36 research outputs found

    Bonding shear strength in timber and GFRP glued with epoxy adhesives

    Get PDF
    The bonding quality of epoxy glued timber and glass fibre reinforced polymers (GFRP) was evaluated by means of compression loading shear test. Three timber species (Radiata pine, Laricio pine and Oak) and two kinds of GFRP (plates and rods made with polyester resin reinforced with mat and roving glass fibre) were glued and tested using three epoxy formulations. The increase in shear strength with age after the setting of epoxy formulations and the effect of surface roughness on timber and GRP gluing (the planing of the surface of timber and the previous sanding of GRP) were studied. It can be concluded that the mechanical properties of these products make them suitable for use in the reinforcement of deteriorated timber structures, and that a rough timber surface is preferable to a planed one, while the previous sanding of GRP surfaces is not advantageous

    Analysis of the stress state of a halved and tabled traditional timber scarf joint with the Finite Element Method

    Get PDF
    The purpose of this study is to determine the stress distribution in the carpentry joint of halved and tabled scarf joint with the finite element method (FEM) and its comparison with the values obtained using the theory of Strength of Materials. The stress concentration areas where analyzed and the influence of mesh refinement was studied on the results in order to determine the mesh size that provides the stress values more consistent with the theory. In areas where stress concentration is lower, different mesh sizes show similar stress values. In areas where stress concentration occurs, the same values increase considerably with the refinement of the mesh. The results show a central symmetry of the isobar lines distribution where the centre of symmetry corresponds to the geometric centre of the joint. Comparison of normal stress levels obtained by the FEM and the classical theory shows small differences, except at points of stress concentration

    In situ acoustic methods to estimate the physical and mechanical aging of oriented strand board

    Full text link
    Following the success achieved in previous research projects usin non-destructive methods to estimate the physical and mechanical aging of particle and fibre boards, this paper studies the relationships between aging, physical and mechanical changes, using non-destructive measurements of oriented strand board (OSB). 184 pieces of OSB board from a French source were tested to analyze its actual physical and mechanical properties. The same properties were estimated using acoustic non-destructive methods (ultrasound and stress wave velocity) during a physical laboratory aging test. Measurements were recorded of propagation wave velocity with the sensors aligned, edge to edge, and forming an angle of 45 degrees, with both sensors on the same face of the board. This is because aligned measures are not possible on site. The velocity results are always higher in 45 degree measurements. Given the results of statistical analysis, it can be concluded that there is a strong relationship between acoustic measurements and the decline in physical and mechanical properties of the panels due to aging. The authors propose several models to estimate the physical and mechanical properties of board, as well as their degree of aging. The best results are obtained using ultrasound, although the difference in comparison with the stress wave method is not very significant. A reliable prediction of the degree of deterioration (aging) of board is presented

    Clasificación visual estructural de la madera de pino radiata procedente de Cataluña

    Get PDF
    Se han clasificado visualmente, según la norma española UNE 56544; 150 piezas de madera aserrada de pino radiata procedentes de Cataluña (España) con una sección de 80x150 mm y una longitud de 2.500 mm. Esta norma establece dos calidades visuales (ME-1 y ME-2) para piezas con grueso menor o igual que 70 mm y una única calidad visual (MEG) para gruesos mayores de 70 mm. Con el fin de conocer el efecto frontera entre la pequeña y la gran escuadría se clasificaron las piezas según ambas categorías. Se determinó la tensión de rotura en flexión, el módulo de elasticidad en flexión y la densidad de cada pieza mediante el ensayo de acuerdo con la norma UNE-EN 408 siguiendo los ajustes definidos en la norma UNE-EN 384. Un 53 % de las piezas se clasificaron como MEG con una resistencia característica a flexión de 28 N/mm2 y un valor medio del módulo de elasticidad de 9.900 N/mm2. Por otra, un 42 % de las piezas se clasificaron como ME-2 y sólo un 3 % como ME-1; en este caso las propiedades mecánicas de la calidad ME-2 no se alejan mucho de las de la calidad MEG. El elevado porcentaje de piezas rechazadas (47 % frente a la MEG) se debe principalmente al defecto de alabeo responsable de un 39 % de rechazo. Si no se considera el alabeo en la clasificación el porcentaje de rechazo desciende al 17 % y las propiedades mecánicas de la calidad MEG presentan un valor característico de resistencia a flexión de 21 N/mm2 y un módulo de elasticidad de 9.100 N/mm2. A sample of 150 pieces of radiata pine sawn timber with 180x120 mm in cross-section and 2.500 mm in length sourcing from Catalonia (Spain) were visually graded according to Spanish standard UNE 56544. This standard establish two visual grades (ME-1 and ME-2) for timber pieces with thickness equal or less than 70 mm, and one grade (MEG) for thickness bigger than 70 mm. In order to know the border effect between small and larger cross-section the pieces were graded in both categories. The modulus of rupture, modulus of elasticity and density were obtained by test according to EN 408 standard and the adjustments of EN 384. A 53 % of pieces were classified as MEG with a characteristic bending strength of 28 N/mm2 and a mean value of MOE of 9.900 N/mm2. On the other hand, a 42 % of pieces were classified as ME-2 and only a 3 % as ME-1; in this case the mechanical properties of ME-2 are not far from MEG properties. The high percentage of rejected pieces (47 % vs MEG) is mainly due to the twist defect with a 39 % of rejected pieces. If twist is not considered in the grading process the reject percentage decreases to 17 % and the mechanical properties of MEG grade present a characteristic value of bending strength of 21 N/mm2 and a MOE of 9.100 N/mm2

