Photoetching method producing well-defined lines with minimum undercutting was developed for etching coolant passages in nickel sheet. Phosphate coating is applied over conventional silver plate maskant and phosphoric acid solution is used to remove silver maskant. Phosphoric acid prevents etching of silver edges and mask has sharply-defined lines