The optical properties of sodium-deficient NaxV2O5 (0.85 < x <1) single
crystals are analyzed in the wide energy range, from 0.012 to 4.5 eV, using
ellipsometry, infrared reflectivity, and Raman scattering techniques. The
material remains insulating up to the maximal achieved hole concentration of
about 15%. In sodium deficient samples the optical absorption peak associated
to the fundamental electronic gap develops at about 0.44 eV. It corresponds to
the transition between vanadium dxy and the impurity band, which forms in the
middle of the pure NaV2O5 gap. Raman spectra measured with incident photon
energy larger then 2 eV show strong resonant behavior, due to the presence of
the hole-doping activated optical transitions, peaked at 2.8 eV.Comment: 7 pages, 4 fugures, to be published in PR