    Avances en flotación columnar

    Get PDF
    Column flotation is particularly attractive for applications involving multiple cleaning stages in conventional cells and for complex minerals that have selectivity problems, substantially raising the grade of the concentrate (2-4%) and higher recovery (2-3%) , with a single cleaning stage, this equipment adapting very well to computer control. Its acceptance in the mining industry is increasing due to multiple advantages including lower cost of installation and operation, less space occupation, substantial decrease in energy consumption, mainly because it does not have a mechanical agitation system, and less consumption of reagents.La flotación en columna es particularmente atractiva para aplicaciones que implican múltiples etapas de limpieza en celdas convencionales y para minerales complejos que presentan problemas de selectividad, elevando sustancialmente el grado del concentrado (2-4%) y de mayor recuperación (2-3 %), con una sola etapa de limpieza, adaptándose muy bien este equipo al control por computadora. Su aceptación en la industria minera está incrementándose debido a múltiples ventajas que incluyen menor costo de instalación y operación, menor ocupación de espacio, disminución sustancial del consumo de energía, principalmente porque no tiene sistema de agitación mecánica, y menor consumo de reactivos

    El problema de la activación natural de la esfalerita durante la flotación selectiva

    Get PDF
    The natural activation of sphalerite during flotation of lead is mainly related to the contamination of lead concentrate. The high content of zinc in the lead concentrate receives economic sanctions by higher refining costs, plus zinc content decreases in its flotation circuit. This research has been conducted on five samples of different minerals to identify the probable causes activation of natural sphalerite. The results indicate that the causes are intergrowths Mineralogical between lead and zinc, and the presence of soluble salts of Cu2 +. The ferrous ions and ferric Fe2 + Fe3 + did not show a significant effect on the activation of sphalerite.La activación natural de la esfalerita durante la flotación del plomo está relacionada principalmente a la contaminación del concentrado de plomo. El alto contenido de zinc en el concentrado de plomo recibe castigos económicos por mayores costos en refinación, además disminuye el contenido de zinc en su circuito de flotación. Esta investigación se ha realizado con cinco muestras de minerales diferentes para identificar las probables causas de activación natural de la esfalerita. Los resultados indican que las causas son intercrecimientos mineralógicos entre el plomo y zinc, y presencia de sales solubles de Cu2+. Los iones ferrosos Fe2+ y férrico Fe3+ no muestran un efecto importante en la activación de la esfalerita

    Tratamiento hidrometalúrgico del oro diseminado en pirita y arsenopirita

    Get PDF
    The ore is complex and presents abundant content of sulphurs: pyrite, arsenopyrite and pyrrhotite, also in few proportion: chalcopyrite, sphalerite and probably sulfhosals that add: copper, silver, arsenic and antimony. Free gold is not appreciated in the obtained results, the major content of gold is in tails of flotation Cu-Ag, constituted by sulphurs of iron, as a non metallic residue prevails the quartz, coal and the insolubles, it is quite strong and naturally very acid, pH:5.3. It is possible to obtain a concentrate of flotation Cu-Ag, with As and Sb like pollutants and around 80% of the total gold stays in tails, to which we effect a direct cyanidation having variant like pH and granulometry, it has not been possible to leach more than 11 % of the gold contained in tails that gives 3.2 grams Au/TM, considering the current prices it has an approximate value 100 US Ton.Elmineralescomplejo,presentaabundantecontenidodesulfuros:pirita,arsenopiritaypirrotita,enmenoresproporciones:calcopirita,esfaleritayprobablementesulfosalesqueaportan:cobre,plata,arseˊnicoyantimonio,noseapreciaorolibre:Porlosresultadosobtenidos,elmayorcontenidodeoroestaˊenelrelavedeflotacioˊnCuAg,constituidoporsulfurosdefierro,comoganganometaˊlicaprevaleceelcuarzo,carboˊneinsolubles,esmuyduro,naturalmentemuyaˊcido,pH:5.3.EsposibleobtenerunconcentradodeflotacioˊnCuAg,conAsySbcomocontaminantesyalrededordel80 Ton.El mineral es complejo, presenta abundante contenido de sulfuros: pirita, arsenopirita y pirrotita, en menores proporciones: calcopirita, esfalerita y probablemente sulfosales que aportan: cobre, plata, arsénico y antimonio, no se aprecia oro libre: Por los resultados obtenidos, el mayor contenido de oro está en el relave de flotación Cu-Ag, constituido por sulfuros de fierro, como ganga no metálica prevalece el cuarzo, carbón e insolubles, es muy duro, naturalmente muy ácido, pH:5.3. Es posible obtener un concentrado de flotación Cu-Ag, con As y Sb como contaminantes y alrededor del 80% del oro total queda en el relave, al cual efectuamos una cianuración directa teniendo como variables pH y granulometría. No se ha logrado lixiviar más del 11% del oro contenido en el relave que ensaya 3.2 gramos Au/TM, considerando los precios actuales tiene un valor aproximado 100 por tonelad

