    Surface fatigue life of M50NiL and AISI 9310 spur gears and R C bars

    Get PDF
    Spur gear endurance tests and rolling element surface fatigue tests were conducted to study vacuum induction melted, vacuum arc remelted (VIM-VAR) M50NiL steel for use as a gear steel in advanced aircraft applications, to determine its endurance characteristics, and to compare the results with those for standard VAR and VIM-VAR AISI 9310 gear material. Tests were conducted with spur gears and rolling contact bars manufactured from VIM-VAR M50NiL and VAR and VIM-VAR AISI 9310. The gear pitch diameter was 8.9 cm. Gear test conditions were an inlet oil temperature of 320 K, and outlet oil temperature of 350 K, a maximum Hertz stress of 1.71 GPa, and a speed of 10000 rpm. Bench rolling element fatigue tests were conducted at ambient temperatures with a bar speed of 12,500 rpm and a maximum Hertz stress of 4.83 GPa. The VIM-VAR M50NiL gears had a surface fatigue life that was 4.5 and 11.5 times that for VIM-VAR and VAR AISI 9310 gears, respectively. The surface fatigue life of the VIM-VAR M50NiL rolling contact bars was 13.2 and 21.6 times that for the VIM-VAR and VAR AISI 9310, respectively. The VIM-VAR M50NiL material was shown to have good resistance to fracture through a fatigue spall and superior fatigue life to both other gears

    Surface fatigue life of carburized and hardened M50NiL and AISI 9310 spur gears and rolling-contact test bars

    Get PDF
    Spur gear endurance tests and rolling-element surface tests were conducted to investigate vacuum-induction-melted, vacuum-arc-melted (VIM-VAR) M50NiL steel for use as a gear steel in advanced aircraft applications, to determine its endurance characteristics, and to compare the results with those for standard VAR and VIM-VAR AISI 9310 gear material. Tests were conducted with spur gears and rolling-contact bars manufactured from VIM-VAR M50NiL and VAR and VIM-VAR AISI 9310. The gear pitch diameter was 8.9 cm (3.5 in.). Gear test conditions were an inlet oil temperature of 320 K (116 F), and outlet oil temperature of 350 K (170 F), a maximum Hertz stress of 1.71 GPa (248 ksi), and a speed of 10,000 rpm. Bench rolling-element fatigue tests were conducted at ambient temperatures with a bar speed of 12,500 rpm and a maximum Hertz stress of 4.83 GPA (700 ksi). The VIM-VAR M50NiL gears had a surface fatigue life that was 4.5 and 11.5 times that for VIM-VAR and VAR AISI 9310 gears, respectively. The surface fatigue life of the VIM-VAR M50NiL rolling-contact bars was 13.2 and 21.6 times that for the VIM-VAR and VAR AISI 9310, respectively. The VIM-VAR M50NiL material was shown to have good resistance to fracture through a fatigue spall and to have fatigue life far superior to that of both VIM-VAR and VAR AISI 9310 gears and rolling-contact bars

    Toward fault-tolerant quantum computation without concatenation

    Full text link
    It has been known that quantum error correction via concatenated codes can be done with exponentially small failure rate if the error rate for physical qubits is below a certain accuracy threshold. Other, unconcatenated codes with their own attractive features-improved accuracy threshold, local operations-have also been studied. By iteratively distilling a certain two-qubit entangled state it is shown how to perform an encoded Toffoli gate, important for universal computation, on CSS codes that are either unconcatenated or, for a range of very large block sizes, singly concatenated.Comment: 12 pages, 2 figures, replaced: new stuff on error models, numerical example for concatenation criteri

    Reconsideration of the Rise and Fall of Detroit Through the Lens of Non-Place

    Get PDF
    http://deepblue.lib.umich.edu/bitstream/2027.42/120372/1/Dennis_ReconsiderationOfTheRiseAndFallOfDetroitThroughTheLensOfNon-Place.pd
    • …
    corecore