO_2析出峰仅出现在掺混页岩灰的样品中,应为油页岩中难分解的碳酸盐在页岩灰作用下加速分解及页岩灰中CaSO_4与残炭反应共同作用所致

    DISTRIBUTION AND SOURCE of POLYCYCLIC AROMATIC HYDROCARBONS IN THE SURFACE SEDIMENTS of QUANZHOU BAY,CHINA

    No full text
    采用气相色谱-质谱联用(gC-MS)方法,对泉州湾表层沉积物中16种优先控制多环芳烃(PAHS)进行定量分析,采用lMW/HMW、bAA/(bAA+CHr)、InP/(InP+bgP)、PPI等特定比值对PAHS来源进行分析.结果表明,沉积物中PAHS的总含量在182.8—721.1 ng.g-1之间,以3—5环为主;PAHS在表层沉积物中的含量分布总体呈现为泉州湾南岸高于北岸、内湾高于外湾;沉积物中PAHS主要来自高温不完全燃烧.与国内外其它海域相比,泉州湾PAHS处于中等污染水平,该区域表层沉积物中的PAHS对生物不存在明显的毒性效应,但具有潜在的毒副作用.The concentrations of 16 polycyclic aromatic hydrocarbons(PAHs) in the surface sediments of Quanzhou Bay,China,were measured with gas chromatography-mass spectrometry(GC-MS).Source-specific PAHs indexes,including LMW/HMW,BaA/(BaA+Chr),InP/(InP+BgP) and Ppi,were used to identify the potential sources of PAHs in this region.The total contents of PAHs in the sediments were in the range of 182.8—721.1 ng · g-1,which were dominated by PAHs of 3—5 rings.The concentration of PAHs in the Bay was higher in the south bank than in the north bank,and higher in the inner bay than in the outer bay as well.The indexes of source identification indicated that incomplete combustion was the dominant source of PAHs in this study.The pollution of PAHs in the Bay was moderate compared with other regions in the world.PAHs in the surface sediments in this area would not cause remarkably negative effects on marine organisms,but potential negative effects should not be overlooked.海洋公益性行业科研专项(No.200705029)资

    水淬钢渣碳酸化固定CO_2

    No full text
    利用HSC-Chemistry软件平台对以气-液-固三相为基础的水淬钢渣碳酸化固定二氧化碳进行了热力学分析,结果表明,温度700 K以下钢渣主要含钙相在水溶液中能够自发与CO_2反应,碳酸化固定CO_2是可行的;并通过实验研究了反应时间、钢渣粒径、CO_2流量及液固比等主要参数对水淬钢渣碳酸化固定CO_2的影响。结果显示,在初期阶段反应迅速,固碳率在3 h达到27.9%,即固定二氧化碳的能力约为279 kg/t(钢渣),随后逐渐趋于平衡。粒度越细对固碳过程越有利,液固比及CO_2流量影响不明显; XRD及SEM结果也验证了水淬钢渣固定CO_2是可行的

    水淬钢渣碳酸化固定CO_2

    No full text
    利用HSC-Chemistry软件平台对以气-液-固三相为基础的水淬钢渣碳酸化固定二氧化碳进行了热力学分析,结果表明,温度700 K以下钢渣主要含钙相在水溶液中能够自发与CO_2反应,碳酸化固定CO_2是可行的;并通过实验研究了反应时间、钢渣粒径、CO_2流量及液固比等主要参数对水淬钢渣碳酸化固定CO_2的影响。结果显示,在初期阶段反应迅速,固碳率在3 h达到27.9%,即固定二氧化碳的能力约为279 kg/t(钢渣),随后逐渐趋于平衡。粒度越细对固碳过程越有利,液固比及CO_2流量影响不明显; XRD及SEM结果也验证了水淬钢渣固定CO_2是可行的

    水淬钢渣碳酸化固定CO_2

    No full text
    利用HSC-Chemistry软件平台对以气-液-固三相为基础的水淬钢渣碳酸化固定二氧化碳进行了热力学分析,结果表明,温度700 K以下钢渣主要含钙相在水溶液中能够自发与CO_2反应,碳酸化固定CO_2是可行的;并通过实验研究了反应时间、钢渣粒径、CO_2流量及液固比等主要参数对水淬钢渣碳酸化固定CO_2的影响。结果显示,在初期阶段反应迅速,固碳率在3 h达到27.9%,即固定二氧化碳的能力约为279 kg/t(钢渣),随后逐渐趋于平衡。粒度越细对固碳过程越有利,液固比及CO_2流量影响不明显; XRD及SEM结果也验证了水淬钢渣固定CO_2是可行的