We have measured the magnetic susceptibility of single crystal samples of
non-hydrated NaxCoO2 (x ~ 0.75, 0.67, 0.5, and 0.3) and hydrated Na0.3CoO2-yH2O
(y ~ 0, 0.6, 1.3). Our measurements reveal considerable anisotropy between the
susceptibilities with H||c and H||ab. The derived anisotropic g-factor ratio
(g_ab/g_c) decreases significantly as the composition is changed from the
Curie-Weiss metal with x = 0.75 to the paramagnetic metal with x = 0.3. Fully
hydrated Na0.3CoO2-1.3H2O samples have a larger susceptibility than
non-hydrated Na0.3CoO2 samples, as well as a higher degree of anisotropy. In
addition, the fully hydrated compound contains a small additional fraction of
anisotropic localized spins.Comment: 6 pages, 5 figure