Eucalyptus globulus heartwood, sapwood and their delignified samples by kraft pulping at 130, 150 and 170 degrees C along time were characterized in respect to total carbohydrates by Py-GC/MS(FID). No significant differences between heartwood and sapwood were found in relation to pyrolysis products and composition. The main wood carbohydrate derived pyrolysis compounds were levoglucosan (25.1%), hydroxyacetaldehyde (12.5%), 2-oxo-propanal (10.3%) and acetic acid (8.7%). Levoglucosan decreased during the early stages of delignification and increased during the bulk and residual phases. Acetic acid decreased hydroxyacetaldehyde and 2-oxo-propanal increased, and 2-furaldehyde and hydroxypropanone remained almost constant during delignification. The C/L ratio was 3.2 in wood and remained rather constant in the first pulping periods until a loss of 15-25% in carbohydrate and 60% in lignin. Afterwards it increased sharply until 44 that correspond to the removal of 25-35% of carbohydrates and 95% of lignin. The pulping reactive selectivity to lignin vs. polysaccharides was the same for sapwood and heartwood. (C) 2013 Elsevier B.V. All rights reserved
Is data on this page outdated, violates copyrights or anything else? Report the problem now and we will take corresponding actions after reviewing your request.