11 research outputs found

    Obtenção de titùnio metålico com porosidade controlada por metalurgia do pó

    No full text
    Titanium is an attractive material for structural and biomedical applications because of its excellent corrosion resistance, biocompatibility and high strength-to-weight ratio. The high reactivity of titanium in the liquid phase makes it difficult to produce it by fusion. Powder metallurgy has been shown to be an adequate technique to obtain titanium samples at low temperatures and solid-phase consolidation. The production of compacts with different porosities obtained by uniaxial pressing and vacuum sintering is briefly reviewed. Powder particle size control has been shown to be very important for porosity control. Sample characterization was made using scanning electron microscopy (SEM) images

    Efeito do tratamento térmico na microestrutura, turbostraticidade e superfície de carbono vítreo reticulado analisado por XPS, espalhamento Raman e voltametria cíclica Thermal treatment effect on the microstructure, turbostraticity, and surface of reticulated vitreous carbon analyzed by xps, Raman scattering, and cyclic voltammetry

    No full text
    <abstract language="eng">The structural and surface properties of reticulated vitreous carbon (RVC) were discussed as a function of its heat treatment temperature (HTT), for samples produced in the range from 700 to 2000 ÂșC, using the furfuryl precursor resin. The samples were analyzed by x-ray photoelectron spectroscopy, first and second order Raman scattering as well as electrochemical response. Exploring the material turbostraticity concept, the interdependence between the RVC chemical surface variation and its defects were demonstrated. The influence of heteroatom presence was discussed in the material ordering for HTT lower than 1300 ÂșC while the graphitization process evolution was also pointed out for HTT higher than 1500 ÂșC

    Morphology and stress study of nanostructured porous silicon as a substrate for PbTe thin films growth by electrochemical process

    No full text
    Porous silicon layers (PSL) were produced by stain etching from a HF:HNO3 500:1 mixture with etching time varying in the range of 1 up to 10 min. The samples have presented nanometric porosity as a function of etching time, characteristic of heavily doped p type silicon. The residual stress and the correlation length of the layers were obtained through the analysis of the micro-Raman spectra using a phonon confinement model including a term to account for the amorphous phase. The residual compressive stress tends to increase as expected due to the contribution of smaller crystallites to be more representative as the etching time increases. PbTe thin films were electrodeposited on PSL from aqueous alkaline solutions of Pb(CH3COO)2, disodium salt of ethylendiaminetetraacetic acid (EDTA) and TeO2 by galvanostatic and potentiostatic method. It was also obtained nanostructured PbTe thin films with polycrystalline morphology evidenced by X-ray Diffraction (XRD) spectra. Scanning Electron Microscopy (SEM) analysis has demonstrated good films reproducibility with an average grain size of 100 nm

    Filmes de diamante CVD dopado com boro. Parte I . Histórico, produção e caracterização Boron-doped CVD diamond films. Part I. History, production and characterization

    No full text
    <abstract language="eng">This review presents a brief account concerning the production, characterization and evolution of the knowledge in the area of diamond and boron-doped diamond films. The most important methods used for the growth of these films, such as chemical vapor deposition and high pressure/high temperature systems, as well as the several kinds of reactors which can be employed are reviewed. However, larger emphasis is given to the CVD method. Morphological, structural and electric properties of these films, as well as their role in the performance of voltammetric electrodes for electrochemistry and electroanalytical chemistry are also discussed