5,622 research outputs found

    Optimization of Laser Beam Transformation Hardening by One Single Parameter

    Get PDF
    The process of laser beam transformation hardening is principally controlled by two independent parameters, the absorbed laser power on a given area and the interaction time. These parameters can be transformed into two functional parameters: the maximum surface temperature and the hardening depth.\ud \ud It has been proved that with a constant hardening depth the results hardness. residual stress. etc.) can be optimized easily with respect to only one independent parameter, the maximum surface temperature. which is applied directly in adaptive control strategies

    Role of magnetic and orbital ordering at the metal-insulator transition in NdNiO3

    Full text link
    Soft x-ray resonant scattering at the Ni L2,3 edges is used to test models of magnetic and orbital-ordering below the metal-insulator transition in NdNiO3. The large branching ratio of the L3 to L2 intensities of the (1/2,0,1/2) reflection and the observed azimuthal angle and polarization dependence originates from a non collinear magnetic structure. The absence of an orbital signal and the non collinear magnetic structure show that the nickelates are materials for which orbital ordering is absent at the metal-insulator transition.Comment: 10 pages, 4 figures, Physical Review B rapid communication, to be publishe

    Fabrication and electrical transport properties of embedded graphite microwires in a diamond matrix

    Full text link
    Micrometer width and nanometer thick wires with different shapes were produced \approx 3~\upmum below the surface of a diamond crystal using a microbeam of He+^+ ions with 1.8~MeV energy. Initial samples are amorphous and after annealing at T1475T\approx 1475~K, the wires crystallized into a graphite-like structures, according to confocal Raman spectroscopy measurements. The electrical resistivity at room temperature is only one order of magnitude larger than the in-plane resistivity of highly oriented pyrolytic bulk graphite and shows a small resistivity ratio(ρ(2K)/ρ(315K)1.275\rho(2{\rm K})/\rho(315{\rm K}) \approx 1.275). A small negative magnetoresistance below T=200T=200~K was measured and can be well understood taking spin-dependent scattering processes into account. The used method provides the means to design and produce millimeter to micrometer sized conducting circuits with arbitrary shape embedded in a diamond matrix.Comment: 12 pages, 5 figures, to be published in Journal of Physics D: Applied Physics (Feb. 2017