    Copolyamides of nylon-4,6 and nylon-4,T

    Get PDF
    Copolyamides of nylon-4,6 and nylon-4,T were prepared by a two-step method: (1) a prepolymerization in an autoclave (40 min at 210°C) and (2) a postcondensation in the solid state (4 h, 260°C). On these materials was studied the melting behavior with DSC, the crystalline structure with WAXS, the water absorption, and the mechanical properties with a torsion pendulum. In these copolyamides the order was found to remain high, but the crystalline structures of -4,6 and -4,T were not isomorphous. The torsion moduli increased with -4,T content both at RT and at 140°C