Thermal and electric properties of Nd(1.85)Ce(0.15)CuO(4-y) and Pr(1.85)Ce(0.15)CuO(4-y)

Abstract

Electric resistivity, magnetic susceptibility, thermoelectric power, and Hall coefficient of Nd(1.85)Ce(0.15)CuO(4-y) and Pr(1.85)Ce(0.15)CuO(4-y) whose onset temperature of the superconductivity are 24 and 23 K were measured. Experimental results show many interesting features. In particular, the Hall coefficients are negative and relatively flat as a function of temperature. However, the temperature dependence of the thermoelectric power (TEP) for these two samples shows the positive sign for both samples in contrast to the previous results. Moreover, TEP for both samples remains flat in the normal state below 250 K, but decreases rapidly above 250 K. TEP of only Pr(1.85)Ce(0.15)CuO(4-y) shows a peak near 50 K. Finally, onset temperatures of sudden drop of TEP are higher than those of resistance drop. The physical properties of these samples produced at different conditions such as different heat treatment temperatures, atmospheres were also measured. TEP and resistance measurement show that oxygen deficiency is essential to produce better superconducting samples. Correlation between TEP and superconductivity for these different samples are discussed

    Similar works