Sewage sludge charcoal production by N2-and CO2-torrefaction

Abstract

Abstract: The production of sewage sludge charcoals under N2 and CO2 as torrefaction atmosphere and their subsequent combustion was compared in this work. The experiments were carried out in a Thermogravimetry-Infrared Spectrometry (TGA-FTIR) analyser and a laboratory scale furnace. High temperatures (230–480 °C) were considered in order to study the removal of N- and S-compounds, one of the main concerns for the thermal valorisation of sewage sludge. Torrefaction treatment at 330 °C under N2 produced a charcoal with a 34% reduction in weight. The release of SO2 during the combustion of this charcoal was negligible and the release of NH3 and COS was reduced by half (46% for NH3 and 5! 2.5% for COS) compared with the combustion of raw sewage sludge. The pollutant removal improved with torrefaction temperature and the charcoal produced at 480 °C released a negligible amount of NH3, COS and SO2 during combustion. The CO2 used as torrefaction atmosphere exhibited a reactive behaviour in the FTIR-TGA analyser, increasing the weight loss rate and shifting the characteristic degradation peak to a temperature around 7 °C lower. Besides, the charcoals produced under CO2 exhibited a less reactive behaviour. Overall, the results here presented prove that the CO2 influences slightly the torrefaction mechanisms and the properties of the sewage sludge charcoals produced

Similar works

Full text

thumbnail-image

University of Johannesburg Institutional Repository

redirect
Last time updated on 21/11/2017

Having an issue?

Is data on this page outdated, violates copyrights or anything else? Report the problem now and we will take corresponding actions after reviewing your request.