    The objective of this study was to examine the association of herd size with animal welfare in dairy cattle herds. Therefore, 80 conventional dairy cattle farms were classified by the number of cows into 4 herd size classes, C1 (100 cows), C2 (100-299 cows), C3 (300-499 cows), and C4 (≄500 cows), and assessed using multiple animal-based measures of the Welfare Quality Assessment protocol for dairy cattle. Data were recorded from April 2014 to September 2016 by an experienced single assessor in northern Germany. Each farm was visited 2 times at an interval of 6 mo (summer period and winter period) to avoid seasonal effects on the outcome. The average herd size was 383 ± 356 Holstein-Friesian cows (range 45 to 1,629). Only farms with freestall (cubicle) housing and a maximum of 6 h access to pasture per day were included in the study. Data were statistically analyzed using a generalized linear mixed model. None of the farms reached the highest overall rating of "excellent." The majority of the farms were classified as "enhanced" (30%) or "acceptable" (66%), and at 6 assessments the farms were rated as "not classified" (4%). Regarding single indicators, mean trough length per cow, percentage of cows with nasal discharge, and vulvar discharge increased with increasing herd size, whereas it was vice versa for displacements of cows. Percentage of lean cows, percentage of dirty lower legs, and duration of the process of lying down showed a curvilinear relationship with the number of cows per farm. Herd size was not associated with any other measures of the Welfare Quality protocol. In conclusion, herd size effects were small, and consequently herd size cannot be considered as a feasible indicator of the on-farm animal welfare level. Housing conditions and management practices seem to have a greater effect on animal welfare than the number of dairy cows per farm

    Comparison of Selective Laser Melted Titanium and Magnesium Implants Coated with PCL

    Get PDF
    Degradable implant material for bone remodeling that corresponds to the physiological stability of bone has still not been developed. Promising degradable materials with good mechanical properties are magnesium and magnesium alloys. However, excessive gas production due to corrosion can lower the biocompatibility. In the present study we used the polymer coating polycaprolactone (PCL), intended to lower the corrosion rate of magnesium. Additionally, improvement of implant geometry can increase bone remodeling. Porous structures are known to support vessel ingrowth and thus increase osseointegration. With the selective laser melting (SLM) process, defined open porous structures can be created. Recently, highly reactive magnesium has also been processed by SLM. We performed studies with a flat magnesium layer and with porous magnesium implants coated with polymers. The SLM produced magnesium was compared with the titanium alloy TiAl6V4, as titanium is already established for the SLM-process. For testing the biocompatibility, we used primary murine osteoblasts. Results showed a reduced corrosion rate and good biocompatibility of the SLM produced magnesium with PCL coating.DFG/299/11-

    SLM produced porous titanium implant improvements for enhanced vascularization and osteoblast seeding

    Get PDF
    To improve well-known titanium implants, pores can be used for increasing bone formation and close bone-implant interface. Selective Laser Melting (SLM) enables the production of any geometry and was used for implant production with 250-microm pore size. The used pore size supports vessel ingrowth, as bone formation is strongly dependent on fast vascularization. Additionally, proangiogenic factors promote implant vascularization. To functionalize the titanium with proangiogenic factors, polycaprolactone (PCL) coating can be used. The following proangiogenic factors were examined: vascular endothelial growth factor (VEGF), high mobility group box 1 (HMGB1) and chemokine (C-X-C motif) ligand 12 (CXCL12). As different surfaces lead to different cell reactions, titanium and PCL coating were compared. The growing into the porous titanium structure of primary osteoblasts was examined by cross sections. Primary osteoblasts seeded on the different surfaces were compared using Live Cell Imaging (LCI). Cross sections showed cells had proliferated, but not migrated after seven days. Although the cell count was lower on titanium PCL implants in LCI, the cell count and cell spreading area development showed promising results for titanium PCL implants. HMGB1 showed the highest migration capacity for stimulating the endothelial cell line. Future perspective would be the incorporation of HMGB1 into PCL polymer for the realization of a slow factor release.DFG/299/11-

    Effects of Housing and Management Factors on Selected Indicators of the Welfare Quality® Protocol in Loose-Housed Dairy Cows

    No full text
    The objective of this study was to examine the effects of housing and management factors on animal welfare indicators in dairy cows using a benchmarking approach. In total, 63 conventional dairy cattle farms with zero-grazing in Northern Germany were assessed using selected animal welfare indicators (body condition score, integument alterations, lameness, milk somatic cell count, and social behaviour) of the Welfare Quality® protocol. Additionally, housing characteristics such as designs of barns, cubicles, and floors were documented during farm visits and farmers were interviewed concerning their common management routines. Farms were categorized into a high welfare or low welfare group by calculating upper and lower tertiles for each of the animal welfare indicators separately. Both groups were compared regarding housing conditions and management practices using univariable and multivariable logistic regressions. Several associations between housing and management factors and animal welfare indicators were demonstrated in univariable analysis (p < 0.20). Significant effects within multivariable logistic regression analysis were determined for lameness (routine use of foot-baths), milk somatic cell count (milking frequency) and social behaviour (cow-to-stall ratio) (p < 0.05). Comparing farms with higher and lower animal welfare status can provide useful information about effective options to improve animal welfare

    Snow and ice surfaces on King George Island (Antarctic Peninsula) with high-resolution TerraSAR-X time series, with links to shapfiles and GeoTIFFs

