    Dependence of the superconducting transition temperature on the doping level in single crystalline diamond films.

    Get PDF
    Homoepitaxial diamond layers doped with boron in the 10^20-10^21 /cm3 range are shown to be type II superconductors with sharp transitions (~0.2K) at temperatures increasing from 0 to 2.1 K with boron contents. The critical concentration for the onset of superconductivity is about 5-7 10^20 /cm3, close to the metal-insulator transition. The H-T phase diagram has been obtained from transport and a.c. susceptibility measurements down to 300mK. These results bring new quantitative constraints on the theoretical models proposed for superconductivity in diamond