    Análisis del estado de tensiones en uniones carpinteras de empalme de llave por el método de los elementos finitos

    Get PDF
    El objeto del presente trabajo es la determinación de la distribución de tensiones en la unión carpintera de empalme de llave mediante el método de los elementos finitos y su comparación con los valores obtenidos mediante la teoría de Resistencia de Materiales. Se analizan las zonas donde se produce concentración de tensiones y se estudia la influencia del refino de la malla sobre los resultados con el fin de determinar el tamaño que proporciona los valores de tensión más ajustados a la teoría. En las zonas donde la concentración de tensiones es menor, distintos tamaños de la malla muestran valores de tensión similares. Los resultados muestran una simetría central de la distribución de isotensiones donde el centro de simetría se corresponde con el centro geométrico de la unión. En las zonas donde se produce concentración de tensiones, los valores de las mismas aumentan considerablemente con el refino de la malla. La comparación de los niveles de tensiones normales obtenidos por el MEF y la teoría clásica muestran diferencias reducidas, excepto en los puntos de concentración de tensiones. The purpose of this study is to determine the stress distribution in the joint carpenter of halved and tabled joint with the finite element method and its comparison with the values obtained using the theory of Strength of Materials. The stress concentration areas where analyzed and the influence of mesh refinement was studied on the results in order to determine the mesh size that provides the stress values more consistent with the theory. In areas where stress concentration is lower, different mesh sizes show similar stress values. The results show a central symmetry of the isobar lines distribution where the centre of symmetry corresponds to the geometric centre of the joint. In areas where stress concentration occurs, the same values increase considerably with the refinement of the mesh. Comparison of normal stress levels obtained by the FEM and the classical theory shows small differences, except at points of stress concentration

    The influence of sensor placement on in-situ ultrasound wave velocity measurement.

    Full text link
    Ultrasound wave velocity was measured in 30 pieces of Spanish Scots pine (Pinus sylvestris L.), 90 x 140 mm in cross-section and 4 m long. Five different sensor placement arrangements were used: end to end (V0), face to opposite face, edge to opposite edge, face to same face and edge to same edge. The pieces were successively shortened to 3, 2 and 1 m, in order to obtain these velocities and their ratios to reference value V0 for different lengths and angles with respect to the piece axis for the crossed measurements. The velocity obtained in crossed measurements is lower than V0. A correction coefficient for crossed velocities is proposed, depending on the angle, to adjust them to the V0 benchmark. The velocities measured on a surface, are also lower than V0, and their ratio with respect to V0 is close to 0.97 for distances equal to or greater than 18 times the depth of the beam

    The effect of moisture content on nondestructive probing measurements

    Get PDF
    When assessing existing timber structures it is not possible to obtain density as the ratio mass/volume, so nondestructive probing methods are used to predict density. As in other nondestructive techniques, moisture content influences measurements. The goal of this paper is to study the influence of timber moisture content on two nondestructive probing techniques (penetration resistance and pullout resistance). 25 large cross section specimens of laricio pine from Spain were measured. The moisture content ranged from 65.1% to 8.3%. Penetration depth decreases and screw withdrawal strength increases when moisture content decreases below the fiber saturation point. There are lineal tendencies in both techniques. No moisture content influence was found in measures above fiber saturation point

    Influence of temperature and moisture content in Non-destructive values of Scots pine (Pinus sylvestris L.)

