4 research outputs found

    Ectopic bone formation in bone marrow stem cell seeded calcium phosphate scaffolds as compared to autograft and (cell seeded) allograft

    Get PDF
    Improvements to current therapeutic strategies are needed for the treatment of skeletal defects. Bone tissue engineering offers potential advantages to these strategies. In this study, ectopic bone formation in a range of scaffolds was assessed. Vital autograft and devitalised allograft served as controls and the experimental groups comprised autologous bone marrow derived stem cell seeded allograft, biphasic calcium phosphate (BCP) and tricalcium phosphate (TCP), respectively. All implants were implanted in the back muscle of adult Dutch milk goats for 12 weeks. Micro-computed tomography (µCT) analysis and histomorphometry was performed to evaluate and quantify ectopic bone formation. In good agreement, both µCT and histomorphometric analysis demonstrated a significant increase in bone formation by cell-seeded calcium phosphate scaffolds as compared to the autograft, allograft and cell-seeded allograft implants. An extensive resorption of the autograft, allograft and cell-seeded allograft implants was observed by histology and confirmed by histomorphometry. Cell-seeded TCP implants also showed distinct signs of degradation with histomorphometry and µCT, while the degradation of the cell-seeded BCP implants was negligible. These results indicate that cell-seeded calcium phosphate scaffolds are superior to autograft, allograft or cell-seeded allograft in terms of bone formation at ectopic implantation sites. In addition, the usefulness of µCT for the efficient and non-destructive analysis of mineralised bone and calcium phosphate scaffold was demonstrated

    Effect of particle morphology and polyethylene molecular weight on the fracture toughness of hydroxyapatite reinforced polyethylene composite

    No full text
    Fracture toughness testing has been performed on hydroxyapatite–polyethylene composites. Sintered and unsintered grades of hydroxyapatite and two grades of high-density polyethylene were used to make 40 vol % hydroxyapatite composites. Compact tension testing was performed at both room temperature and at 37 °C and at three strain rates. The effect of increasing the loading rate from 2 to 200 μmgrm s–1 was to increase the fracture toughness. Increasing the testing temperature or decreasing the surface area of the reinforcing particles also increased the fracture toughness. However, using a lower molecular weight, injection moulding, grade of polyethylene reduced the fracture toughness. Thus for higher fracture toughness, a low surface area sintered hydroxyapatite in a high-molecular weight polyethylene is required
    corecore