    Objective: to analyze the efficiency of prescribed antibiotic therapy in patients with viral and bacterial pneumonia of variable severity in the epidemic and postpandemic periods (October 2009 to February 2011).Subjects and methods. Case histories of 85 patients (mean age, 35.92±13.3 years) were retrospectively analyzed; out of them 31 patients were followed up and treated in intensive care units (ICU). The patients were grouped according to PaO2/FiO2: 1) PaO2/FiO2 >300 (n=54); 2) PaO2/FiO2 <300 (n=26); 3) PaO2/FiO2< 200 (n=5).Results. Regression analysis proved the importance of antimicrobial therapy used in admitted patients hav ing risk factors and PaO2/FiO2 > 300. Bacteriological followup revealed that all the patients who had PaO2/FiO2 <200 and died in ICU had been nosocomially reinfected with polyresistant microorganisms and targeted antimicrobial therapy could not be per formed.Conclusion. Early antibiotic therapy in patients with PaO2/FiO2 >300 and risk factors improves the prognosis of the dis ease. All the patients who have PaO2/FiO2 >300 and are ineffectively treated for antibacterial pneumonia should undergo follow up analysis of bronchoalveolar lavage to be switched to targeted antibiotic therapy. The patients who have PaO2/FiO2< 200 are at the highest risk for nosocomial reinfection and pose difficulties in choosing adequate antibiotic therapy. There is a significant relationship between the detection of polyresistant microorganisms and ICU mortality rates.Цель. Анализ эффективности назначенной антибактериальной терапии у больных вирусно-бактериальной пневмонией с разной степенью тяжести в эпидемический и постпандемический период (октябрь 2009 — февраль 2011 года).Материалы и методы. Проведен ретроспективный анализ 85 историй болезни пациентов с средним возрастом 35,92±13,3 года, из которых — 31 наблюдался и проходил лечение в условиях ОРИТ. Деление пациентов на группы произведено по критерию PaO2/FiO2: PaO2/FiO2 >300: 54 пациента; PaO2/FiO2 <300: 26 пациентов; PaO2/FiO2 < 200: 5 пациентов.Результаты. Методом регрессионного анализа доказана важность использования антибактериальной терапии у поступивших пациентов, отягощенных факторами риска с уровнем PaO2/FiO2>300. Исходя из результатов динамического бактериологического исследования, у всех пациентов с PaO2/FiO2< 200 c летальным исходом в условиях ОРИТ выявлен факт внутригоспитальной реинфекции полирезистентной микрофлорой с невозможностью осуществления целенаправленной антибактериальной терапии.Заключение. Раннее использование антибактериальной терапии у пациентов с PaO2/FiO2 >300, отягощенных факторами риска улучшает прогноз заболевания. У всех пациентов с PaO2/FiO2< 300 при неэффективности антибактериальной пневмонии следует проводить динамический анализ бронхо-альвеолярного лаважного содержимого с переходом на целенаправленную антибактериальную терапию. У пациентов с PaO2/FiO2< 200 существует максимально высокий риск нозокомиального реинфицирования с трудностями подбора адекватной антибактериальной терапии. Прослеживается достоверная взаимосвязь выявления полирезистентной флоры и летальностью в условиях ОРИТ

    Влияние автооблучения на формирование наноразмерных слоев золота при ионно-лучевом напылении