    Full text link
    Good results evaluating material properties using non-destructive testing (NDT) techniques have been achieved for decades. Several studies to understand the influence of temperature and moisture content on NDT have concluded different effects. In this study, NDT parameters were measured on the principal structural Spanish sawn timber species, Scots pine (Pinus sylvestris L.). NDT were conducted on 216 specimens of nominal dimensions 20 by 20 by 400 mm. Specimens were divided into several groups and studied at six different temperatures and four different moisture contents. Commercial equipment and techniques applied were Sylvatest Duo (ultrasonic wave technique), Steinkamp BPV (ultrasonic wave technique), and Grindo Sonic Mk5 "Industrial" (vibration analysis technique). Differences in NDT values within specimens at different temperatures and moisture contents were obtained. Main results of this study and relationships that describe changes in NDT values by effect of temperature and moisture content are presented

    Visual grading of large cross section structural timber of Pinus sylvestris L. according to UNE 56544:2007 standard

    Get PDF
    Large cross section structural timber have been used in many structures over long periods of time and still make up an important part of the market due to its mechanical properties. Furthermore, it is frequent its employment in new construction site. It involves the need for a visual grading standard for timber used in construction according to the quality assessment. The material has to satisfy the requirements according to the currently regulations. UNE 56544 is the Spanish visual grading standard for coniferous structural timber. The 2007 version defined a new visual grade in the standard for large section termed Structural Large Timber (MEG). This research checks the new visual grading and consists of 116 structural size specimens of sawn coniferous timber of Scotch pine (Pinus sylvestris L.) from Segovia, Spain. The pieces had a cross section of 150 by 200 mm. They were visually graded according to UNE 56544:2007. Also, mechanical properties have been obtained according to standard EN 408. The results show very low output with an excessive percentage of rejected pieces (33%). The main reasons for the rejection of pieces are fissures and twis

    Análisis de parámetros de fendas para la estimación de las propiedades mecánicas de vigas de madera de Pinus sylvestris L. Analysis of parameters for assessing drying fissures to estimate their influence on the mechanical properties of Pinus sylvestris L. wooden beams

    Get PDF
    El principal objetivo de este estudio es evaluar la influencia de las fendas de secado en las propiedades mecánicas de vigas de madera. Para esto, se utilizan 40 vigas de Pino silvestre (Pinus sylvestris L) de 4200 mm de longitud y 150x200 mm de sección que fueron ensayadas según norma EN 408. Las fendas se registran detalladamente atendiendo a su longitud y posición en cada cara de la viga, y midiendo el espesor y la profundidad cada 100mm a lo largo de la viga. Solo el 10% de la muestra es rechazada por las fendas, según los criterios establecidos por la norma española de clasificación visual UNE 56544. Para evaluar la influencia de las fendas en las propiedades mecánicas, se usan tres parámetros globales basados en el área, el volumen o la profundad de la fenda, y dos locales basados en la profundidad máxima y la profundidad en la zona de rotura. Además se determina la densidad de las piezas. Estos parámetros se comparan con las propiedades mecánicas (tensión de rotura, módulo de elasticidad y energía de rotura) y se encuentra escasa relación entre ellos. Las mejores correlaciones se encuentran entre los parámetros relacionados con la profundidad de las fendas, tanto con el módulo de elasticidad como con la tensión de rotura. The aim of this study is the evaluation of the influence of drying fissures on the mechanical properties of timber beams. For that purpose, 40 sawn timber pieces of Scots pine (Pinus sylvestris L.) with 150x200 mm in cross-section and 4200 mm in length have been tested according to EN 408, obtaining MOR and MOE. The fissures were registered in detail measuring their length and position in each face of the beam, and the thickness and depth every 100 mm in length. Only 10 % of the pieces were rejected because fissures, according to UNE 56544 Spanish visual grading standard. To evaluate the influence of fissures in mechanical properties three global parameters: Fissures Area Ratio or ratio between the area occupied by fissures and the total area in the neutral axis plane of the beam; Fissures Volume Ratio or ratio between volume of fissures and the total volume of the beam; Fissures Average Depth and two local parameters were used: Fissures Maximum Depth in the beam, and Fissures Depth in the broken zone of the beam. Also the density of the beams was registered. These parameters were compared with mechanical properties (tensile strength, elasticity modulus, and rupture energy) and the relationship between them had not been founded. The best relationship was founded between the elasticity modulus y the tensile strength with the parameters which included the depth of the fissures
    corecore