    Silver recovery from zinc metallurgical sludge – analysis of solutions

    Full text link
    During the hydrometallurgical process of zinc production, conducted in the ZGH “Bolesław” S.A. in Bukowno [Mine and Metallurgical Plant], about 40,000 tons of sludge is generated. After dehydration in the Larox filter presses, sludge contains ca. 16-18% of Zn, 20-25% of Fe, and 200-300 ppm of Ag. Next, sludge is transported to the Olkusz concentrator for flotation to obtain concentrate enriched with Ag (1,000-1,500 ppm). The concentrate is then sent to the HC “Miasteczko Śląskie” [zinc smelter], while the flotation tailings are subjected to recycling in waelz kiln in Bukowno to regain mainly Zn and Pb, in the form of oxides (also sent later to the HC “Miasteczko Śląskie”)

    Silver recovery from zinc metallurgical sludge – analysis of solutions

    No full text
    During the hydrometallurgical process of zinc production, conducted in the ZGH “Bolesław” S.A. in Bukowno [Mine and Metallurgical Plant], about 40,000 tons of sludge is generated. After dehydration in the Larox filter presses, sludge contains ca. 16-18% of Zn, 20-25% of Fe, and 200-300 ppm of Ag. Next, sludge is transported to the Olkusz concentrator for flotation to obtain concentrate enriched with Ag (1,000-1,500 ppm). The concentrate is then sent to the HC “Miasteczko Śląskie” [zinc smelter], while the flotation tailings are subjected to recycling in waelz kiln in Bukowno to regain mainly Zn and Pb, in the form of oxides (also sent later to the HC “Miasteczko Śląskie”)

    Silver recovery from zinc metallurgical sludge – analysis of solutions

    No full text
    During the hydrometallurgical process of zinc production, conducted in the ZGH “Bolesław” S.A. in Bukowno [Mine and Metallurgical Plant], about 40,000 tons of sludge is generated. After dehydration in the Larox filter presses, sludge contains ca. 16-18% of Zn, 20-25% of Fe, and 200-300 ppm of Ag. Next, sludge is transported to the Olkusz concentrator for flotation to obtain concentrate enriched with Ag (1,000-1,500 ppm). The concentrate is then sent to the HC “Miasteczko Śląskie” [zinc smelter], while the flotation tailings are subjected to recycling in waelz kiln in Bukowno to regain mainly Zn and Pb, in the form of oxides (also sent later to the HC “Miasteczko Śląskie”)