Predviđanje životnog vijeka oštećene plinske cijevi PE 80

Abstract

This paper deals with new approach to life estimation of damaged thick-walled gas pipes made of high-density polyethylene (PE 80). The most common approaches to polyethylene gas pipes durability prediction rely on methods of fracture mechanics, which involve defining the stress intensity factor experimentally. However, such tests are carried out on standardized specimens neglecting the influence of real pipe geometry and processing method. On the other hand, these data are not always available to gas distributors, which are responsible for installed pipelines durability. Investigations based on long-term experiments involving three parameters: pressure, length and depth of initial notch type crack gave empirical mathematical model for life prediction of polyethylene gas pipes.U radu je prikazan novi pristup za procjenu preostalog vremena uporabe oštećenih plinovodnih cijevi od polietilena visoke gustoće (PE 80). U praksi se najčešće primjenjuju metode mehanike loma za procjenu trajnosti polietilenskih plinovodnih cijevi koje uključuju eksperimentalno definiranje koeficijenta intenzivnosti naprezanja. Međutim takvi su testovi napravljeni na normiranim ispitnim tijelima pri čemu je zanemaren utjecaj stvarne geometrije i postupak proizvodnje cijevi. S druge strane, podaci o koeficijentu intenzivnosti naprezanja nisu uvijek dostupni distributerima prirodnog plina. Provedbom dugotrajnih ispitivanja temeljenih na distributerima dostupnim podacima: tlaku u cijevima, duljini zareznog oštećenja i dubini zareznog oštećenja dobiven je empirijski matematički model za procjenu preostalog vremena uporabe oštećenih polietilenskih plinovodnih cijevi

    Similar works