    This project is funded by the National Institute for Health Research Health Technology Assessment (NIHR HTA) Programme (project number 10/137/01) and will be published in full in Health Technology Assessment. The Health Services Research Unit of the University of Aberdeen iscore funded by the Chief Scientist Office (CSO) of the Scottish Government Health and Social Care Directorates. The views and opinions expressed therein are those of the authors and do not necessarily reflect those of the CSO, HTA programme, NIHR, NHS or the Department of Health.Peer reviewedPublisher PD

    Comparison of cycling high temperature corrosion at 650°C in the presence of NaCl of various austenitic stainless steels

    Get PDF
    The high temperature corrosion at 650°C in the presence of NaCl at atmospheric pressure of AISI 304L, AISI 309, AISI 310S, AISI 314 and AISI 321 austenitic stainless steel was studied. The specimens were cyclically heated in the furnace and immersed in a 3.5% aqueous NaCl solution after cooling for 15 min. After each cycle, the change in mass of the samples was measured. The corroded samples were analysed by SEM /EDX, and the corrosion products were analysed by XRD. The chloride ions react with the steel surface to form porous and poorly adherent oxides and metal chlorides. After the mass increase during the first exposure cycles, spalling of the oxides occurred. The high temperature austenitic stainless steels (AISI 309, AISI 310S, AISI 314) showed less mass loss than conventional austenitic steels (AISI 304L). Surprisingly, the stainless steel AISI 321 showed a similar low weight loss after the cyclic test as AISI 309, but a detailed analysis of the exposed surfaces after the test showed a similar corrosion attack as for AISI 304. After the cyclic test at high temperature in the presence of NaCl, a higher concentration of Cr and Ni definitely improves the corrosion resistance under the present conditions, but a certain addition of Si is even more obvious
    corecore