CORE
🇺🇦
make metadata, not war
Services
Services overview
Explore all CORE services
Access to raw data
API
Dataset
FastSync
Content discovery
Recommender
Discovery
OAI identifiers
OAI Resolver
Managing content
Dashboard
Bespoke contracts
Consultancy services
Support us
Support us
Membership
Sponsorship
Community governance
Advisory Board
Board of supporters
Research network
About
About us
Our mission
Team
Blog
FAQs
Contact us
K_Ⅰ,K_Ⅱ复合型裂纹的脆性断裂
Authors
周爱华
杨成寿
王自强
高桦
Publication date
1 January 1979
Publisher
Abstract
本文用三点弯曲和四点弯曲试样,在K_Ⅱ/K_Ⅰ=0—14的范围内,对GC-4超高强度钢、30Cr2MoV中强度转子钢和稀土球墨铸铁进行了线弹性平面应变复合型脆断试验。结果表明:复合型裂纹的脆断开裂方向与现有的三种复合型理论符合较好;但是,复合型裂纹扩展阻力随K_Ⅱ/K_Ⅰ比值增加而增大,与现有复合型理论差别较大。本文从塑性区的形状、大小和裂纹顶端在开裂方向的应力状态等方面对此问题进行了分析并指出,现有理论关于复合型裂纹扩展阻力与变形特征无关的假设,对于具有一定塑性变形能力的金属材料,是不合适的。文章还对简单且偏于安全的处理复合型问题的工程分析方法作了讨论
Similar works
Full text
Available Versions
Institute Of Mechanics,Chinese Academy of Sciences
See this paper in CORE
Go to the repository landing page
Download from data provider
oai:dspace.imech.ac.cn:311007/...
Last time updated on 12/02/2018