    Get PDF
    2–13 nm gold films were obtained by the method of ion-beam sputtering on silicon and quartz substrates. It is shown that the use of an additional operation of deposition followed by the sputtering of a gold layer of 2–3 nm thickness makes it possible to reduce the electrical resistance and surface roughness of the metal films, in comparison with similar films obtained without its use. The results of measuring the temperature coefficient of resistance of nanosized gold films on silicon substrates allowed us to conclude that the films deposited become continuous at a thickness of 6-8 nm. The results of optical measurements of 10 nm gold films, obtained on quartz substrates, showed that the reflection coefficient of electromagnetic radiation at a wavelength of 850 nm is 2.8 % higher than the corresponding coefficient for the same films obtained without using this operation, and is 83 %. An important role in the formation of nanoscale gold layers is played by the processes of self-irradiation of the growing layer of the high-energy component of the gold atoms flux. When using an additional operation of deposition/sputtering, high-energy gold atoms are implanted into the substrate to a depth of about 2 nm. On the one hand, these atoms are point defects in the surface damaged layer of the substrate; on the other hand, they serve as additional centers of cluster formation. This ensures strong adhesion of the metal layer to the substrate and, therefore, the gold films become continuous and more homogeneous in microstructure. The method of ion-beam deposition can be successfully applied to obtain high-quality conductive optically transparent nanosized gold films.Методом ионно-лучевого напыления получены пленки золота толщиной 2–13 нм на кремниевых и кварцевых подложках. Показано, что применение дополнительной операции напыления с последующим распылением слоя золота толщиной 2–3 нм позволяет снизить электрическое сопротивление и поверхностную шероховатость получаемых металлических пленок по сравнению с аналогичными пленками, полученными без ее использования. Результаты измерения температурного коэффициента сопротивления образцов наноразмерных пленок золота на кремниевых подложках позволили заключить, что напыляемые пленки становятся сплошными при толщине 6–8 нм. Результаты оптических измерений пленок золота толщиной 10 нм, полученных на кварцевых подложках, показали, что коэффициент отражения электромагнитного излучения на длине волны 850 нм на 2,8 % выше соответствующего коэффициента для таких же пленок, полученных без использования данной операции, и составляет 83 %. Важную роль в формировании наноразмерных слоев золота играют процессы автооблучения растущего слоя высокоэнергетической составляющей потока атомов золота. При использовании дополнительной операции напыления/распыления происходит внедрение в подложку высокоэнергетических атомов золота на глубину до 2 нм. С одной стороны, эти атомы являются источниками точечных дефектов в приповерхностном нарушенном слое подложки; а с другой – они служат дополнительными центрами кластерообразования. За счет этого обеспечивается высокая адгезия слоя металла к подложке, и, как следствие, пленки золота становятся сплошными и более однородными по микроструктуре. Метод ионно-лучевого напыления может быть успешно применен для получения качественных проводящих оптически прозрачных наноразмерных пленок золота

    Применение барьерных слоев диоксида титана для формирования мультиферроиков ферромагнетик/сегнетоэлектрик

    Get PDF
    The layered multiferroics Co/PZT were obtained by ion-beam sputtering-deposition method, where PZT is a ferroelectric ceramic based on lead titanate zirconate of the composition PbZr0.45Ti0.55O3 with a thermostable plane-parallel ferroelectric/ferromagnet interface. Using cross-sectional scanning electron microscopy (SEM), we studied the interface of a cobalt layer up to several micrometers thick with a thick ceramic substrate of lead zirconate titanate. It has been shown that the use of a titanium dioxide barrier layer of TiO2 instead of PZT allows quality improvement of the interface by reducing the duration of ion-beam planarization of the ferroelectric substrate, and also to eliminate the formation of intermediate chemical compounds. Based on the data of X-ray phase analysis (XRD), it was concluded that the TiO2 layer is amorphous. Magnetoelectric measurements have shown that the use of titanium dioxide instead of PZT under appropriate planarization modes can increase the low-frequency magnetoelectric effect to 5 mV/(cm∙Ое), compared with structures with a sputtering planarizing layer of PZT, where the magnitude of the low-frequency magnetoelectric effect is 2 mV/(cm∙Оe). These results allow us to improve the characteristics of these structures when used as sensitive elements in devices for formation – processing of information and magnetic field sensors based on the magnetoelectric effect.С помощью метода ионно-лучевого распыления – осаждения получены слоистые мультиферроики Co/ЦТС (ЦТС – сегнетоэлектрическая керамика на основе цирконата титаната свинца состава PbZr0,45Ti0,55O3 с термостабильным плоскопараллельным интерфейсом сегнетоэлектрик/ферромагнетик), обладающие воспроизводимыми низкочастотными магнитоэлектрическими характеристиками при комнатной температуре. Методом растровой электронной микроскопии (РЭМ) поперечного сечения исследована граница раздела слоя кобальта толщиной до нескольких микрометров с толстой керамической подложкой цирконата – титаната свинца. Показано, что использование барьерного слоя диоксида титана TiO2 вместо ЦТС позволяет добиться улучшения качества интерфейса за счет уменьшения длительности ионно-лучевой планаризации сегнетоэлектрической подложки, а также исключить образование промежуточных химических соединений. На основе данных рентгенофазового анализа (РФА) сделан вывод об аморфности слоя TiO2, который по сравнению с кристаллическим позволяет более равномерно, без искажений, передавать внутренние напряжения, возникающие между сегнетоэлектрической подложкой и ферромагнитным слоем. Это приводит к более эффективному магнитоэлектрическому взаимодействию и значительному по величине (в единицы – десятки мВ/А) низкочастотному магнитоэлектрическому эффекту при комнатной температуре. Магнитоэлектрические измерения показали, что использование диоксида титана вместо ЦТС при соответствующих режимах планаризации приводит к увеличению низкочастотного магнитоэлектрического эффекта до 5 мВ/(см ∙Э) по сравнению со структурами с напылением планаризующего слоя ЦТС, где величина данного эффекта составляет 2 мВ/(см ∙Э). Эти результаты позволяют улучшить характеристики указанных структур при использовании в качестве чувствительных элементов в устройствах формирования – обработки информации и датчиков магнитного поля на основе магнитоэлектрического эффекта

