58 research outputs found

    Physical and Electrical Performance of Vapor–Solid Grown ZnO Straight Nanowires

    Get PDF
    Physical and electrical properties of wurtzitic ZnO straight nanowires grown via a vapor–solid mechanism were investigated. Raman spectrum shows four first-order phonon frequencies and a second-order Raman frequency of the ZnO nanowires. Electrical and photoconductive performance of individual ZnO straight nanowire devices was studied. The results indicate that the nanowires reported here are n-type semi-conductors and UV light sensitive, and a desirable candidate for fabricating UV light nanosensors and other applications

    Experimental and theoretical investigation of ligand effects on the synthesis of ZnO nanoparticles

    Get PDF
    ZnO nanoparticles with highly controllable particle sizes(less than 10 nm) were synthesized using organic capping ligands in Zn(Ac)2 ethanolic solution. The molecular structure of the ligands was found to have significant influence on the particle size. The multi-functional molecule tris(hydroxymethyl)-aminomethane (THMA) favoured smaller particle distributions compared with ligands possessing long hydrocarbon chains that are more frequently employed. The adsorption of capping ligands on ZnnOn crystal nuclei (where n = 4 or 18 molecular clusters of(0001) ZnO surfaces) was modelled by ab initio methods at the density functional theory (DFT) level. For the molecules examined, chemisorption proceeded via the formation of Zn...O, Zn...N, or Zn...S chemical bonds between the ligands and active Zn2+ sites on ZnO surfaces. The DFT results indicated that THMA binds more strongly to the ZnO surface than other ligands, suggesting that this molecule is very effective at stabilizing ZnO nanoparticle surfaces. This study, therefore, provides new insight into the correlation between the molecular structure of capping ligands and the morphology of metal oxide nanostructures formed in their presence

    Release of engineered nanomaterials from personal care products throughout their life cycle

    Full text link
    The impetus for this study was to provide release estimates that can serve to improve predictions of engineered nanomaterial (ENM) exposure for risk assessment. We determined the likely release of ENMs from personal care products (PCPs) through a consumer survey on use and disposal habits, and research on the types and quantities of ENMs in PCPs. Our estimates show that in the US zinc oxide (ZnO), with 1,800-2,100 mt yr-1, and titanium dioxide (TiO2), with 870-1,000 mt yr-1, represent 94 % of ENMs released into the environment or landfills from the use of PCPs. Around 36-43 % of ENMs from PCPs were estimated to end up in landfills, 24-36 % released to soils, 0.7-0.8 % to air, and 28-32 % to water bodies. ENMs in sunscreen represent around 81-82 % of total release, from ZnO and TiO2 as UV blockers, followed by facial moisturizer (7.5 %), foundation (5.7 %), and hair coloring products (3.1 %). Daily care products such as body wash, shampoo, and conditioner had by far the highest per capita and total use, but contributed little to the ENM release estimates as these products generally contain little or no ENMs. However, if ENMs are incorporated into these daily care products, this may substantially increase ENM release. © 2014 Springer Science+Business Media

    Synthesis of ZnO nanoparticles by flame spray pyrolysis and characterisation protocol

    No full text
    There is uncertainty concerning the potential toxicity of zinc oxide (ZnO) nanoparticles, which may be attributed in part to a lack of understanding with regard to the physiochemical properties of the nanoparticles used in toxicological investigations. This paper reports the synthesis of a ZnO nanopowder by flame spray pyrolysis and demonstrates that the typically employed characterisation techniques such as specific surface area measurement and X-ray diffraction provide insufficient information on the sample, especially if it is intended for use in toxicity studies. Instead, a more elaborate characterisation protocol is proposed that includes particle morphology as well as detailed compositional analysis of the nanoparticle surface. Detailed transmission electron microscopy analysis illustrated the polydispersity within the sample: particles were elongated in the c-crystallographic direction, with average Ferret length ∼23 nm and Ferret width ∼14 nm. Dynamic light scattering (0.1 w/v% in deionised water, pH 7.4) revealed the particles were agglomerated with a modal secondary particle size of ∼1.5 μm. Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy indicated the presence of carbonate and hydroxide impurities on the surface of the ZnO nanoparticles and an increase of such impurities was observed as the sample was aged, which might influence the nanoparticle dissolution and/or cellular uptake behaviour. These data will be utilised, in order to facilitate the interpretation and understanding of results from toxicological investigations using in vitro cell lines

    Three-dimensional inhomogeneities in PEDOT:PSS Films

    No full text
    Spin-cast PEDOT/PSS film are investigated using scanning probe-based spectroscopic techniques. The films are found to consist of relatively well-conducting islands that are embedded in a less conductive matrix. A scanning-tunneling microscope-based method is developed to obtain three-dimensional conductivity images with nanometer resolution. Order-of-magnitude variations in the film conductivity are observed in all spatial directions. In addition, charge transport in the normal direction depends on the injection spot and is found to be ohmic or space-charge-limited. We found that both the morphology and the conductivity of the top layer differ substantially from those in the bulk, which is attributed to an enhanced PSS content in the top layer

    Potential tuning of porous silicon luminescence

    No full text
    Electrochemical investigations were conducted of the effect of potential on the luminescence of porous silico (PS). The use of liquid contacts allows the potential to be controlled during studies of the photoluminescence (PL) and electroluminescence (EI). The PL and EL of PS samples prepared from n-type substrates is considered. To obtain luminescence from such PS it is necessary to generate holes in the valence band. This is achieved by either photoexcitation or an electrochemical process involving the reduction of persulfate. This paper describes the investigations of the effect of potential on the PL and EL of PS. A mechanism of 'potential tuning' based on electron occupancy and Auger quenching is then proposed
    corecore