32 research outputs found

    Controllable spin-glass behavior and large magnetocaloric effect in Gd-Ni-Al bulk metallic glasses

    No full text
    Glass-forming ability, spin-glass (SG) behavior, and magnetocaloric effect in Gd55NixAl45-x (x?15, 20, 25, 30) metallic alloys were investigated. A ferromagnetic SG behavior was observed for glassy ribbons with compositions of x?15, 20, and 25, but it disappeared for that of x?30.Furthermore, the maximum magnetic entropy change ( DSm max) increased with the increasing Ni/ Al-ratio while the decrease of full width at half DSm max was almost negligible. Accordingly, DSm max of 9.25 J kg 1 K 1, adiabatic temperature change of 4.3K and refrigeration capacity of 851 J kg 1 under 50 kOe were obtained for Gd55Ni30Al15 glassy alloy. VC 2012 American Institute of Physics

    兼具大非晶形成能力与高磁热效应的Gd基块体非晶合金及其制备方法

    No full text
    本发明公开了一种兼具大非晶形成能力与高磁热效应的Gd基块体非晶合金,其分子式为GdaNibAlcMd,其中M为B、Si、C、P中的一种或多种,a、b、c、d分别为对应元素的原子含量,并且满足50≤a≤60,10≤b≤40,10≤c≤40,0≤d≤10,a+b+c+d=100。与现有技术相比,本发明的Gd基块体非晶合金的直径能够达到2~3.5mm,最大磁熵变高达6.12~9.25Jkg-1K-1,磁致冷能力高达606~851Jkg-1,过冷液相区宽度高达40~60K,是一种在制冷技术领域中具有很好应用前景的合金材料

    高饱和磁感应强度低成本铁基纳米晶软磁合金

    No full text
    本发明涉及一种铁基纳米晶软磁合金,其特征在于合金组成满足关系式:FeaBbCcMdCue,式中M为选自Si、Al、Cr和Mn中的一种或多种,下标a、b、c、d、e分别表示各对应合金元素的原子百分比,并且满足以下条件:78≤a≤88;4≤b≤16;3≤c≤10;0≤d≤8;0.3≤e≤1.5;a+b+c+d+e=100,所述铁基纳米晶合金由非晶基体相和纳米晶相组成。该合金的显著特征在于兼具高饱和磁感应强度,低矫顽力,低损耗等优异的软磁性能,并且不含贵金属元素及挥发性元素,降低了原材料的加工成本,便于推广应用。本发明还涉及上述合金的制备方法

    兼具高非晶形成能力和优异磁性能的Fe基块体非晶合金及其制备方法

    No full text
    本发明涉及一种Fe基块体非晶合金,该合金的组成表示为FeaSibBcPdMe,其中,a、b、c、d、e为原子百分含量,并满足72≤a≤82,13≤b+c+d≤28,0<e≤8,且满足a+b+c+d+e=100,M为选自Cr、Zr、Hf、Ta、W、V、Mn、Al、Mo和Nb中至少一种。本发明还涉及所述Fe基块体非晶合金的制备方法

    一种高耐蚀性铁基软磁非晶合金及其制备方法

    No full text
    本发明公开了一种高耐蚀性铁基软磁非晶合金及其制备方法。该铁基软磁非晶合金的分子式为FeaCrbNicModPeCfBgSih,式中a、b、c、d、e、f、g、h表示各对应原子的摩尔百分含量,60≤a≤80,0.5≤b≤4,2≤c≤12,2.5≤d≤4.5,8.5≤e≤11.5,2.5≤f≤5.5,3≤g≤6,1≤h≤4,且满足a+b+c+d+e+f+g+h=100。与现有的铁基软磁非晶合金相比,该非晶合金同时具有高耐蚀性、高非晶形成能力以及优异磁性能,能够作为电磁器件材料在恶劣的环境中,如湿热盐雾、氨气或各种酸、海水、污水等腐蚀介质中使用

    Effect of Fe to P concentration ratio on structures, crystallization behavior, and magnetic properties in (Fe0.79+xP0.1-xC0.04B0.04Si0.03)99Cu1 alloys

