6 research outputs found

    Effects of different sterilization methods on the morphology, mechanical properties, and cytotoxicity of chitosan membranes used as wound dressings

    No full text
    The aim of this work was to compare the effects induced by two different sterilization methods (exposure to gamma radiation or ethylene oxide) and an antiseptic technique (immersion in 70% ethanol aqueous solution) on the morphology, tensile strength, percentage of strain at break, and in vitro cytotoxicity to Vero cells on chitosan membranes designed for wound healing. Four distinct membrane compositions were evaluated, with chitosan, glycerol, and chitin used as components. Gamma radiation, in spite of being one of the most commonly employed sterilizing agents, negatively affected the morphology of membranes composed solely by chitosan as well as the percentage of strain at break of the chitosan-membranes containing glycerol on their composition. Moreover, its use affected the color of the chitosan membranes. The use of 70% ethanol aqueous solution did not change the chitosan-membrane characteristics significantly, but its use has limitations concerning the process scale up. With ethylene oxide (EtO), chitosan-membrane morphology, percentage of strain at break, and in vitro cytotoxicity to Vero cells were not significantly affected. The tensile strength of the membranes containing chitin were reduced after the treatment with ethylene oxide; however, the obtained values were comprised in the range verified for normal human skin. Therefore, because the final characteristics of the membranes treated with ethylene oxide are appropriate when considering their use as wound healing devices, and because this sterilization process is easily adjusted to use on an industrial scale, EtO can be considered the most adequate sterilizing agent for chitosan membranes. However, it should be considered that this chemical is associated with toxicity, flammability, and environmental risks, as well as with possible material contamination with ethylene oxide residues. (C) 2004 Wiley Periodicals, Inc.71B226827

    The Effect of Sterilization Methods on the Physical Properties of Silk Sericin Scaffolds

    No full text
    Protein-based biomaterials respond differently to sterilization methods. Since protein is a complex structure, heat, or irradiation may result in the loss of its physical or biological properties. Recent investigations have shown that sericin, a degumming silk protein, can be successfully formed into a 3-D scaffolds after mixing with other polymers which can be applied in skin tissue engineering. The objective of this study was to investigate the effectiveness of ethanol, ethylene oxide (EtO) and gamma irradiation on the sterilization of sericin scaffolds. The influence of these sterilization methods on the physical properties such as pore size, scaffold dimensions, swelling and mechanical properties, as well as the amount of sericin released from sericin/polyvinyl alcohol/glycerin scaffolds, were also investigated. Ethanol treatment was ineffective for sericin scaffold sterilization whereas gamma irradiation was the most effective technique for scaffold sterilization. Moreover, ethanol also caused significant changes in pore size resulting from shrinkage of the scaffold. Gamma-irradiated samples exhibited the highest swelling property, but they also lost the greatest amount of weight after immersion for 24 h compared with scaffolds obtained from other sterilization methods. The results of the maximum stress test and Young’s modulus showed that gamma-irradiated and ethanol-treated scaffolds are more flexible than the EtO-treated and untreated scaffolds. The amount of sericin released, which was related to its collagen promoting effect, was highest from the gamma-irradiated scaffold. The results of this study indicate that gamma irradiation should have the greatest potential for sterilizing sericin scaffolds for skin tissue engineering

    A three-dimensional block structure consisting exclusively of carbon nanotubes serving as bone regeneration scaffold and as bone defect filler

    Get PDF
    Many recent studies have been conducted to assess the ability of composite materials containing carbon nanotubes (CNTs) with high bone affinity to serve as scaffolds in bone regenerative medicine. These studies have demonstrated that CNTs can effectively induce bone formation. However, no studies have investigated the usefulness of scaffolds consisting exclusively of CNTs in bone regenerative medicine. We built a three-dimensional block entity with maximized mechanical strength from multi-walled CNTs (MWCNT blocks) and evaluated their efficacy as scaffold material for bone repair. When MWCNT blocks containing recombinant human bone morphogenetic protein-2 (rhBMP-2) were implanted in mouse muscle, ectopic bone was formed in direct contact with the blocks. Their bone marrow densities were comparable to those of PET-reinforced collagen sheets with rhBMP-2. On day 1 and day 3, MC3T3-E1 preosteoblasts were attached to the scaffold surface of MWCNT blocks than that of PET-reinforced collagen sheets. They also showed a maximum compression strength comparable to that of cortical bone. Our MWCNT blocks are expected to serve as bone defect filler and scaffold material for bone regeneration
    corecore