Effect of crystalline admixtures on the self-healing capability of early-age concrete studied by means of permeability and crack closing tests

Abstract

This paper analyzes the self-healing properties of early-age concretes, engineered using a crystalline admixture (4% by the weight of cement), by measuring the permeability of cracked specimens and their crack width. Two concrete classes (C30/37 and C45/55) and three healing exposure conditions have been investigated: water immersion at 15 °C, at 30 °C and wet/dry cycles. Specimens were pre-cracked at 2 days, to values of crack width in the range of 0.10 0.40 mm. The results show almost perfect healing capability for specimens healed under water at 30 °C, better than for specimens healed under water at 15 °C, while insufficient for the wet/dry exposure.Roig Flores, M.; Pirritano, F.; Serna Ros, P.; Ferrara, L. (2016). Effect of crystalline admixtures on the self-healing capability of early-age concrete studied by means of permeability and crack closing tests. Construction and Building Materials. 114:447-457. doi:10.1016/j.conbuildmat.2016.03.196S44745711

    Similar works