锂空气电池高容量长寿命Co3O4纳米空心球阴极催化剂

Abstract

以六水合硝酸钴(Co(NO3)2·6H2O)、六次甲基四胺(HMT)、蔗糖、柠檬酸钠(Na3C6H5O7)为原料,140oC下水热碳化处理即得反应前驱物,经煅烧处理后,可得多孔Co3O4纳米空心球.锂空气电池Co3O4/SP阴极催化剂具有优异的循环寿命性能,这归因于Co3O4空心球的纳米颗粒构成、较高比表面积的多孔结构,为电池反应提供了大量的反应位点,为充放电产物提供了足够的存储空间