35 research outputs found

    Use of the novel hemostatic textile Stasilon® to arrest refractory retroperitoneal hemorrhage: a case report

    Get PDF
    <p>Abstract</p> <p>Introduction</p> <p>Stasilon<sup>® </sup>is a novel hemostatic woven textile composed of allergen-free fibers of continuous filament fiberglass and bamboo yarn. The development of this product resulted from controlled <it>in vitro </it>thrombogenic analysis of an array of potentially hemostatic textile materials and it has been cleared for both external and internal use by the United States Food and Drug Administration for the arrest of hemorrhage. The goal of the study was to assess the hemostatic and adhesive properties of Stasilon<sup>® </sup>in the setting of life-threatening refractory hemorrhage.</p> <p>Case presentation</p> <p>A 39-year-old Caucasian man presented with severe necrotic pancreatitis that failed multiple aggressive attempts to control associated bleeding with electrocautery, suture ligation, and sequential anatomic packing with cotton-based sponges. Subsequent retroperitoneal packing with Stasilon<sup>® </sup>produced a non-adherent wound-dressing interface and resulted in the achievement of persistent hemostasis in the operative field.</p> <p>Conclusion</p> <p>In our patient, Stasilon<sup>® </sup>was demonstrated to be effective in the arrest of refractory hemorrhage.</p

    Badanie odporności tkanin wykonanych z ramii i lnu na wyciąganie okrywy

    No full text
    The paper presents an investigation of the resistance to pile loop extraction of terry fabrics in relation to the pile height, impacts/finishing, and weft density. Terry fabrics analysed in the experimental work were made from linen/cotton or ramie/cotton yarns. The pile height of the fabrics was 6 and 12 mm, and the weft density varied from 80 to 200 dm-1. The samples were affected by impacts or finishing operations. Grey fabrics were also investigated. Analysing a 10 mm pulling distance, the highest resistance to pile loop extraction of grey terry fabrics (1064.2 mN) was determined for linen/cotton fabric with a 6 mm loop pile. It was found that an increase in the weft density of ramie/cotton terry fabrics from 80 to 160 dm-1 led to an increase in the resistance to pile loop extraction for all pulling distances investigated but with a different intensity: for a 5 mm pulling distance the difference was 3.2 times, and for a 25 mm pulling distance it was in 2.1 times. The decrease in the resistance to pile loop extraction of 18.6 - 38.0% of industrially finished and tumbled linen/cotton fabrics compared with grey ones was determined at a 10 mm pulling distance. The changes in the resistance to pile loop extraction in relation to the tumbling period were not statistically significant.Badano odporność na wyciąganie pętli okrywy tkanin frotowych w zależności od długości okrywy, sposobu wykańczania i gęstości wątku. Tkaniny frotowe zastosowane w eksperymencie wykonano z mieszanek len/bawełna oraz ramia/bawełna. Badano tkaniny o wysokości okrywy 6 i 12 mm oraz gęstości wątku od 80 - 200 dm-1. Próbki badano surowe oraz poddano działaniu rożnych procesów wykańczających

    Upakowanie włókien w przędzach typu „open-packed”

    No full text
    Theoretical observations of the packing properties of non-compressible round fibres for two idealized modifications of the open-packed yarn model are discussed. The modifications differ in the method of arrangement of fibres within the cross-sectional ring layer. Modification I has a number of fibres regularly increasing in further layers, and Modification II has the fibres maximum packed in the layers. A procedure for obtaining the number of fibres in the layers of Modification II was proposed. The investigation showed that with the beginning of the 5th layer, the above-mentioned modifications have different packing properties. Because of additional fibres in the layers of Modification II, packing fractions in the layers and yarn obtained were greater if compared with those for Modification I. Analysis of packing properties was made up to 12 layers of the yarn model and also was done for a case of an infinitely large numbers of layers or fibres in a yarn.W pracy omówiono teoretyczne właściwości upakowania nieściśliwych okrągłych włókien dla dwóch wyidealizowanych modyfikacji modelu przędzy typu „open-packed”. Modyfikacje różniły się w sposobie układania włókien w obrębie warstwy przekroju poprzecznego. Wykazano, że wraz z początkiem piątej warstwy modyfikacje mają różne właściwości upakowania. Analiza właściwości upakowania została wykonana do 12 warstw modelu przędzy oraz w przypadku nieskończenie dużej liczby warstw i włókien w przędzy