    Phase Behavior of Aqueous Na-K-Mg-Ca-CI-NO3 Mixtures: Isopiestic Measurements and Thermodynamic Modeling

    Get PDF
    A comprehensive model has been established for calculating thermodynamic properties of multicomponent aqueous systems containing the Na{sup +}, K{sup +}, Mg{sup 2+}, Ca{sup 2+}, Cl{sup -}, and NO{sub 3}{sup -} ions. The thermodynamic framework is based on a previously developed model for mixed-solvent electrolyte solutions. The framework has been designed to reproduce the properties of salt solutions at temperatures ranging from the freezing point to 300 C and concentrations ranging from infinite dilution to the fused salt limit. The model has been parameterized using a combination of an extensive literature database and new isopiestic measurements for thirteen salt mixtures at 140 C. The measurements have been performed using Oak Ridge National Laboratory's (ORNL) previously designed gravimetric isopiestic apparatus, which makes it possible to detect solid phase precipitation. Water activities are reported for mixtures with a fixed ratio of salts as a function of the total apparent salt mole fraction. The isopiestic measurements reported here simultaneously reflect two fundamental properties of the system, i.e., the activity of water as a function of solution concentration and the occurrence of solid-liquid transitions. The thermodynamic model accurately reproduces the new isopiestic data as well as literature data for binary, ternary and higher-order subsystems. Because of its high accuracy in calculating vapor-liquid and solid-liquid equilibria, the model is suitable for studying deliquescence behavior of multicomponent salt systems

    Controlled Growth of Co Nanofilms on Si(100) by Ion-Beam puttering

    No full text
    International audienceThe effect of process conditions on the properties of cobalt films grown on silicon by ion-beam sputtering is analyzed from the nucleation stage to film thicknesses corresponding to the properties of bulk material. The argon ion energy is shown to play a central role in determining the sputtering process. Sputtering a cobalt target with argon ions less than 0.8 keV in energy produces granular layers. The cobalt layers grown at argon ion energies above 1.2 keV are continuous even in the nucleation stage. The layers 1.2 to 2 nm in thickness have high resistivity and are comparable in magnetic properties to bulk material. The high-energy component of the total flux of cobalt atoms ejected from the target plays an important role in the initial stages of deposition, especially at argon ion energies from 1.2 to 2.2 keV. In the nucleation stage, the energy deposited by cobalt atoms in the silicon substrate facilitates the formation of a continuous layer in the initial stage of the process

    A New Approach to the Formation of Nanosized Gold and Beryllium Films by Ion-Beam Sputtering Deposition

    No full text
    Thin films of beryllium and gold that are several tens of nanometers thick were obtained, for the first time, on silicon and quartz substrates by the ion-beam method with tenfold alternation of deposition and partial sputtering of the nanosized metal layer. Scanning electron and atomic force microscopy indicate the predominant lateral growth of nanosized metal layers along the substrate surface. Optical spectra indicate the suppression of the localized plasmon resonance. The growth of the film occurs under the influence of the high-energy component of the sputtered metal atoms’ flux. The main role in the formation of the nanosized metal film is played by the processes of the elastic collision of incident metal atoms with the atoms of a substrate and a growing metal film. Metal films that are obtained by the tenfold application of the deposition–sputtering of a nanoscale metal layer are characterized by stronger adhesion to the substrate and have better morphological, electrical, and optical characteristics than those that are obtained by means of direct single deposition