    No full text
    The effect of Fe to P concentration ratio on structures, crystallization behavior, and magnetic properties in (Fe0.79txP0.1 xC0.04B0.04 Si0.03 )99Cu1alloys was investigated. The increase of Fe to P concentration ratio changes the structure and crystallization process of as-quenched ribbon. Nanocrystalline alloys with excellent soft magnetic properties were synthesized upon annealing the as-quenched ribbon with primary crystals. The (Fe0.84P0.05C0.04B0.04 Si0.03 )99Cu1 nanocrystalline alloy exhibits excellent magnetic properties, such as high saturation magnetic flux density of 1.74 T, low coercivity of 4.9 A/m, high effective permeability of 22 900 (at 1 kHz), low core loss of 3.1 W/kg at 1.0 T and 400 Hz, and 8.9 W/kg at 1.0 T and 1 kHz, respectively

    一种铁基纳米晶软磁合金及其制备方法

    No full text
    本发明公开了一种新型铁基纳米晶软磁合金及其制备方法。该铁基纳米晶软磁合金的分子式为FexPyCzMaCub,式中M为B、Si、Al、Cr、Mn、Mo和Ge中的一种或多种,x、y、z、a、b分别表示各对应组分的原子百分含量,其中70≤x≤90、1≤y≤20、1≤z≤20、0≤a≤10、0.1≤b≤2,且x+y+z+a+b=100;其微结构为尺寸介于5-40nm的体心立α-Fe纳米晶相与富含磷和碳的非晶相共存,且以非晶相为基体相。与现有的纳米晶软磁合金相比,该合金同时具备高饱和磁感应强度,低矫顽力,低铁损,高磁导率;另外,由于不含Nb、Zr、Co、Ni、Y等贵金属元素,从而大大降低了加工成本,具有优良的应用前景

    高饱和磁化强度铁基纳米晶软磁合金材料及其制备方法

    No full text
    本发明涉及到高饱和磁化强度铁基纳米晶软磁合金及其制备方法,其特征在于其是由铁、硅、硼、磷、铜构成的FexSiyBzPaCub合金,式中x、y、z、a、b分别表示各对应组分的原子百分比含量,其中x=70-90%、y=1-15%、z=1-20%、a=1-20%、b=0.1-1%,且x+y+z+a+b=100%;该铁基纳米晶软磁合金的微结构为尺寸介于1-35nm的体心立方α-Fe(Si)纳米晶相与富含磷和硼的非晶相共存,且以非晶相为基体相。制备方法主要是将配比好的原料先制备成合金锭,然后制成非晶合金,再进行其它工序的处理,最后得到高饱和磁化强度的铁基纳米晶软磁合金。该发明能够大幅提高纳米晶软磁合金的饱和磁化强度,同时能够保持较低的矫顽力并有效降低原材料成本

    一种铁基大块非晶软磁合金及其制备方法

    No full text
    本发明公开了一种铁基大块非晶软磁合金及其制备方法,该非晶合金的分子式为(Fe0.5Co0.5)70.7-xB20Si5Nb4.3Tbx,其中x的取值范围为0≤x≤2.5,该非晶合金是通过往FeCoBSiNb体系中添入稀土元素Tb来制得的。与现有技术相比,本发明的优点在于:用工业原料制备的这一系列铁基大块非晶合金具有较大的非晶形成能力和优异的软磁性能,制备出的非晶棒材直径为2mm-3mm,饱和磁化强度为0.69T-0.92T,矫顽力矫顽力为2.1A/m-3.8A/m,相对其他掺杂稀土元素体系比较低,而且制备方法简单、成本较低。本发明提供的铁基大块非晶合金可以用作磁性传感器芯体,应用于信息、通讯等领域

    钴基块体非晶合金及其制备方法

    No full text
    一种钴基块体非晶合金,其特征在于该合金的分子简式为CoaFebNbcB22.4Si5.6,并 满足60<a<65,2<b<5,3<c<7。本发明还公开了该钴基块体非晶合金的制备方法。与现 有技术相比,本发明的优点在于:所得产品具有优异软磁性能、良好的机械性能和非晶 形成能力的钴基块体非晶合金体系
    corecore