    Litewskie tekstylia ludowe i możliwości ich projektowania

    No full text
    Lithuanian folk textile heritage is an important part of world culture heritage, on which various ideas and traditions are imprinted with the emphasis on the education of self-consciousness of society and preservation of national identity. This paper deals with a complex analysis of Lithuanian national fabrics, the data of which have been collected by the authors’ abundant expeditions into Lithuanian rural territories. The current research presents the peculiarities of designs, colours and ornamentation of authentic woven textile manufactured since the middle of the 19th century up to now. The significance of this study is that it investigates only authentic textiles obtained from weavers or their relatives in Lithuanian villages, and the presence of these articles has been undisclosed up to now. This research presents collected, registered and investigated data concerning colours, ornamentation and patternsas expressive possibilities of designs of Lithuanian folk textile: dimai and pick-up fabrics. The current analysis discovers new features of originality of the national fabrics.Litewskie dziedzictwo folklorystyczne stanowi ważną część światowego dziedzictwa kulturowego, jego idee i tradycje odznaczają się naciskiem na edukację samoświadomości społeczeństwa i zachowanie tożsamości narodowej. W pracy przeprowadzono kompleksową analizę litewskich tkanin narodowych. Zaprezentowane badania przedstawiają osobliwości wzorów, kolorów i ozdób autentycznych tkanin tekstylnych wytwarzanych od połowy XIX wieku do dziś. Badano wyłącznie autentyczne tkaniny uzyskane od tkaczy lub ich krewnych w litewskich wioskach. W artykule przedstawiono zebrane, zarejestrowane i sprawdzone dane dotyczące kolorów, ornamentów i wzorów jako możliwości projektowania tkaniny folklorystycznych dimai i pick-up. Zaprezentowana analiza wskazuje cechy oryginalności litewskich tkanin

    Właściwości wytrzymałościowe lnianych przędz łączonych różnymi węzłami

    No full text
    Analizowano różne właściwości mechaniczne przy zrywaniu lnianych przędz łączonych różnymi węzłami, stosując test na rozciąganie dla czterech węzłów o różnej strukturze - węzeł prosty, zwykły, tkacki i rybacki. Zastosowano cztery próbki: 50 tex (A - bielona, B - surowa) i 68 tex (C - bielona, D - surowa), każda wyprzędziona z lnu. W pracy przedstawiono wartości siły zrywającej, wytrzymałości przy zerwaniu, wydłużenia przy zerwaniu, pracy do zerwania oraz jednostkowej pracy do zerwania dla przędz łączonych węzłami. Ponadto, przeanalizowano współczynnik retencji dla siły zrywającej, wydłużenia przy zerwaniu i pracy przy zerwaniu. Stwierdzono, że wytrzymałość przędz łączonych węzłami zależy w dużym stopniu od struktury węzłów, podczas gdy przędze surowe i bielone wykazały podobne właściwości wytrzymałościowe.The various tensile properties of knotted line flax spun yarns have been studied by applying a tensile test for four different structures of knots, namely the square knot, overhand knot, weaver's knot, and fisherman's knot. Four types, i.e. 50 tex (A - bleached, B - grey) and 68 tex (C - bleached, D - grey) samples, each spun from line flax, were used for experiment. In this study, the values of breaking force, tenacity, elongation at break, work of break, and specific work of break of the knotted yarns are presented. In addition, the coefficients of retention for the breaking force, elongation at break and work of break are discussed. According to this study, the tensile behaviour of knotted yarns is highly affected by the knot structure. Meanwhile the bleached knotted yarns and the grey knotted yarns exhibited rather similar tensile properties or only small differences were established

    Folklorystyczne tkaniny z wątkiem górnym - tekstylne dziedzictwo północnej i wschodniej Litwy

    No full text
    Lithuania has deep traditions in hand-loom weaving. This paper deals with the evaluation and systematisation of North and East Lithuanian hand woven overshot fabrics. This textile heritage has not yet been investigated thoroughly. Investigations of authentic woven fabrics, their patterns, colours as well as weaving technologies are presented with special regard for textile identification, technological analysis and experience of masters. The importance lies in the fact that not only original articles are still extant for Lithuanian rural masters or with their families but the existence of these original works up to now has been undisclosed. In this study textile materials from the last 150 years were investigated. All the data for this research was collected directly from the textile masters during numerous expeditions by the authors in 2013, and in this study we present woven fabrics and weaving traditions as a significant expression of the ethno-cultural identity of an individual and the region.Na Litwie istnieją długie tradycje tkania na krosnach ręcznych. Materiał ten nie był dotychczas starannie badany. Analizowano tkaniny pod względem stosowanych wzorów, kolorystyki, jak również technologii tkackich. Badano tkaniny wyprodukowane w ostatnich 150-ciu latach. Brano pod uwagę tkaniny zbadane na podstawie ankiet przeprowadzonych w terenie. Zwrócono uwagę na zależność wzorów od technologii tkania oraz na występowanie podobnego wzornictwa w krajach sąsiednich a nawet znacznie oddalonych od Litwy

