    Growth Techniques for Bulk ZnO and Related Compounds

    Full text link
    ZnO bulk crystals can be grown by several methods. 1) From the gas phase, usually by chemical vapor transport. Such CVT crystals may have high chemical purity, as the growth is performed without contact to foreign material. The crystallographic quality is often very high (free growth). 2) From melt fluxes such as alkaline hydroxides or other oxides (MoO3, V2O5, P2O5, PbO) and salts (PbCl2, PbF2). Melt fluxes offer the possibility to grow bulk ZnO under mild conditions (<1000 deg. C, atmospheric pressure), but the crystals always contain traces of solvent. The limited purity is a severe drawback, especially for electronic applications. 3) From hydrothermal fluxes, usually alkaline (KOH, LiOH) aqueous solutions beyond the critical point. Due to the amphoteric character of ZnO, the supercritical bases can dissolve it up to several per cent of mass. The technical requirements for this growth technology are generally hard, but this did not hinder its development as the basic technique for the growth of {\alpha}-quartz, and meanwhile also of zinc oxide, during the last decades. 4) From pure melts, which is the preferred technology for numerous substances applied whenever possible, e.g. for the growth of silicon, gallium arsenide, sapphire, YAG. The benefits of melt growth are (i) the high growth rate and (ii) the absence of solvent related impurities. In the case of ZnO, however, it is difficult to find container materials that are compatible from the thermal (fusion point Tf = 1975 deg. C) and chemical (required oxygen partial pressure) point of view. Either cold crucible (skull melting) or Bridgman (with reactive atmosphere) techniques were shown to overcome the problems that are inherent to melt growth. Reactive atmospheres allow to grow not only bulk ZnO single crystals, but also other TCOs such as {\beta}-Ga2O3 and In2O3.Comment: 10 pages, 7 figures, talk on MRS Fall 2011 Bosto

    The inverse perovskite BaLiF3: single-crystal neutron diffraction and analyses of potential ion pathways

    Get PDF
    Doped barium lithium trifluoride has attracted attention as component for scintillators, luminescent materials and electrodes. With lithium and fluoride, it contains two possibly mobile species, which may account for its ionic conductivity. In this study, neutron diffraction on oxide-containing BaLiF3 single-crystals is performed at up to 636.2°C. Unfortunately, ion-migration pathways could not be mapped by modelling anharmonic ion displacement or by inspecting the scattering-length density that was reconstructed via maximum-entropy methods. However, analyses of the topology and bond-valence site energies derived from the high-temperature structure reveal that the anions can migrate roughly along the edges of the LiF6 coordination octahedra with an estimated migration barrier of ∼0.64 eV (if a vacancy permits), whereas the lithium ions are confined to their crystallographic positions. This finding is not only valid for the title compound but for ion migration in all perovskites with Goldschmidt tolerance factors near unity
    • …
    corecore