Abiotic ammonium formation in the presence of Ni-Fe metals and alloys and its implications for the Hadean nitrogen cycle
Experiments with dinitrogen-, nitrite-, nitrate-containing solutions were conducted without headspace in Ti reactors (200°C), borosilicate septum bottles (70°C) and HDPE tubes (22°C) in the presence of Fe and Ni metal, awaruite (Ni80Fe20) and tetrataenite (Ni50Fe50). In general, metals used in this investigation were more reactive than alloys toward all investigated nitrogen species. Nitrite and nitrate were converted to ammonium more rapidly than dinitrogen, and the reduction process had a strong temperature dependence. We concluded from our experimental observations that Hadean submarine hydrothermal systems could have supplied significant quantities of ammonium for reactions that are generally associated with prebiotic synthesis, especially in localized environments. Several natural meteorites (octahedrites) were found to contain up to 22 ppm Ntot. While the oxidation state of N in the octahedrites was not determined, XPS analysis of metals and alloys used in the study shows that N is likely present as nitride (N3-). This observation may have implications toward the Hadean environment, since, terrestrial (e.g., oceanic) ammonium production may have been supplemented by reduced nitrogen delivered by metal-rich meteorites. This notion is based on the fact that nitrogen dissolves into metallic melts
Chromate reduction in highly alkaline groundwater by zerovalent iron: Implications for its use in a permeable reactive barrier
It is not currently known if the widely used reaction of zerovalent iron (ZVI) and Cr(VI) can be used in a permeable reactive barrier (PRB) to immobilize Cr leaching from hyperalkaline chromite ore processing residue (COPR). This study compares Cr(VI) removal from COPR leachate and chromate solution by ZVI at high pH. Cr(VI) removal occurs more rapidly from the chromate solution than from COPR leachate. The reaction is first order with respect to both [Cr(VI)] and the iron surface area, but iron surface reactivity is lost to the reaction. Buffering pH downward produces little change in the removal rate or the specific capacity of iron until acidic conditions are reached. SEM and XPS analyses confirm that reaction products accumulate on the iron surface in both liquors, but that other surface precipitates also form in COPR leachate. Leachate from highly alkaline COPR contains Ca, Si, and Al that precipitate on the iron surface and significantly reduce the specific capacity of iron to reduce Cr(VI). This study suggests that, although Cr(VI) reduction by ZVI will occur at hyperalkaline pH, other solutes present in COPR leachate will limit the design life of a PRB