    Influences of the operating variables of acetosolv pulping on pulp properties of oil palm frond fibres

    Get PDF
    The effect of acetosolv pulping variables viz. pulping time, temperature, catalyst (HCl) and acetic acid on oil palm frond fibres was investigated. The following conditions were found to be optimum to pulp frond fibres: 140 ºC, 0.5% HCl, 75% acetic acid, and 1/10 solid/liquor ratio. Under these conditions we could obtain these properties: Kappa number 13-16, zero-span tensile breaking length – 83 km, sheet density – 0.57 g cm-3, tensile index – 48 N m g-1, tear index – 5.4 mN m2 g-1, brightness – 16% ISO and opacity – 98%. Higher values of these operating parameters would degrade the fibre characteristics such as zero-span tensile breaking length, tensile index, and sheet density

    Influences of the operating variables of acetosolv pulping on pulp properties of oil palm frond fibres

    No full text
    The effect of acetosolv pulping variables viz. pulping time, temperature, catalyst (HCl) and aceticacid on oil palm frond fibres was investigated. The following conditions were found to be optimum topulp frond fibres: 140 ºC, 0.5% HCl, 75% acetic acid, and 1/10 solid/liquor ratio. Under these conditionswe could obtain these properties: Kappa number 13-16, zero-span tensile breaking length � 83 km, sheetdensity � 0.57 g cm-3, tensile index � 48 N m g-1, tear index � 5.4 mN m2 g-1, brightness � 16% ISO andopacity � 98%. Higher values of these operating parameters would degrade the fibre characteristicssuch as zero-span tensile breaking length, tensile index, and sheet density

    Influences of the operating variables of acetosolv pulping on pulp properties of oil palm frond fibres

    No full text
    The effect of acetosolv pulping variables viz. pulping time, temperature, catalyst (HCl) and acetic acid on oil palm frond fibres was investigated. The following conditions were found to be optimum to pulp frond fibres: 140 ºC, 0.5% HCl, 75% acetic acid, and 1/10 solid/liquor ratio. Under these conditions we could obtain these properties: Kappa number 13-16, zero-span tensile breaking length - 83 km, sheet density - 0.57 g cm-3, tensile index - 48 N m g-1, tear index - 5.4 mN m² g-1, brightness - 16% ISO and opacity - 98%. Higher values of these operating parameters would degrade the fibre characteristics such as zero-span tensile breaking length, tensile index, and sheet density

    Influences of the operating variables of acetosolv pulping on pulp properties of oil palm frond fibres

    No full text
    The effect of acetosolv pulping variables viz. pulping time, temperature, catalyst (HCl) and acetic acid on oil palm frond fibres was investigated. The following conditions were found to be optimum to pulp frond fibres: 140 ºC, 0.5% HCl, 75% acetic acid, and 1/10 solid/liquor ratio. Under these conditions we could obtain these properties: Kappa number 13-16, zero-span tensile breaking length - 83 km, sheet density - 0.57 g cm-3, tensile index - 48 N m g-1, tear index - 5.4 mN m² g-1, brightness - 16% ISO and opacity - 98%. Higher values of these operating parameters would degrade the fibre characteristics such as zero-span tensile breaking length, tensile index, and sheet density
    corecore