    Flotación y concentración de minerales de manganeso: MnO2

    Get PDF
    The ores of manganese are difficult to concentrate, nevertheless in this study of research, it has been achieved to raise the grade of manganese applying different equipments, machines, flow charts and diverse chemical reagents of flotation, obtaining the best results by means of flotation of the gangue, being the tail the concentrate of manganeso. The original ore has 23,8% Mn, on having it concentrate by inverse flotation, one manages to obtain 47,50% Mn in the concentrate, product very quoted on the intermal and external market.Los minerales de manganeso son difíciles de concentrar, no obstante, en este estudio de investigación se ha logrado elevar la ley del manganeso aplicando diferentes equipos, máquinas, diagramas de flujo y diversos reactivos químicos de flotación, obteniendo los mejores resultados mediante flotación de la ganga siendo el relave el concentrado de manganeso. El mineral original tiene 23,8% de Mn, al concentrarlo por flotación inversa se llega a obtener 47,50% Mn en el concentrado; producto muy cotizado en el mercado interno y externo

    Flotatión and recovery of fluorite of a polysulfhide ore of seal with lead-silver-zinc-iron

    Get PDF
    La fluorita (F2Ca) es un mineral que tiene múltiples aplicaciones, las principales son: fabricación de ácido fluorhídrico, industria siderúrgica, soldadura y ornamental. El mineral estudiado pertenece a la zona central del Perú, además de fluorita tiene valores metálicos de plomo, plata y zinc que responden bien a la flotación diferencial de sulfuros con buenos resultados en la calidad de los concentrados y altas recuperaciones. El concentrado de fluorita obtenido es de grado cerámico, no se logra obtener fluorita de grado ácido por la probable presencia de fluoruros de aluminio que están afectando la calidad del concentrado.Fluorite (F2Ca) is an ore that has multiple aplications, the main ones are: manufacture of fluorhidric acid, steel iron industry, welding and ornamental purposes. This ore belongs to the central zone of Peru and besides fluorite, it has metallic values of lead, silver and zinc, these respond well to differential flotation of sulfhur with good results in the quality of the concentrates and high recoveries. The obtained fluorite concentrate is of ceramic degree, fluorite of acid degree ca not be obtained because of the presence of Aluminium fluorides that affect the quality of the concentrate

    Flotación de minerales oxidados de plomo

    Get PDF
    The main oxidized lead minerals are: cerussite and anglesite, which due to their crystallography and wettability should not be buoyant, for this reason it is necessary to study the flotation properties for these minerals, the main ones are: solubility, surface physico-chemical , thermodynamics, fines content and others, it is concluded that anglesite is less buoyant than cerussite, both can be floated directly with amyl xanthate: long-chain hydrocarbon collector and cationic collectors such as alamine 26-D. The flotation of oxides improves when they are previously sulfurized before adding xanthate type collector, obtaining economically acceptable results. The above is applied to a polymetallic mineral of galena, sphalerite and cerussite; up to four flow charts are discussed, two are experimented, and with the bulk flotation scheme Pb-Zn, followed by flotation of oxides, after sulfurization with sodium sulfide excellent results are obtained, taking into account the complexity of the mineral.Los principales minerales oxidados de plomo son: cerusita y anglesita, los que debido a su cristalografía y mojabilidad no deberían ser flotables, por esta razón es necesario estudiar las propiedades de flotación para estos minerales, las principales son: solubilidad, físico-química de superficie, termodinámica, contenido de finos y otros, se concluye que la anglesita es menos flotable que la cerusita, ambas se pueden flotar directamente con xantato amílico: colector de cadena larga de hidrocarburo y colectores catiónicos como el alamine 26-D. La flotación de óxidos mejora cuando se sulfurizan previamente antes de adicionar colector tipo xantato, obteniéndose resultados económicamente aceptables. Lo anteriormente expuesto lo aplicamos a un mineral polimetálico de galena, esfalerita y cerusita; se discute hasta cuatro diagramas de flujo, se experimenta dos, y con el esquema de flotación bulk Pb-Zn, seguida de flotación de óxidos, previa sulfurización con sulfuro de sodio se obtienen excelentes resultados, teniendo en cuenta la complejidad del mineral

    Disminución del contenido de azufre en carbón mineral,mediante procesos metalúrgicos para uso industrial