    Analiza możliwości nanoszenia olejku eukaliptusowego zawartego w mikrokapsułach na włókna naturalne i materiały frotowe

    No full text
    This research studied the influence of thermo-fixing temperature and binder concentration on the fixation of microcapsules with Eucalyptus essential oil to yarns and terry fabrics as well as physical properties of textiles with microcapsules. SEM micrographs confirmed that the grafting of microcapsules onto yarns spun from cotton, grey linen, bleached linen, ramie and bamboo fibres as well as onto ramie-cotton terry fabrics was effective. We conclude that a thermo-fixing temperature of 160 °C and higher caused the deformation of microcapsules or the partial or entire loss of an active product of the majority of microcapsules. Larger microcapsules were commonly damaged faster and were worse than smaller ones. It was determined that variation of the binder concentration from 20 to 95 g/l increased the area density of ramie/cotton terry fabric 1.7 times. The area density of terry fabric grafted with microcapsules in relation to the weft density could be described by linear equations.W pracy badano wpływ temperatury stabilizacji termicznej i stężenie materiału wiążącego na naniesienie mikrokapsuł wypełnionych olejkiem eukaliptusowym do włókien i materiałów frotowych. Badano również właściwości fizyczne materiałów włókienniczych z mikrokapsułami. Zdjęcia SEM potwierdziły, że naniesienie mikrokapsuł na przędze przędzione z bawełny, surowego lnu, bielonego lnu, ramii i włókien bambusowych, jak również na materiały frotowe wykonane z mieszanek ramia/bawełna było efektywne. Mogliśmy wywnioskować, że temperatura stabilizacji 160 °C i wyższa powoduje deformację większości mikrokapsułek i w efekcie częściowy lub całkowity ubytek substancji aktywnej. Większe mikrokapsułki były zazwyczaj niszczone szybciej i w efekcie były gorsze niż kapsułki mniejsze. Stwierdzono również, że zmiana w stężeniach czynnika wiążącego pomiędzy 20 - 95 g/l zwiększa masę powierzchniową materiałów frotowych ramia/bawełna 1,7 razy

    Wpływ dodatków funkcyjnych na właściwości kompozytowych włókien taśmowych

    No full text
    While the functional compound Polycom JB 7100 is often introduced into polyolefins as a modifier, processing aid and bonding agent, little is known about its influence upon the basic structure and mechanical properties of composite tape yarns. Polycom JB 7100 is a master bath of inorganic materials and polyolefins. To show the effects of different amounts (0 - 6 wt%) of this additive in polypropylene (PP)-based composite tape yarns, experiments were made without changes to other additive portions and at constant process parameters. The linear composition-property relations showing the effects of portions of the variable component on the changes in morphology, geometrical properties and tensile behaviour were obtained. Tape yarns, in which a portion of PP was replaced by the functional compound Polycom JB 7100, had tensile properties about 2 - 9% lower than the yarns without this additive, whereas the values of width, thickness and linear density after applications of the additive were about 3 - 4% greater if compared with those of the basic sample.Badano oddziaływanie zróżnicowanych ilości czynnego związku chemicznego Polycom JB 7100/składnik PP na właściwości poliolefinowych przędz tasiemkowych wytworzonych przy stałych udziałach innych domieszek i stałych warunkach procesu ich wytwarzania. Analiza sporządzonych mikrofotografii EDX i SEM wykazała, że aglomeracje cząstek materiałów nieorganicznych lub elementu wapnia na powierzchniach przędz tasiemkowych uległy zwiększeniu po zastosowaniu domieszki Polycom JB 7100. Zaproponowano matematyczny opis badanych zjawisk za pośrednictwem liniowych współzależności obrazujących wpływ zmian udziału wagowego domieszki na właściwości wytrzymałościowe próbek przędz tasiemkowych. Przeprowadzone badania wykazały, że szerokość, grubość i gęstość liniowa przędz tasiemkowych uległa zwiększeniu o około 3-4% po zwiększeniu domieszki Polycomu JB 7100 do mierzonej wagowo ilości. Z drugiej strony, zastosowana domieszka spowodowała zmniejszenie siły zrywającej, wytrzymałości, pracy zrywania i modułu początkowego przędzy tasiemkowej o około 2-9%. Zaobserwowane zmiany można wytłumaczyć różnicami powstałymi na skutek zmian w prędkości wytłaczania polimeru, orientacji filamentów i ciągłości tworzących się nowych struktur
    corecore