105 research outputs found

    Synthesis and Adsorption Properties of 4-Vinylpyridine and Styrene Copolymer In Situ Immobilized on Silica Surface

    Get PDF
    Copolymer of 4-vinylpyridine with styrene was in situ immobilized on silica gel surface via the heterogeneous radical polymerization. Anchorage of the copolymer on the surface layer was confirmed by IR spectroscopy. The quantity of copolymer on the silica gel surface was evaluated as 25.73 wt.% by TG and DSC-MS analysis. “Islet” location of polymer layer on the silica surface was confirmed by the scanning electron microscopy. A high adsorption activity of silica gel with immobilized copolymer towards microquantitatives of Cu(II), Cd(II), Pb(II), Fe(III), and Ni(II) ions in steady state conditions as well as of Ni(II) ions in dynamic regime was found

    In Situ Immobilization on the Silica Gel Surface and Adsorption Capacity of Poly[N-(4-carboxyphenyl)methacrylamide] on Toxic Metal Ions

    Get PDF
    In situ immobilization of poly[N-(4-carboxyphenyl)methacrylamide] has been performed on silica gel surface. Infrared (IR) and mass spectroscopies as well as thermogravimetry (TG) analysis have been used to elucidate the structure of immobilized polymer. An adsorption capacity of the synthesized composite towards Cu(II), Pb(II), Mn(II), Fe(III), Co(II), and Ni(II) ions has been estimated. Adsorption activity to microquantities of Pb(II), Cu(II), and Ni(II) in a neutral aqueous medium has been observed

    Investigation of surface structure, electrokinetic and stability properties of highly dispersed Ho₂O₃-Yb₂O₃/SiO₂ nanocomposites

    Get PDF
    A series of highly dispersed Ho2O3–Yb2O3/SiO2 nanocomposites was synthesized using a liquid-phase method and examined using Fourier transform infrared (FTIR) spectroscopy, X-ray diffraction (XRD), nitrogen adsorption–desorption, transmission electron microscopy (TEM), Scanning Electron Microscopy (SEM), and photon correlation spectroscopy (PCS). X-ray fluorescence spectrometry (XRF) confirmed a similar amount of weight percentage of Ho, Yb and Si oxides in the prepared samples. Samples HoYbSi1 (Ho2O3:Yb2O3:SiO2 = 0.5:10:89.5, wt. %), HoYbSi2 (Ho2O3:Yb2O3:SiO2 = 1:10:89, wt. %) and HoYbSi3 (Ho2O3:Yb2O3:SiO2 = 2:10:88, wt. %) calcined at 550 °C are amorphous. TEM and SEM analysis confirm a sphere-like morphology with a quite homogeneous size and shape. As compared with the initial silica, the agglomerated particles of nanocomposites in the aqueous medium are in the range from 200 to 850 nm according to PCS data. The effect of anionic polyacrylic acid (PAA) adsorption on fumed silica (SiO2) and Ho2O3–Yb2O3/SiO2 nanocomposite surfaces on suspension stability was studied. The turbidymetry method was used to monitor the initial silica and triple nanooxides suspensions stability as a function of time