CORE
🇺🇦
make metadata, not war
Services
Services overview
Explore all CORE services
Access to raw data
API
Dataset
FastSync
Content discovery
Recommender
Discovery
OAI identifiers
OAI Resolver
Managing content
Dashboard
Bespoke contracts
Consultancy services
Support us
Support us
Membership
Sponsorship
Community governance
Advisory Board
Board of supporters
Research network
About
About us
Our mission
Team
Blog
FAQs
Contact us
金属空气电池阴极的制备方法与金属空气电池
Authors
刘兆平
孙珊珊
+3 more
张勤号
苗鹤
薛业建
Publication date
7 September 2016
Publisher
Abstract
本发明提供了一种金属空气电池阴极的制备方法,包括以下步骤:A)将粘结剂、成膜剂、疏水性材料、导电剂与处理液混合后球磨,得到浆料;B)将步骤A)得到的浆料涂布于泡沫镍表面,烧制后得到疏水透气层;C)将疏水透气层与催化剂层冷压后进行烧制,得到金属空气电池阴极。本申请提供的金属空气电池阴极的制备方法,制备得到的阴极结构具有较强的结构强度、良好的疏水透气性和较好的孔隙率,最终使包括该阴极的金属空气电池具有较好的电池性能、结构重现性和长期稳定性
Similar works
Full text
Available Versions
Institutional Repository of Ningbo Institute of Material Technology & Engineering, CAS
See this paper in CORE
Go to the repository landing page
Download from data provider
oai:ir.nimte.ac.cn/:174433/154...
Last time updated on 22/01/2018