    Spin and lattice excitations of a BiFeO3 thin film and ceramics

    Full text link
    We present a comprehensive study of polar and magnetic excitations in BiFeO3 ceramics and a thin film epitaxially grown on an orthorhombic (110) TbScO3 substrate. Infrared reflectivity spectroscopy was performed at temperatures from 5 to 900 K for the ceramics and below room temperature for the thin film. All 13 polar phonons allowed by the factor-group analysis were observed in theceramic samples. The thin-film spectra revealed 12 phonon modes only and an additional weak excitation, probably of spin origin. On heating towards the ferroelectric phase transition near 1100 K, some phonons soften, leading to an increase in the static permittivity. In the ceramics, terahertz transmission spectra show five low-energy magnetic excitations including two which were not previously known to be infrared active; at 5 K, their frequencies are 53 and 56 cm-1. Heating induces softening of all magnetic modes. At a temperature of 5 K, applying an external magnetic field of up to 7 T irreversibly alters the intensities of some of these modes. The frequencies of the observed spin excitations provide support for the recently developed complex model of magnetic interactions in BiFeO3 (R.S. Fishman, Phys. Rev. B 87, 224419 (2013)). The simultaneous infrared and Raman activity of the spin excitations is consistent with their assignment to electromagnons

    Anisotropy in the magnetic interaction and lattice-orbital coupling of single crystal Ni3TeO6

    Get PDF
    [[abstract]]This investigation reports on anisotropy in the magnetic interaction, lattice-orbital coupling and degree of phonon softening in single crystal Ni3TeO6 (NTO) using temperature- and polarization-dependent X-ray absorption spectroscopic techniques. The magnetic field-cooled and zero-field-cooled measurements and temperature-dependent Ni L3,2-edge X-ray magnetic circular dichroism spectra of NTO reveal a weak Ni-Ni ferromagnetic interaction close to ~60 K (TSO: temperature of the onset of spin ordering) with a net alignment of Ni spins (the uncompensated components of the Ni moments) along the crystallographic c-axis, which is absent from the ab-plane. Below the Néel temperature, TN~ 52 K, NTO is stable in the antiferromagnetic state with its spin axis parallel to the c-axis. The Ni L3,2-edge X-ray linear dichroism results indicate that above TSO, the Ni 3d eg electrons preferentially occupy the out-of-plane 3d3z2−r2 orbitals and switch to the in-plane 3dx2−y2 orbitals below TSO. The inherent distortion of the NiO6 octahedra and anisotropic nearest-neighbor Ni-O bond lengths between the c-axis and the ab-plane of NTO, followed by anomalous Debye-Waller factors and orbital-lattice in conjunction with spin-phonon couplings, stabilize the occupied out-of-plane (3d3z2−r2) and in-plane (3dx2−y2) Ni eg orbitals above and below TSO, respectively.[[notice]]補正完
    corecore