    Get PDF
    The sample that is the object of this research work is a kind of bituminous coal, from the Mount Huáscar, province of Oyón, department of Lima. Provided by the Coal Mine Company. The mineralogical characterization of the sample coal, to show the presence of the following minerals: Graphite (grf) and Pyrite (py). The percentage distribution indicates graphite and 96,91% 3,09% pyrite, the particles are mostly free, accordingly modal analysis indicates that the degree of liberation of graphite and pyrite is 100%, that is counted all particles are free, as can be seen in the photos N.º 1, 2 ,3 and 4. Based on the characterization done it can be concluded that sulfur is in the pyrite, which is the polluter coal. Metallurgical tests were conducted preliminary gravity and flotation; being the outcome of the gravity is not satisfactory. The three tests metallurgical more representative of flotation process, concentrate obtained indicate that the low percentage of ash in 62,8% improves the percentage of fixed carbon in 19,2% and increases the calorific power at 12,2% compared with the original coal (head); this indicates that improves the quality of coal. As for the decrease in the percentage of sulphur the best test selected is No. 3, where low of 2,32% to 1,37%. Also more time milling notes that the particles of pyrite are already beginning to rise in concentrate.La muestra, que es materia del presente trabajo de investigación, es un carbón mineral de tipo bituminoso, procedente del Cerro Huáscar, provincia de Oyón, departamento de Lima. Proporcionado por la Compañía Coal Mine Company. La caracterización mineralógica de la muestra de carbón arroja la presencia de los siguientes minerales: Grafito (grf) y Pirita (py). La distribución porcentual indica 96,91% de grafito y 3,09% de pirita, las partículas mayormente están libres, en consecuencia el análisis modal indica que el grado de liberación del grafito y pirita es de 100%; es decir todas las partículas contadas están libres, como se puede observar en las figuras Nº 1, 2, 3 y 4 . En base a la caracterización realizada se puede concluir que el azufre se encuentra en la pirita, que es el que contamina el carbón. Se realizaron pruebas metalúrgicas preliminares de gravimetría y flotación; siendo los resultados de la gravimetría no satisfactorios. Las tres pruebas metalúrgicas del proceso de flotación más representativas indican que en el concentrado obtenido baja el porcentaje de cenizas en 62,8%, mejora el % de carbón fijo en 19,2% y se incrementa el poder calorífico en 12,2% comparado con el carbón original (cabeza); esto indica que mejora la calidad del carbón. En cuanto a la disminución del porcentaje de azufre la mejor prueba seleccionada es la Nº 3, donde baja de 2,32% a 1,37%. También se concluye que a mayor tiempo de molienda se observa que las partículas de pirita ya empiezan a levantarse en el concentrado

    Factores que afectan la selección del proceso metalúrgico para beneficiar minerales complejos de oro

    Get PDF
    The need to develop and know methods for metallurgical treatment to process gold-bearing refractory minerals or hard to treat be- cause of carbon contents, tellurium, antimony, arsenic, carbonates and gold in solution solid sulfides, forces us to study the different methods of specific oxidation that should be applied in each mineral before to leach ore to reach high recoveries into precious metals Through Gravimetrically followed by cyanidation is obtained 94.74% of gold extract in the studied mineral.La necesidad de desarrollar y conocer métodos de tratamiento metalúrgico para beneficiar minerales auríferos refractarios o difíciles de tratar por presentar contenidos de carbón, teluros, antimonio, arsénico, carbonatos y oro en solución sólida en sulfuros, nos obliga a estudiar los diversos métodos de oxidación específica que se deben aplicar a cada mineral previo a lixiviar para alcanzar altas recuperaciones en metales preciosos. Por gravimetría seguida de cianuración, se obtiene 94.74% de extracción de oro en el mineral estudiado

    Association Between Preexisting Versus Newly Identified Atrial Fibrillation and Outcomes of Patients With Acute Pulmonary Embolism

    Get PDF
    Background Atrial fibrillation (AF) may exist before or occur early in the course of pulmonary embolism (PE). We determined the PE outcomes based on the presence and timing of AF. Methods and Results Using the data from a multicenter PE registry, we identified 3 groups: (1) those with preexisting AF, (2) patients with new AF within 2 days from acute PE (incident AF), and (3) patients without AF. We assessed the 90-day and 1-year risk of mortality and stroke in patients with AF, compared with those without AF (reference group). Among 16 497 patients with PE, 792 had preexisting AF. These patients had increased odds of 90-day all-cause (odds ratio [OR], 2.81; 95% CI, 2.33-3.38) and PE-related mortality (OR, 2.38; 95% CI, 1.37-4.14) and increased 1-year hazard for ischemic stroke (hazard ratio, 5.48; 95% CI, 3.10-9.69) compared with those without AF. After multivariable adjustment, preexisting AF was associated with significantly increased odds of all-cause mortality (OR, 1.91; 95% CI, 1.57-2.32) but not PE-related mortality (OR, 1.50; 95% CI, 0.85-2.66). Among 16 497 patients with PE, 445 developed new incident AF within 2 days of acute PE. Incident AF was associated with increased odds of 90-day all-cause (OR, 2.28; 95% CI, 1.75-2.97) and PE-related (OR, 3.64; 95% CI, 2.01-6.59) mortality but not stroke. Findings were similar in multivariable analyses. Conclusions In patients with acute symptomatic PE, both preexisting AF and incident AF predict adverse clinical outcomes. The type of adverse outcomes may differ depending on the timing of AF onset.info:eu-repo/semantics/publishedVersio
    corecore