Specific heats at constant pressure, C_p, of Fe-Ni (fcc) alloys have been measured a temperatures 300~1000 K. For alloys containing more than 50%Ni, the C_p-T curve shows a sharp λ-type peak at ferromagnetic Curie temperature. For the alloys less in concentration of nickel, however, only a dull peak is observed. The C_p-T curve is analyzed using the values of thermal expansion coefficient and of compressibility measured on the same conditions, separating the magnetic contribution from total specific heats