We have studied the changes in the ferromagnetic behavior of graphite powder
and graphite flakes after treatment with diluted sulphuric acid. We show that
this kind of acid treatment enhances substantially the ferromagnetic
magnetization of virgin graphite micrometer size powder as well as in graphite
flakes. The anisotropic magnetoresistance (AMR) amplitude at 300 K measured in
a micrometer size thin graphite flake after acid treatment reaches values
comparable to polycrystalline cobalt.Comment: 3.2 pages, 4 figure