    Magnetocrystalline anisotropy in single-crystal Co-Ni-Al ferromagnetic shape-memory alloy

    Get PDF
    科研費報告書収録論文(課題番号:13555181・基盤研究(B)(2) ・H13~H14/研究代表者:貝沼, 亮介/新しいB2型強磁性形状記憶合金の開発と多機能素子への展開

    Bone marrow mesenchymal stem cells do not enhance intra-synovial tendon healing despite engraftment and homing to niches within the synovium

    Get PDF
    Intra-synovial tendon injuries display poor healing, which often results in reduced functionality and pain. A lack of effective therapeutic options has led to experimental approaches to augment natural tendon repair with autologous mesenchymal stem cells (MSCs) although the effects of the intra-synovial environment on the distribution, engraftment and functionality of implanted MSCs is not known. This study utilised a novel sheep model which, although in an anatomically different location, more accurately mimics the mechanical and synovial environment of the human rotator cuff, to determine the effects of intra-synovial implantation of MSCs

    Effect of Grain Boundary Character Distribution on the Impact Toughness of 410NiMo Weld Metal

    Get PDF
    Grain boundary character distributions in 410NiMo weld metal were studied in the as-welded, first-stage, and second-stage postweld heat treatment (PWHT) conditions, and these were correlated with the Charpy-V impact toughness values of the material. The high impact toughness values in the weld metal in the as-welded and first-stage PWHT conditions compared to that in the second-stage condition are attributed to the higher fraction of low-energy I pound boundaries. A higher volume fraction of retained austenite and coarser martensite after second-stage PWHT accompanied by the formation of the ideal cube component in the 2-hour heat-treated specimen led to a reduction in the toughness value. A subsequent increase in the PWHT duration at 873 K (600 A degrees C) enhanced the formation of {111}aOE (c) 112 >, which impedes the adverse effect of the cubic component, resulting in an increase in the impact toughness. In addition to this, grain refinement during 4-hour PWHT in the second stage also increased the toughness of the weld metal