    Dynamic Compaction of Biomaterial Powders

    No full text
    Dynamic compaction which requires no external heating for consolidation was used to compact hydroxyapatite. Static precompaction of 3 MPa and dynamic compaction using a projectile velocity of 50 m/s resulted in compacts having a compaction degree of 65% and a tensile strength of 12.4 ± 2.7 MPa This strength was very close to that obtained with sintered compacts one and seemed to indicate that some interparticle boundaries had been created during dynamic compaction