    No full text
    Changes of glaciers and snow cover in polar regions affect a wide range of physical and ecosystem processes on land and in the adjacent marine environment. In this study, we investigate the potential of 11-day repeat high-resolution satellite image time series from the TerraSAR-X mission to derive glaciological and hydrological parameters on King George Island, Antarctica during the period Oct/25/2010 to Apr/19/2011. The spatial pattern and temporal evolution of snow cover extent on ice-free areas can be monitored using multi-temporal coherence images. SAR coherence is used to map glacier extent of land terminating glaciers with an average accuracy of 25 m. Multi-temporal SAR color composites identify the position of the late summer snow line at about 220 m above sea level. Glacier surface velocities are obtained from intensity feature-tracking. Surface velocities near the calving front of Fourcade Glacier were up to 1.8 ± 0.01 m/d. Using an intercept theorem based on fundamental geometric principles together with differential GPS field measurements, the ice discharge of Fourcade Glacier was estimated to 20700 ± 5500 m**3/d (corresponding to ~19 ± 5 kt/d). The rapidly changing surface conditions on King George Island and the lack of high-resolution digital elevation models for the region remain restrictions for the applicability of SAR data and the precision of derived products

    SLM Produced Porous Titanium Implant Improvements for Enhanced Vascularization and Osteoblast Seeding

    No full text
    To improve well-known titanium implants, pores can be used for increasing bone formation and close bone-implant interface. Selective Laser Melting (SLM) enables the production of any geometry and was used for implant production with 250-”m pore size. The used pore size supports vessel ingrowth, as bone formation is strongly dependent on fast vascularization. Additionally, proangiogenic factors promote implant vascularization. To functionalize the titanium with proangiogenic factors, polycaprolactone (PCL) coating can be used. The following proangiogenic factors were examined: vascular endothelial growth factor (VEGF), high mobility group box 1 (HMGB1) and chemokine (C-X-C motif) ligand 12 (CXCL12). As different surfaces lead to different cell reactions, titanium and PCL coating were compared. The growing into the porous titanium structure of primary osteoblasts was examined by cross sections. Primary osteoblasts seeded on the different surfaces were compared using Live Cell Imaging (LCI). Cross sections showed cells had proliferated, but not migrated after seven days. Although the cell count was lower on titanium PCL implants in LCI, the cell count and cell spreading area development showed promising results for titanium PCL implants. HMGB1 showed the highest migration capacity for stimulating the endothelial cell line. Future perspective would be the incorporation of HMGB1 into PCL polymer for the realization of a slow factor release

    Poly-epsilon-caprolactone Coated and Functionalized Porous Titanium and Magnesium Implants for Enhancing Angiogenesis in Critically Sized Bone Defects

    No full text
    For healing of critically sized bone defects, biocompatible and angiogenesis supporting implants are favorable. Murine osteoblasts showed equal proliferation behavior on the polymers poly-epsilon-caprolactone (PCL) and poly-(3-hydroxybutyrate)/poly-(4-hydroxybutyrate) (P(3HB)/P(4HB)). As vitality was significantly better for PCL, it was chosen as a suitable coating material for further experiments. Titanium implants with 600 microm pore size were evaluated and found to be a good implant material for bone, as primary osteoblasts showed a vitality and proliferation onto the implants comparable to well bottom (WB). Pure porous titanium implants and PCL coated porous titanium implants were compared using Live Cell Imaging (LCI) with Green fluorescent protein (GFP)-osteoblasts. Cell count and cell covered area did not differ between the implants after seven days. To improve ingrowth of blood vessels into porous implants, proangiogenic factors like Vascular Endothelial Growth Factor (VEGF) and High Mobility Group Box 1 (HMGB1) were incorporated into PCL coated, porous titanium and magnesium implants. An angiogenesis assay was performed to establish an in vitro method for evaluating the impact of metallic implants on angiogenesis to reduce and refine animal experiments in future. Incorporated concentrations of proangiogenic factors were probably too low, as they did not lead to any effect. Magnesium implants did not yield evaluable results, as they led to pH increase and subsequent cell death.DFG/299/11-

    Poly-Δ-caprolactone Coated and Functionalized Porous Titanium and Magnesium Implants for Enhancing Angiogenesis in Critically Sized Bone Defects

    No full text
    For healing of critically sized bone defects, biocompatible and angiogenesis supporting implants are favorable. Murine osteoblasts showed equal proliferation behavior on the polymers poly-Δ-caprolactone (PCL) and poly-(3-hydroxybutyrate)/poly-(4-hydroxybutyrate) (P(3HB)/P(4HB)). As vitality was significantly better for PCL, it was chosen as a suitable coating material for further experiments. Titanium implants with 600 ”m pore size were evaluated and found to be a good implant material for bone, as primary osteoblasts showed a vitality and proliferation onto the implants comparable to well bottom (WB). Pure porous titanium implants and PCL coated porous titanium implants were compared using Live Cell Imaging (LCI) with Green fluorescent protein (GFP)-osteoblasts. Cell count and cell covered area did not differ between the implants after seven days. To improve ingrowth of blood vessels into porous implants, proangiogenic factors like Vascular Endothelial Growth Factor (VEGF) and High Mobility Group Box 1 (HMGB1) were incorporated into PCL coated, porous titanium and magnesium implants. An angiogenesis assay was performed to establish an in vitro method for evaluating the impact of metallic implants on angiogenesis to reduce and refine animal experiments in future. Incorporated concentrations of proangiogenic factors were probably too low, as they did not lead to any effect. Magnesium implants did not yield evaluable results, as they led to pH increase and subsequent cell death
    corecore