Thin film trilayer junction of LaSr0.33MnO3 - SrTiO3 -
La0.67Sr0.33MnO3 shows a factor of 9.7 change in resistance, in a
magnetic field around 100 Oe at 14K. The junction magnetoresistance is bias and
temperature dependent. The energy scales associated with bias and temperature
dependence are an order of magnitude apart. The same set of energies also
determine the bias and temperature dependence of the differential conductance
of the junction. We discuss these results in terms of metallic cluster
inclusions at the junction-barrier interface.Comment: 3 pages, 4 figure